Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (11): 513-518    DOI:
Current Issue | Archive | Adv Search |
CYCLIC DEFORMATION BEHAVIOUR OF Ni_3(Al,Zr) SINGLE CRYSTAL AT ROOM TEMPERATURE
GU Yuefeng;LIU Yi;LIN Dongliang(T.L.Lin)(Shanghai Jiaotong University;Shanghai 200030);GUO Jianting(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-01-13;in revised form 1995-07-03)
Cite this article: 

GU Yuefeng;LIU Yi;LIN Dongliang(T.L.Lin)(Shanghai Jiaotong University;Shanghai 200030);GUO Jianting(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-01-13;in revised form 1995-07-03). CYCLIC DEFORMATION BEHAVIOUR OF Ni_3(Al,Zr) SINGLE CRYSTAL AT ROOM TEMPERATURE. Acta Metall Sin, 1995, 31(11): 513-518.

Download:  PDF(464KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fully reversed strain-controlled tension-compression tests were performed at room temperature to study cyclic-deformation properties of Ni_3(Al,Zr) single crystal.Both cyclic strain hardening and a tension-compression flow stress asymmetry were recorded,the stress asymmetry becomes more prominent as the strain amplitude becomes larger;the cyclic hardening can divide into initiation and saturation stages.TEM observation showed that there are a profusion superlattic intrinsic stacking faults(SISFs) in fatigued Ni_3(Al,Zr) single crystal samples.The cyclic strain hardening is explained by the dislocation structure.
Key words:  Ni_3(Al      Zr)      cyclic deformation      tension-compression stress      hardening     
Received:  18 November 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I11/513

1GuardKW,WestbrookJH,TransAIME,1959;215:8072Noguchi,OyaY,SuzukiT.MetallTrans,1981;12A:16473EzzSS,PopeDP.ScrMetall,1985;19:7414BondaNR,PopeDP,LairdC,ActaMetall,1987;35:23715BondaNR,PopeDP,LairdC.ActaMetall,1987;35:23856HsiungLM,StoloffNS.ActaMetallMater,1990;38:11917谷月峰.上海交通大学博士学位论文,上海,19948TakeuchiS,KuramotoE,YamamotoT,TaokaT.JpnJApplPhys,1973;12:4869BakerI,SchulsonEM.PhysStatusSolid,1985;a89:16310YanW,JonesIP,SmallmanRE.PhysStatusSolid,1991;a125:46911ChibaA,HanadaS.PhilosMag,1994;A69:75112MughrabiH,WuthrichC.PhilosMag,1976;A33:96313PakHR,HsiungLM,KatoM.In:KochCC,LiuCT,StoloffNSeds.,HighTemperatureOrderIntermetallicAlloy,Vol.39,Pittsburgh,PA:MRS,1985:23914LallC,ChinS,PopeDP.MetallTrans,1979;10A:132315PlcquerasJ,GrosskreutzJC,FrankW.PhysStatusSolid,1972;a11:56716BauschingerJ.Civilingenieur,1981;27:28917YamaguchiM,PaidarV,PopeDP,VitekV.PhilosMag,1982;45:86718PaidarV,YamaguchiM,PopeDP,VitekV.PhilosMag,1982;45:883
[1] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[2] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[3] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[4] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[5] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[6] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[7] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[8] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[9] WU Xiaolei, ZHU Yuntian. Heterostructured Metallic Materials: Plastic Deformation and Strain Hardening[J]. 金属学报, 2022, 58(11): 1349-1359.
[10] ZHAO Yonghao, MAO Qingzhong. Toughening of Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1385-1398.
[11] LI Suo, CHEN Weiqi, HU Long, DENG Dean. Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint[J]. 金属学报, 2021, 57(12): 1653-1666.
[12] LIU Jizhao, HUANG Hefei, ZHU Zhenbo, LIU Awen, LI Yan. Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation[J]. 金属学报, 2020, 56(5): 753-759.
[13] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[14] Miao JIN, Wenquan LI, Shuo HAO, Ruixue MEI, Na LI, Lei CHEN. Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. 金属学报, 2019, 55(4): 436-444.
[15] CHEN Lei, HAO Shuo, ZOU Zongyuan, HAN Shuting, ZHANG Rongqiang, GUO Baofeng. Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation[J]. 金属学报, 2019, 55(12): 1495-1502.
No Suggested Reading articles found!