ON THE COMPOSITE AND INTRINSIC HARDNESS OF Ti(C, N) FILMS
XU Kewei; BAI Chendong; HE Jiawen (State Key; Laboratory for Mechanical Behaviour of Materials; Hi'an Jiaotong University;Xi'an 710049)(Manuscript received 1994-08-23; in revised form 1995-01-26)
Cite this article: 

XU Kewei; BAI Chendong; HE Jiawen (State Key; Laboratory for Mechanical Behaviour of Materials; Hi'an Jiaotong University;Xi'an 710049)(Manuscript received 1994-08-23; in revised form 1995-01-26). ON THE COMPOSITE AND INTRINSIC HARDNESS OF Ti(C, N) FILMS. Acta Metall Sin, 1995, 31(21): 429-434.

Download:  PDF(429KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The model proposed by Joensson and Hogmark takes the parameter, C, as a constant for different film-substrate systems. The parameter was modified in the present paper according to different hardness ratio of film to substrate and used them to study the variation of the hardness of PCVD Ti(C, N) films with the composition and the microstructure.Comparing with bulk materials, Ti(C, N) films have a relative high hardness due to the smaller crystal size and the higher compressive residual stress. It is controlled by the carbon content and hold a linear increase with the carbon content for a definite deposition technique.Correspondent:(XU Kewei, professor, Hi'an Jiaotong University, Hi'an 710049)
Key words:  Ti(C      N) film      composite hardness      intrinsic hardness     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I21/429

1BueckleH.In:WestbrookJH,ConradH,eds.,ScienceofHardnessTestinganditsResearchApplications,MetalsPark,Ohio:ASM,1973.4532ValvodaV,CernyR,KuzelRJr.ThinSolidFilms,1988:158:2253DoernerMF,NixWD.JMaterRes.1986;1,6014WollenbergRL,PinchHL.In:ShielsSA,BagnallC,WitkowskiRE,VanderCFCoort.cds.,MicrostructuralScience,1987;13:175VingsboO,HogmarkS,JoenssonB,IngemarssonA.ASTMSTP889,1984:2576李恒德,肖纪美.材料的表面与界面,北京:清华大学出版社,19907TamuraM,KuboH.SurfCoatTechnol,1991;49:1948ThomasASurfaceEngineering,1987;3(2):1179PiviereJ,DelafondJ.SurfaceEngineering,1993;9(1):5910HedenqvistP,OlssonM,HogmarkS.SurfaceEngineering,1992;8(1):3911JoenssonB,HogmarksThinSolidFilms,1984;114:25712李世直,石玉龙,徐翔,赵程.薄膜科学与技术,1989;2(2):7013GeorgeUO.ExperimentalMechanics,1964;21(1):13514HuangRF,WenLS,GuoLPGongJ,YuBN,SurfCoatTechnol,1992;50:97(
[1] Mingfang WU,Fei LIU,Fengjiang WANG,Yanxin QIAO. INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT[J]. 金属学报, 2015, 51(9): 1129-1135.
[2] WU Mingfang, KUANG Hongjin, WANG Fengjiang, LIN Hongxiang, XU Guoxiang. PARTIALLY TRANSIENT LIQUID PHASE-DIFFUSION BONDING ON Ti(C, N)-Al2O3 CERAMIC MATRIX COMPOSITES USING Zr/Cu/Zr AS INTERLAYER[J]. 金属学报, 2014, 50(5): 619-625.
[3] ;. Preparation of Ti(CxN1-x) thick films on titanium by plasma electrolytic carbonitriding[J]. 金属学报, 2008, 44(9): 1105-1110 .
[4] LIU Hongxi; JIANG Yehua; ZHOU Rong; ZHOU Rongfeng; JIN Qinglin TANG Baoyin. ROLLING CONTACT FATIGUE LIFE AND MECHANICAL PROPERTY OF TiN FILM FABRICATED BY PLASMA IMMERSION ION IMPLANTATION[J]. 金属学报, 2008, 44(3): 325-330 .
[5] WANG Quanzhao; LIU Yue; GUAN Dehui; YU Baohai; CHEN Zhiliang; BI Jing. Effect of tin content on microstructures and mechanical properties of Ti(C,N)/NiCr cermets[J]. 金属学报, 2005, 41(11): 1121-1126 .
[6] XIONG Weihao;HU Zhenhua;CUI Kun (State Key Laboratory of Dies Technology;Huazhong University of Science and Technology; Wuhan 430074). FORMATION MECHANISM OF MICROCRYSTAL INTERFACE LAYER IN Ti(C, N)-BASED CERMET[J]. 金属学报, 1997, 33(5): 473-478.
[7] XIONG Weihao;HU Zhenhua;CUI Kun(State Key;Laboratory;of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(State Key Laboratory of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(Manuscript received 1996-04-26). TRANSITIONAL LAYER OF PHASE INTERFACES IN Ti(C,N)-BASED CERMET[J]. 金属学报, 1996, 32(10): 1075-1080.
[8] LIU Ning; ZHAO Hingzhong; JIANG Laizhu; LUO Huiguo; HU Zhenhua; CUI Kun(Huazhong University of Science and Technology; Wuhan 430074). TRANSVERSE RUPTURE STRENGTH OF Ni BONDED Ti(C, N) CERMET AND FRACTAL DIMENSION ANALYSIS OF ITS FRACTURE SURFACES[J]. 金属学报, 1995, 31(5): 229-235.
[9] DU Hegui;DU Gang Northeast University of Technology; Shenyang. ON THE FORMATION OF Ti(C, N) IN BLAST FURNACE[J]. 金属学报, 1991, 27(3): 89-94.
No Suggested Reading articles found!