| X-RAY PHOTOELECTRON SPECTROSCOPY OF HIGH Tc SUPERCONDUCTOR YBa_2 Cu_3 O_(7-x) |
| TIAN Lu;WANG Wenhao;GONG Yandong;SUN Yuzhen;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
TIAN Lu;WANG Wenhao;GONG Yandong;SUN Yuzhen;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang. X-RAY PHOTOELECTRON SPECTROSCOPY OF HIGH Tc SUPERCONDUCTOR YBa_2 Cu_3 O_(7-x). Acta Metall Sin, 1991, 27(5): 130-135.
|
|
|
Abstract The XPS spectra of superconducting (123-orthorhombic structure) and non-superconducting (123-tetragonal structure) YBa_2Cu_3O_(7-x). ceramics were obtained at room temperature and 130 K in RIBER LAS 3000 surface analysis system, in which a sample cooling stage and a surface cleaning scraper, both made by the authors'own, were installed. No evidence of Cu~(3+) was found. The O1s shows double lines.They are attributed to O1 and O4 with higher binding energy and to O2 and O3 with lower binding energy respectively, and it was confirmed by calculation of SW-X_α method. The differences and changes in valence states of Y, Ba, Cu and O in both samples were discussed.
|
|
Received: 18 May 1991
|
1 Capponi J J, Chaillout C, Hewat A W, Leiay P, Maresio M, Nguyen N, Raveau B, Tholeace T L, Teurnier R. Eur Phys Lett, 1989; 3: 1310 2 Wang Wenhao, Tian Lu, Gong Yandong, Sun Yuzhen. Surf Sci, 1989; 213: 303 3 江晓平.低温物理学报,1987;9:192 4 Steiner P, Kinsinger V, Sander I, Siegwart B, Hufner S, Politis C, Hoppe R, Muller H P. Z Phys, 1987; B67: 497 5 Bianconi A, Congiu A, Castellano C, De Santis M, De Logu P, Gargano A, Giorgi R. Solid State Commun, 1987; 63: 1135 6 Anderson P W. In: Broglia R A, Schrieffer J R eds., Proc of the E. Fermi Inter. Summer School of Physics on Frontiers and Borderline in Many Particle Physics, Varenna, Italy, 1987, Amsterdam: North-Holland, 1987: 156 7 Fujimori A, Takayama-Muromachi E, Uchida Y, Okai B. Phys Rev, 1987; B35: 8814 8 Feil H. Solid State Commun, 1989; 69: 245 9 Larsson S. Chem Phys Lett, 1976; 40: 362 10 McIntyre N S, Cook M G. Anal Chem, 1975; 47: 2208 11 Beno M A, Soderholm L, Capone D W, Hinks D G, Jogensen J D, Grace J D, Schuller I K, Segre C U, Zhang K. Appl Phys Lett, 1987; 51: 57 12 Wagner C D, Riggs W M, Davis L E, Moulder J F. In: Mullerber G E ed, Handbook of X Ray Photoelectron Spectroscopy, USA: Perkin Elmer Co., 1979 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|