Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (22): 440-444    DOI:
Current Issue | Archive | Adv Search |
EFFECTS OF PHASE STRUCTURES OF TiNi ON THE ELECTROCHEMICAL PROPERTIES
WANG Chunsheng; (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027) LEI Yongquan; YANG Xiaoguang; JIANG Jianjun; WU Jing;WANG Qidong (Zhejiang University; Hangzhou; 310027)
Cite this article: 

WANG Chunsheng; (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027) LEI Yongquan; YANG Xiaoguang; JIANG Jianjun; WU Jing;WANG Qidong (Zhejiang University; Hangzhou; 310027). EFFECTS OF PHASE STRUCTURES OF TiNi ON THE ELECTROCHEMICAL PROPERTIES. Acta Metall Sin, 1995, 31(22): 440-444.

Download:  PDF(312KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of two different phase structures of TiNi on its electrochemical properties were studied. By utilizing the transformation hysteresis, both TiNi samples with austenite and martensite structure were prepared and tested at the same temperature. The former has better kinetic properties than the later. In this paper the effect of hydrogen dissolved in the alloy to form solid solution on phase transformation temperature was also investigated with the electric resistance method.
Key words:  TiNi alloy      phase structure      electrochemical property     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I22/440

1JustiEW,EweHH,KalberlanAW,SaridakisNM.EnergyConvers,1970,10:1832WakaoS,SawaH,NakanoH,Chubachis,AbeM,JLess-CommonMet,1987;13:3113NamTH,ShimizuK,SaburiT,NennoS.MaterTransJIM,1989;30:5394MurataT,KoshiroK.GSNews,1991;50:215舟久保熙康编,千东范译.形状记忆合金.北京:机械工业出版社,1992:836ShorshorovMK,StepanovI,FlomenblitYM,TravkinVV.PhysMetMetallogr,1985;60(2):1097WillemsJJG.PhilipsJRes,1984,39(1):18周作祥,何春红,王正平,王春明.物理化学学报,1992;8(4):5589王春生.浙江大学博士学位论文,199510FruchartD,SoubeyrousJL,MiragliaS,ObbadeS,LorthioirG,BasileF,ColinC,FaudotF,OchinP,DezellusA.ZPhysChem,1993;5:225f
[1] Jiangang NIU, Wei XIAO. The Lattice Instability Induced by Ti-Site Ni in B2 Austenite in TiNi Alloy[J]. 金属学报, 2019, 55(2): 267-273.
[2] YANG Chenggong, SHAN Jiguo, REN Jialie. PHASE TRANSFORMATION TEMPERATURE CONTROL OF WELD METAL OF LASER WELDED TiNi SHAPE MEMORY ALLOY JOINT[J]. 金属学报, 2013, 49(2): 199-206.
[3] YANG Chenggong, SHAN Jiguo, REN Jialie. STUDY ON SHAPE RECOVERY TEMPERATURE OF TiNi ALLOY LASER WELD JOINT[J]. 金属学报, 2012, 48(5): 513-518.
[4] ZHANG Zhiqiang DONG Limin YANG Yang GUAN Shaoxuan LIU Yuyin YANG Rui. INFLUENCES OF QUENCHING TEMPERATURE ON THE MICROSTRUCTURE AND DEFORMATION BEHAVIORS OF TC16 TITANIUM ALLOY[J]. 金属学报, 2011, 47(10): 1257-1262.
[5] LV Dongsheng; LI Weishan; TAN Chunlin; ZE Ronghua. PREPARATION AND ELECTROCHEMICAL BEHAVIORS OF Co-B ALLOY POWDERS[J]. 金属学报, 2010, 46(3): 346-351.
[6] LIANG Yonghuang MAN Ruilin. PREPARATION AND CHARACTERIZATION OF ORGANIC HYBRID FILMS ON THE SURFACE OF Al TUBES[J]. 金属学报, 2010, 46(12): 1522-1528.
[7] ZHENG Bin ZHOU Wei WANG Yinong QI Min. MARTENSITE TRANSFORMATION IN TiNi ALLOY UNDER COUPLING TEMPERATURE AND HIGH MAGNETIC FIELD USING LANDAU THEORY MODEL[J]. 金属学报, 2009, 45(1): 37-42.
[8] GAO Fang; JIANG Chengbao; LIU Jinghua; XU Huibin. Effects of the Third Element Additions on Phase Constitution and Magnetostriction of Fe--Ga Alloys[J]. 金属学报, 2007, 43(7): 683-687 .
[9] . Phase Structure and Magnetostriction of B element doped[J]. 金属学报, 2006, 42(8): 830-834 .
[10] ZHENG Yanjun; CUI Lishan. Temperature Memory Effect of Partial Transformation in TiNi Alloys[J]. 金属学报, 2004, 40(9): 915-919 .
[11] LI Chuanjian;WANG Xinlin; LI Xiumei; WANG Chongyu (Advanced Materials Institute; Central Iron & Steel Research Institute; Beliing 100081). THE EFFECT OF CAST RATE ON THE ELECTROCHEMICAL PROPERTIES OF Ml(NiCoMnTi)_5 HYDROGEN STORAGE ALLOY[J]. 金属学报, 1998, 34(3): 288-292.
[12] XIE Guoqiang; CHU Fengmin. YANG Jilian; LI Wendan; ZHANG Baisheng (China Institute of Atomic Energy; P. O.Box 275(51); BeiJing 102413) (Manuscript received 1996-09-09; in revised form 1996- 11 -22). MARTENSITE IN U-10%Zr ALLOY[J]. 金属学报, 1997, 33(8): 785-790.
[13] JIANG Jianjun (Huazhong University of Science and Technology; Wuhan 430074); LEI YOngquan;SUN Dalin;WU Jing;WANG Qidong (Zhejiang University; Hangzhou 310027). EVALUATION AND ANALYSIS OF THE ELECTROCHEMICAL CAPACITY OF METAL HYDRIDE ELECTRODE USING HYDROGEN STORAGE ALLOYS IN ALKALINE AQUEOUS SOLUTION[J]. 金属学报, 1997, 33(7): 729-736.
[14] HE Zhirong(Shaanxi Institute of Technology; Hanzhong 723003); MIYAZAKI Shuichi (University of Tsukuba; Tsukuba; Japan) (Manuscript received 1995-09-11; in revised form 1995-11-22). EFFECT OF Ni CONTENT ON TRANSFORMATION BEHAVIOUR OF TiNi SHAPE MEMORY ALLOYS[J]. 金属学报, 1996, 32(4): 351-356.
[15] JIANG Jianjun(Huazhong University of Science and Technotogy; Wuhan 430074).LEI Yongquan; SUN Dalin; WANG Chunsheng; WU Jing; WANG Qidong(ZhejiangUniversity; Hangzhou 310027)(Manuscript received 1994-11-08; in revised form 1995-04-24). INFLUENCE OF RARE EARTH COMPOSITION ON ELECTROCHEMICAL PROPERTIES OF RE(NiCoMnTi)_5 HYDROGEN STORAGE ALLOYS[J]. 金属学报, 1995, 31(20): 379-383.
No Suggested Reading articles found!