Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (18): 277-282    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMICAL CALCULATIONS OF INFLUENCES OF HOT-DEFORMATION ON A_(e3) FOR ALLOY STEELS
LIU Zhenyu; WANG Guodong; ZHANG Qiang;MA Longxiang(Northeastern University; Shenyang)
Cite this article: 

LIU Zhenyu; WANG Guodong; ZHANG Qiang;MA Longxiang(Northeastern University; Shenyang). THERMODYNAMICAL CALCULATIONS OF INFLUENCES OF HOT-DEFORMATION ON A_(e3) FOR ALLOY STEELS. Acta Metall Sin, 1994, 30(18): 277-282.

Download:  PDF(304KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the superelement model, the method to calculate Ae3 of hot-deformed Fe-ΣXi-C(Xi=Mn, Si, Mo, Al, Cu, Ni, Co, Cr etc) multicomponent alloy steels has been developed, and the influences of hot-deformation of γ-phase on Ae3 were analzed. The calculated Ae3 for nondeformed alloy steels are in good agreements with measured ones given by the previous works.
Key words:  hot-deformation      A_(e3)      superelement      model      alloy steel     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I18/277

1UmemotoM,TamuraI.ProcofIntConfofHSLASteel'85Beijing,1985:3732AnanGetal,ISIJInternational,1992:32:33AaronsonHI,DomionHA,PoundGM.TransofAIME,1966;236:7534徐祖耀,刘世楷.贝氏体相变与贝氏体.北京:科学出版社,19915ZenerC.TransAIME,1946;167:5136杨柳,刘世楷,杨萍.金属学报,1993;29:Al7AaronsonHI,DomianHA.TransAIME,1966;236:7818GrangeRA,MetalProgress,1961:203:739林慧国,傅代直.钢的奥氏体转变曲线.北京:机械工业出版社,1988
[1] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[2] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[3] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[4] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[5] ZHANG Zhidong. Exact Solution of Ferromagnetic Three-Dimensional (3D) Ising Model and Spontaneous Emerge of Time[J]. 金属学报, 2023, 59(4): 489-501.
[6] ZHU Zhihao, CHEN Zhipeng, LIU Tianyu, ZHANG Shuang, DONG Chuang, WANG Qing. Microstructure and Mechanical Properties of As-Cast Ti-Al-V Alloys with Different Proportion of α / β Clusters[J]. 金属学报, 2023, 59(12): 1581-1589.
[7] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[8] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[9] CHEN Huabin, CHEN Shanben. Key Information Perception and Control Strategy of Intellignet Welding Under Complex Scene[J]. 金属学报, 2022, 58(4): 541-550.
[10] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[11] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[12] LUO Wenze, HU Long, DENG Dean. Numerical Simulation and Development of Efficient Calculation Method for Residual Stress of SUS316 Saddle Tube-Pipe Joint[J]. 金属学报, 2022, 58(10): 1334-1348.
[13] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[14] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[15] XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan. Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. 金属学报, 2021, 57(6): 822-830.
No Suggested Reading articles found!