SUPERPLASTICITY IN A WARM-ROLLED Al-8Mg-0.2Zr ALLOY |
HUANG Xiaoxu;LIU Qing;YAO Mei Harbih Institute of Technology Correspondent; professor; Post Box 433; Harbin Institute of Technology; Harbin 150006 |
|
Cite this article:
HUANG Xiaoxu;LIU Qing;YAO Mei Harbih Institute of Technology Correspondent; professor; Post Box 433; Harbin Institute of Technology; Harbin 150006. SUPERPLASTICITY IN A WARM-ROLLED Al-8Mg-0.2Zr ALLOY. Acta Metall Sin, 1992, 28(5): 93-94.
|
Abstract Superior superplasticity was revealed in a warm-rolled Al-8Mg-0.2Zr alloy at temperatureeven 325℃. Elongation up to 400% may be obtained under tension at constant strain rate 1×10~(-3)s~(-1), and ahigher elongation as high as 630% may be reached by two-stage strain rate.
|
Received: 18 May 1992
|
1 McNelley T R, Lee E-W, Mills M E. Metall Trans, 1986; 17A: 1035 2 Lee E-W, McNelley T R. Mater Sci Eng, 1987; 93: 45 3 Hales S J, McNelley T R. Acta Metall, 1988; 36: 1229 4 刘庆,黄晓旭,姚枚,杨金凤.金属学报,1991;27:B414 |
No Suggested Reading articles found! |
|
|