Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (6): 43-48    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF DYNAMIC STRAIN AGING ON LOW CYCLE FATIGUE BEHAVIOUR OF 18--8 AUSTENITIC STAINLESS STEEL
CHEN Wenzhe;QIAN Kuangwu Fuzhou UniversityPENG Kaiping;assistant;Department of Mechanical Engineering;Fuzhou University Fuzhou 350002
Cite this article: 

CHEN Wenzhe;QIAN Kuangwu Fuzhou UniversityPENG Kaiping;assistant;Department of Mechanical Engineering;Fuzhou University Fuzhou 350002. EFFECT OF DYNAMIC STRAIN AGING ON LOW CYCLE FATIGUE BEHAVIOUR OF 18--8 AUSTENITIC STAINLESS STEEL. Acta Metall Sin, 1993, 29(6): 43-48.

Download:  PDF(1570KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the symmetric tensile-compressive low cyclic fatiguebehaviour and dynamic strain aging (DSA) pre-treatment influenced on 18-8 austeniticstainless steel. Within the tested amplitude range of strain: ±0.5%-±1.5%, the three pro-cesses of cyclic hardening, cyclic saturation and cyclic softening were observed. In the sameamplitude of strain, the peak stress of the samples pre-treated by DSA is higher than that ofsolid-solution and cold working pre-treatment, but almost no differences of the fatigue livesof them were found. TEM observation shows that the uniform and stable dislocation net-works with high density form after DSA pre-treatment, which increases the cyclic peak stress.The cyclic softening is resulted from the low dislocation density and elongated cell structurewith low energy.
Key words:  18-8 austenitic stainless steel      dynamic strain aging      low cycle fatigue     
Received:  18 June 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I6/43

1 QIAN Kuangwu, CHEN Wenzhe, XIAO Lingang, NI Chaofang. Proc 8th Int Conf on Strength of Metals and Alloys, Vol. 2, Tampere, Finland, 22--26, August. 1988, Pergamon Press, 1988: 1251
2 陈文哲,钱匡武.金属科学与工艺,1989;8:1
3 陈文哲,钱匡武.金属学报,1989;25:A132
4 QIAN Kuangwu, PENG Kaiping, CHEN Wenzhe. Proc 6th Int. Conf on Mechanical Behavior of Materials (ICM-6) , Kyoto, Japan, 1991: 601
5 夏月波,王中光.金属学报,1989;25:A421
6 夏月波,王中光.第三届全国疲劳学术交流会,桂林,1986,1986;V4-1-1
7 王栓柱.金属疲劳.福州:福建科学技术出版社,1985:73
8 柴惠芬,汪立勤,Laird C.金属学报.1989;25:A201&
[1] Jinlan AN,Lei WANG,Yang LIU,Guohua XU,Guangpu ZHAO. INFLUENCES OF LONG-TERM AGING ON MICRO- STRUCTURE EVOLUTION AND LOW CYCLE FATIGUE BEHAVIOR OF GH4169 ALLOY[J]. 金属学报, 2015, 51(7): 835-843.
[2] GUO Pengcheng, QIAN Lihe, MENG Jiangying, ZHANG Fucheng. MONOTONIC TENSION AND TENSION-COMPRES- SION CYCLIC DEFORMATION BEHAVIORS OF HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. 金属学报, 2014, 50(4): 415-422.
[3] CAI Yulong, FU Shihua, WANG Yuhui, TIAN Chenggang, GAO Yue, CHENG Teng, ZHANG Qingchuan. SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION[J]. 金属学报, 2014, 50(12): 1491-1497.
[4] YU Huichen, DONG Chengli, JIAO Zehui, KONG Fantao, CHEN Yuyong, SU Yongjun. HIGH TEMPERATURE CREEP AND FATIGUE BEHAVIOR AND LIFE PREDICTION METHOD  OF A TiAl ALLOY[J]. 金属学报, 2013, 49(11): 1311-1317.
[5] HAN Guoming, CUI Chuanyong, GU Yuefeng, HU Zhuangqi, SUN Xiaofeng. INVESTIGATION OF TEMPERATURE DEPENDENCE OF PLC EFFECT IN A NICKEL BASE SUPERALLOY[J]. 金属学报, 2013, 49(10): 1243-1247.
[6] FU Shihua CHENG Teng ZHANG Qingchuan CAO Pengtao HU Qi. STUDY ON TWO CRITICAL MECHANISMS OF PLC EFFECT OF 5456 Al–BASED ALLOY[J]. 金属学报, 2012, 48(12): 1453-1458.
[7] JIANG Huifeng CHEN Xuedong FAN Zhichao DONG Jie JIANG Heng LU Shouxiang. EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2009, 45(3): 326-330.
[8] HUANG Zhiwei; YUAN Fuhe; WANG Zhongguang; ZHU Shijie; WANG Fugang. Low Cycle Fatigue Behavior of A Cast Nickel Base Superalloy M963 at Elevated Temperature[J]. 金属学报, 2007, 43(7): 678-682 .
[9] . [J]. 金属学报, 2007, 43(10): 1025-1030 .
[10] Chen Ling. Discussion of energy model for low cycle fatigue life prediction[J]. 金属学报, 2006, 42(2): 195-200 .
[11] Cong Wang. PORTEVIN-LE CHATELIER EFFECT OF LA41 MAGNESIUM ALLOYS[J]. 金属学报, 2006, 42(2): 191-194 .
[12] . The Effect of Solute Concentration by Solution Treatment on Portevin-Le Chatelier effect in Al-Cu Alloys[J]. 金属学报, 2006, 42(12): 1248-1252 .
[13] JIANG Huifeng; ZHANG Qingchuan; JIANG Zhenyu; WU Xiaoping. Experimental Investigations on the Temporal and Spatial Behaviors of the PLC Effect in Al--Cu Alloys[J]. 金属学报, 2005, 41(7): 727-732 .
[14] YAO Jun; GUO Jianting; YUAN Chao; LI Zhijun. Low Cycle Fatigue Behavior Of Cast Nickel Base Superalloy K52[J]. 金属学报, 2005, 41(4): 357-362 .
[15] YU Huichen; SUN Yanguo; XIE Shishu; K. TANAKA. Low Cycle Fatigue Crack Propagation in Stainless Steel Under Combined Torsion and Tension[J]. 金属学报, 2005, 41(1): 73-.
No Suggested Reading articles found!