Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (15): 140-144    DOI:
Current Issue | Archive | Adv Search |
ULTRA-MICROHARDNESS OF N~+ IMPLANTED LAYER ON 1Cr18Ni9TiSTAINLESS STEEL
YANG Anjing;CAI Yiwei;CHEN Qiulong(Shanghai Jiaotong University)
Cite this article: 

YANG Anjing;CAI Yiwei;CHEN Qiulong(Shanghai Jiaotong University). ULTRA-MICROHARDNESS OF N~+ IMPLANTED LAYER ON 1Cr18Ni9TiSTAINLESS STEEL. Acta Metall Sin, 1994, 30(15): 140-144.

Download:  PDF(318KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An ultra-microhardness tester typed UMHT-3 was used to measure the characteristic hardness of N+ implanted layer on 1Cr18Ni9Ti stainless steel.Depth and nitrogen concentration profile of the N+ implanted layer were determined by means of AES in combination with high precision profilometer. The depth of N+ implanted layer in 1Cr18Ni9Ti steel is 0.18μm at 90 keV and 3x10~17 N+/cm2. Its characteristic hardness,HV 3.47 GPa under load of l mN, shows that N+ implantation can increase the surface hardness by more than 3 times. The appropriate testing load selected should be equal or less than l mN.
Key words:  1Cr18Ni9Ti      ion implantation      ultra-microhardness     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I15/140

1JonssonB,HogmarkS.ThinSolidFilms,1984:114:2572OnateJC,DennisJK,HamiltonS.HeatTreatMet.1987;14(3):7
[1] LIU Yi, JIANG Guofeng, XU Kun, LUO Ximing, CHEN Dengquan, LI Wei. EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING[J]. 金属学报, 2015, 51(2): 209-215.
[2] HUANG Yuan KONG Deyue HE Fang WANG Yulin LIU Wenxi. PREPARATION OF Mo/Ag LAMINAR COMPOSITES BY USING IRRADIATION DAMAGE ALLOYING METHOD[J]. 金属学报, 2012, 48(10): 1253-1259.
[3] LEI Mingkai WANG Kesheng OU Yi Xiang ZHANG Lei. PLASMA–BASED LOW–ENERGY NITROGEN ION IMPLANTATION OF 2Cr13 MARTENSITIC STAINLESS STEEL USED IN PUMPS AND VALVES[J]. 金属学报, 2011, 47(12): 1490-1494.
[4] LENG Chongyan ZHOU Rong ZHANG Xu LU Dehong LIU Hongxi . WEAR PERFORMANCE OF Ti6Al4V ALLOY MODIFIED BY Ag+Ta DUAL--ION IMPLANTATION[J]. 金属学报, 2009, 45(6): 764-768.
[5] LIU Hongxi; JIANG Yehua; ZHOU Rong; ZHOU Rongfeng; JIN Qinglin TANG Baoyin. ROLLING CONTACT FATIGUE LIFE AND MECHANICAL PROPERTY OF TiN FILM FABRICATED BY PLASMA IMMERSION ION IMPLANTATION[J]. 金属学报, 2008, 44(3): 325-330 .
[6] LIU Huiying WANG Xuejin WANG Langping WANG Xiaofeng AI Hongjun. INFLUENCE OF SURFACE MODIFICATION OF Ti BY FLUORINE ION-IMPLANTATION ON FORMATION AND EXPRESSION OF COLLAGEN-I ON OSTEOBLAST[J]. 金属学报, 2008, 44(12): 1485-1490.
[7] LIU Hongxi; WANG Langping; WANG Xiaofeng; HUANG Lei; TANG Baoyin. Effects of TiC Films on the Rolling Contact Fatigue Life and Mechanical Properties of Bearing Steel[J]. 金属学报, 2006, 42(11): 1197-1201 .
[8] CHEN Tao; CHANG Haiwei; LEI Mingkai. Surface Alloying Of Al Ion Implantation Into Fe Target At Elevated Temperature[J]. 金属学报, 2005, 41(4): 417-420 .
[9] CHANG Haiwei; CHEN Tao; LEI Mingkai. A Mathematical Model on Coalescence and Removal of Inclusion Particles in Continuous Casting Tundish[J]. 金属学报, 2004, 40(6): 629-.
[10] NIU Lin; CAO Chunan; LIN Haichao (State Key Laboratary for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: NIU Lin; Tel: (024)23915893; Fax: (094)23894149; E-mail: lin.h.c@icpm.syb.ac.cn. EFFECT OF POTENTIAL PERTURBATION POLARIZATION ON THE STRESS CORROSION CRACKING OF 1Cr18Ni9Ti STAINLESS STEEL[J]. 金属学报, 1998, 34(9): 959-965.
[11] PENG Xiao; PING Dehai; LI Tiefan; WU Weitao(State Key Laboratory for Corrosion and Protection; Insititute of Corrosion and Protection of Metals; Chinese Academ of Sciences; Shenyang 110015)(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1996-03-15). MICROSTRUCTURE OF OXIDE SCALE AND OXIDATION MECHANISM OF Y~+ IMPLANTED ALLOY Ni20Cr[J]. 金属学报, 1997, 33(4): 398-405.
[12] AN Chu; HEI Zukun(Dalian Maritime University; Dalian 116024)OKABE Yoshio (Sukitama University of Industy; Wako; Japan). IWAKI Masaya (The Institute of Physical and Chemical Research; Wako; Japan). COLOURING OF PURE IRON AFTER Ti~+-O~+ DUAL ION IMPLANTATION[J]. 金属学报, 1995, 31(15): 116-122.
[13] XU Jingyang;VAN BRUSSEL;B J;NOORDHUIS J;BRONSVELD P M;DE HOSSON J Th M Shanghai Institute of Metallurgy; Academia Sinica Department of Applied Physics; Materials Science Center; University of Groningen; The Netherlands. X-RAY DIFFRACTION DETERMINATION OF STRESS RELAX IN LASER MELTED AREA OF STAINLESS STEEL[J]. 金属学报, 1993, 29(9): 92-96.
[14] JIANG Bingyao;WANG Xi;SUN Jian;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia SinicaLIU Xianghuai;professor;Shanghai Institule of Metallurgy.Academia Siniea;Shanghai 20005. EFFECT OF Mg SEGREGATION AT GRAIN BOUNDARIES ON CORROSION BEHAVIOUR OF Ni_3Al(0.1B)[J]. 金属学报, 1993, 29(5): 87-91.
[15] CHEN Lifan; BA Tu; Sill Changxu (State key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang). EFFECTS OF B~+ IMPLANTATION ON MECHANICAL PROPERTIES AND MICROSTRUCTURE OF POLYCRYSTALLINE Ni[J]. 金属学报, 1992, 28(9): 17-24.
No Suggested Reading articles found!