| EFFECT OF DYNAMIC STRAIN AGING ON LOW CYCLE FATIGUE BEHAVIOUR OF 18--8 AUSTENITIC STAINLESS STEEL |
| CHEN Wenzhe;QIAN Kuangwu Fuzhou UniversityPENG Kaiping;assistant;Department of Mechanical Engineering;Fuzhou University Fuzhou 350002 |
|
Cite this article:
CHEN Wenzhe;QIAN Kuangwu Fuzhou UniversityPENG Kaiping;assistant;Department of Mechanical Engineering;Fuzhou University Fuzhou 350002. EFFECT OF DYNAMIC STRAIN AGING ON LOW CYCLE FATIGUE BEHAVIOUR OF 18--8 AUSTENITIC STAINLESS STEEL. Acta Metall Sin, 1993, 29(6): 43-48.
|
|
|
Abstract Studies were made of the symmetric tensile-compressive low cyclic fatiguebehaviour and dynamic strain aging (DSA) pre-treatment influenced on 18-8 austeniticstainless steel. Within the tested amplitude range of strain: ±0.5%-±1.5%, the three pro-cesses of cyclic hardening, cyclic saturation and cyclic softening were observed. In the sameamplitude of strain, the peak stress of the samples pre-treated by DSA is higher than that ofsolid-solution and cold working pre-treatment, but almost no differences of the fatigue livesof them were found. TEM observation shows that the uniform and stable dislocation net-works with high density form after DSA pre-treatment, which increases the cyclic peak stress.The cyclic softening is resulted from the low dislocation density and elongated cell structurewith low energy.
|
|
Received: 18 June 1993
|
1 QIAN Kuangwu, CHEN Wenzhe, XIAO Lingang, NI Chaofang. Proc 8th Int Conf on Strength of Metals and Alloys, Vol. 2, Tampere, Finland, 22--26, August. 1988, Pergamon Press, 1988: 1251 2 陈文哲,钱匡武.金属科学与工艺,1989;8:1 3 陈文哲,钱匡武.金属学报,1989;25:A132 4 QIAN Kuangwu, PENG Kaiping, CHEN Wenzhe. Proc 6th Int. Conf on Mechanical Behavior of Materials (ICM-6) , Kyoto, Japan, 1991: 601 5 夏月波,王中光.金属学报,1989;25:A421 6 夏月波,王中光.第三届全国疲劳学术交流会,桂林,1986,1986;V4-1-1 7 王栓柱.金属疲劳.福州:福建科学技术出版社,1985:73 8 柴惠芬,汪立勤,Laird C.金属学报.1989;25:A201& |