DIRECT HYDROGEN REDUCTION OF GALENA AT MODERATE TEMPERATURE
LIU Zhonghua;LIU Chunpeng Kunming Institute of Technology
Cite this article: 

LIU Zhonghua;LIU Chunpeng Kunming Institute of Technology. DIRECT HYDROGEN REDUCTION OF GALENA AT MODERATE TEMPERATURE. Acta Metall Sin, 1991, 27(5): 136-140.

Download:  PDF(637KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The direct reduction of galena with hydrogen at 873-973 K could be described by the shrinking core model in the chemical control region. The reaction was revealed to be of first order with respeot to hydrogen concentration and the activation energy is 79.0 kJ/mol. Because of the fairly large interface tension between the solid galena and the liquid Pb, the SEM second electron images showed that the liquid Pb film is difficult to be formed on the unreacted galena surface in reaction process.
Key words:  gas-solid reaction      galena      direct reduction     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/136

1 Liu Zhonghua, Liu Chunpeng, Xu Yousheng. Chin J Met Sci Technol, 1988; 4: 368
2 Szekely J, Evans J W. Sohn H Y. Gas-Solid Reactions. New York: Academic. 1976: 68
3 林传仙,白正华,张哲儒.矿物及有关化合物热力学数据手册.北京:科学出版社,1985:14
4 Davey T R A, Willis G M. J Met, 1977; 29(3) : 24
5 Smithells C J. Metals Reference Book, Vol. Ⅱ, 3rd ed, London: Butterworths, 1962: 571
6 Richardson F D. Physical Chemistry of Melts in Metallurgy. Vol. Ⅰ, London: Academic, 1974: 28
[1] Yongli JIN,Hai YU,Jieyu ZHANG,Zengwu ZHAO. Effects of Magnetic Field on Reduction of CaOContaining Iron Oxides[J]. 金属学报, 2019, 55(3): 410-416.
No Suggested Reading articles found!