| ELECTRON THEORY STUDY OF ORDER-DISORDER TRANSFORMATIONS IN Fe-Al ALLOYS |
| ZHANG Jianmin; ZHANG Ruilin; YU Ruihuang(S. H. YU); ZHENG Weitao;HU Anguang (Jilin University; Changchun)(Manuscript received 5 April 1993; in revised form 9 August; 1993) |
|
Cite this article:
ZHANG Jianmin; ZHANG Ruilin; YU Ruihuang(S. H. YU); ZHENG Weitao;HU Anguang (Jilin University; Changchun)(Manuscript received 5 April 1993; in revised form 9 August; 1993). ELECTRON THEORY STUDY OF ORDER-DISORDER TRANSFORMATIONS IN Fe-Al ALLOYS. Acta Metall Sin, 1994, 30(5): 204-209.
|
|
|
Abstract According to the bond energy formula of the empirical electron theory of solids and molecules, the mechanism of order-disorder transformations is analysed from the results of the bond energy and the bond structures of the alloys. The Fe-Al binary alloys have an order-disorder transformation which is resulted in the change of numbers of covalent electron pair on bonds. Correspondent: ZHANG Jianmin, Department of Materials Scicnce, Institute of Materiurs Science, Jilin University, Changchun 130023
|
|
Received: 18 May 1994
|
| 1BradleyAJ,JayAH.ProcRSoc,1932;A136:2102BradleyAJ,JayAH.JIronSteelInst,1932;125:3393McQueenHJ,KuczynskiGC.TransMetallSocAIME,1959;215:6194LesoilleMRetal.TheMechanismofPhaseTransformationsinCrystallineSolids,MonographandReportSeries,London;1969;33:2235QkiKetal.,JpnJAppPhys,1973;10:15226TaylorA,JonesRM.JPhysChemSolids,1958;6:167余瑞璜.吉林大学自然科学学报,1979;4:548余瑞璜.金属学报,1982;3:336< |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|