Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (6): 38-42    DOI:
Current Issue | Archive | Adv Search |
REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS
CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015
Cite this article: 

CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015. REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS. Acta Metall Sin, 1993, 29(6): 38-42.

Download:  PDF(835KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Changes of fatigue crack growth rate, dα/dN, at affecting region of eitherplastic or elastic shock wave have been studied with three-point bending specimens made oflow alloy steel 16Mn. The dα/dN at whole affecting regions by shock wave, about 100 mmdepth, is significantly reduced, especially at the plastic wave affecting region. Thedα/dN keeps basically constant at pure elastic wave affecting region under same ΔK. It isconsidered that the decrease of effective stress intensity factor ΔK_(eff) of the material with crackclosure effect is the main reason for reducing dα/dN after shock wave treatment. At plasticwave affecting region, crack closure occurs mainly through plastic deformations at crack tipand oxides; at elastic wave affecting region, through plastic deformations and roughness.
Key words:  steel 16Mn      shock wave      fatigue crack growgh rate     
Received:  18 June 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I6/38

1 高桦.固体力学学报,1987;(2) :164
2 斯重遥,陈亮山,刘易军.第6届全国焊接学术会议论文集,西安,1990
3 陈怀宁,陈亮山,斯重遥.第5届沈阳市焊接学术会议论文集.1991
4 北京工业学院.爆炸及其作用下册.北京:国防工业出版社,1979:180
5 赵铁民,陈亮山,陈怀宁.斯重遥.第七届全国焊接学术会议论文集,青岛,1993<
[1] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[2] FENG Aixin NIE Guifeng XUE Wei CAO Yupeng XU Xiaoxiang LI Bin SHI Fen . EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET[J]. 金属学报, 2012, 48(2): 205-210.
[3] LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04). CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE[J]. 金属学报, 1996, 32(8): 862-866.
[4] CHEN Liangshan; ZHAO Tiemin ;SI Zhongyao (Institute of Metal Research;Chinese Academy of Sciences; Shenyang)(Manuscript received 18 November;1993; in revised form 21 January;1994). EFFECT OF REFLECTED TENSION SHOCK WAVE ON MICROSTRUCTURE AND FATIGUE PROPERTY OF 16Mn STEEL WELD[J]. 金属学报, 1994, 30(23): 519-523.
[5] ZHAO Tiemin;CHEN Liangshan;SI Zhongyao(Institute of Metal Research;Chinese Academy of Scicnces; Shenyang);TAN Shengyu;CUI Guangyuan (ShenyangInstitute of Artillery). EFFECT OF EXPLOSION SHOCK WAVE INTENSITY ON DISLOCATION STRUCTURE IN FERRITE OF STEEL 16Mn WELD[J]. 金属学报, 1994, 30(15): 130-135.
[6] PENG Xianghe;GAO Zhihui;MA Mingtu;YAN Zaixian Chongqing University Chongqing Institute of Automobile. NONPROPORTIONAL CYCLIC PLASTICITY OF NORMALIZED STEEL 16Mn[J]. 金属学报, 1993, 29(10): 1-9.
[7] WANG Weiming; HUANG Yuhua; XU Hao (Northeast University of Technology; Shenyang). PROPAGATION OF FATIGUE SHORT CRACKS IN STEEL 16Mn[J]. 金属学报, 1992, 28(9): 42-46.
[8] GAO Juxian;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EFFECT OF EXPLOSIVE CONSOLIDATION PARAMETERS ON CONSOLIDATION QUALITY[J]. 金属学报, 1990, 26(6): 159-161.
[9] GAO Juxian;SHAO Binghuang;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EXPLOSIVE CONSOLIDATION OF METAL UNDER CYLINDRICAL CONVERGING SHOCK WAVE[J]. 金属学报, 1990, 26(5): 125-130.
No Suggested Reading articles found!