SUPERPLASTIC WELDING OF FLAME SPRAYED NiFeCrBSi ALLOY COATING ON CrWMn STEEL
LI Yanxiang;WEN Jiuba;HUANG Jinfiang;ZHU Yaomin(Luoyang Instituteof Technology)
Cite this article: 

LI Yanxiang;WEN Jiuba;HUANG Jinfiang;ZHU Yaomin(Luoyang Instituteof Technology). SUPERPLASTIC WELDING OF FLAME SPRAYED NiFeCrBSi ALLOY COATING ON CrWMn STEEL. Acta Metall Sin, 1994, 30(15): 136-139.

Download:  PDF(361KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The compressive superplastic tests at constant temperature were carried out on flame sprayed NiFeCrBSi(G112)alloy coating on CrWMn steel.A section conversion method has been used to measure the values m at different temperatures. The optimum superplastic condition was determined by optimizing the strain rate ratio of flame sprayed coating and substrate under defomation.The welding effects of the porosities inside the deformed coating and the bonding interfaces between the coating and substrate at different deformation temperatures have been analysed. The influence of deformation conditions on the multiple impact failure behaviors of the superplastically deformed coatings have also been investigated. The results show that the porosities inside the coating and the bonding interface between the coating and the substrate can be effectively welded at the superplastic temperature range of the substrate steel CrWMn if the value W of strain rate ratio between the coating and the substrate are approximate to one and as a result a good multiple impact behaviour can be obtained.
Key words:  flame spray      bonding interface      superplastic welding      CrWMn steel      Gll2 alloy     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I15/136

1AC,刘春林译.金属与合金的超塑效应.北京:科学出版社,19832毛健,杨万宏,汪武祥,邹金文,周瑞发.金属学报,1993;29:A187
[1] XIE Hongbiao GAO Yanan WANG Tao XIAO Hong. EFFECT OF MULTIPASS HOT ROLLING ON THE PROPERTY AND BONDING INTERFACE OF CLAD BAR[J]. 金属学报, 2011, 47(12): 1513-1519.
[2] YA NG Yunlin; LI Zhi; LI Yan(LuoYang institute of TechnoLogy); Luoyang 471039)(Manuscript received 1994-08-31; in revised form 1995-03-31). FRACTURE ANALYSIS OF JOINT AFTER CONSTANT TEMPERATURE SUPERPLASTIC WELDING[J]. 金属学报, 1995, 31(20): 384-38.
[3] ZHAO Xiaopeng(Institute of Metal Research;Chinese Academy of Sciences;Shenyang;International Center for Materials Physics;Chinese Academy of Sciences;Shenyang);TIAN Hiaobin(Institute of Metal Research;Chinese Academy of Sciences;Shenyang);ZHOU Benlian(Institute of Metal Research;Chinese Academy of Sciences;Shenyang;International Center for Materials Physics;Chinese Academy of Sciences; Shenyang);LI Shihong(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 28 July 1993;in revised form 8 November 1993). A BIOMIMETIC MODEL OF SHORT FIBRE REINFORCED COMPOSITE MATERIALS──Ⅱ Strength Theory of Imperfect-Bonding Interface[J]. 金属学报, 1994, 30(16): 187-193.
[4] WEN Jiuba;XI Jukui Luoyang Institute of Technology. SUPERPLASTIC WELDING OF STEELS 40Cr-CrWMn[J]. 金属学报, 1993, 29(10): 92-96.
[5] LIN Chengfu;WEN Lishi;QIAN Shengwei;KANG Datao Institute of Metal Research; Academia Sinica; Shenyang Yanshang University Institute of Metal Research;Academia Sinica;Shenyang 110015. CORROSION FAILURE ANALYSIS OF FLAME SPRAYED Zn-Al15 COATING IN SEA WATER[J]. 金属学报, 1990, 26(2): 116-119.
No Suggested Reading articles found!