Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (22): 445-450    DOI:
Current Issue | Archive | Adv Search |
ELECTROCHEMICAL BEHAVIOUR FOR REDUCTION OF Tm~(3+) IN MOLTEN CHLORIDES
YANG Qiqin; (Department of Chemistry; Zhongshan University; Guangzhou 510275) QIU Kairong; LIU Guankun; GUAN Tong(Zhongshan University;Guangzhou 510275)
Cite this article: 

YANG Qiqin; (Department of Chemistry; Zhongshan University; Guangzhou 510275) QIU Kairong; LIU Guankun; GUAN Tong(Zhongshan University;Guangzhou 510275). ELECTROCHEMICAL BEHAVIOUR FOR REDUCTION OF Tm~(3+) IN MOLTEN CHLORIDES. Acta Metall Sin, 1995, 31(22): 445-450.

Download:  PDF(365KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrode processes of Tm3+ in molten chlorides were investigated by cyclic voltammetry, open circuit potential-time curve after potentiostatic electrolysis and X-ray diffraction. Tm3+ is reduced to Tm2+ at first and then the metallic Tm is deposited on the W and Mo electrode respectively. The Tm-Ni alloys are formed at first and then the metallic Tm is deposited on Ni electrode. The diffusion coefficient and diffusion activation energy of Tm3+ in molten chlorides were determined. InD=-4.35-58.2x10~3 /RT is obtained.
Key words:  electroreduction of Tm~(3+)      molten chlorides      electrode process      diffusion coefficient      Tm-Ni alloy     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I22/445

1JohnsonKE,MackenzieJR.JElectrochemSoc,1969;116:17032GilberB,DenarteauV,DuyckaertsG.JElectroanalChem,1978;89:1233FlengasSN,InrgahamTR,JElectrochemSoc,1959;106:7144MamantovG,ManningDL,DaleJM,JElectroanalChem,1965;9:2535BardAJ,FaulknerLR.ElectrochemicalMethods.NewYork:JohnWiley&Sons,1980:218,2196章复中,谷力军.稀土,1982;(1):52D
[1] Yuanrong LIU,Weimin CHEN,Ying TANG,Yong DU,Lijun ZHANG. APPLICATION OF PRAGMATIC NUMERICAL INVERSE METHOD IN COMPUTATION OF INTERDIFFUSION COEFFICIENTS IN Al TERNARY ALLOYS[J]. 金属学报, 2016, 52(8): 1009-1016.
[2] Zujiang HUANG, Min ZHOU, Yang YANG, Quanzhi CHEN, Shiguang TANG, Weizhou LI. STUDY OF ANODIC ALUMINUM OXIDE FILM AS AN INTERLAYER TO SUPPRESS ELEMENT DIFFUSION[J]. 金属学报, 2016, 52(3): 341-348.
[3] ZHANG Jinling1,2,3, FENG Zhiyong1, HU Lanqing1,2,3,WANG Shebin1,2,3, XU Bingshe1,2,3. PRECIPITATION BEHAVIOR OF AZ91 MAGNESIUM ALLOYS WITH DIFFERENT La CONTENTS[J]. 金属学报, 2012, 48(5): 607-614.
[4] . PHASE FIELD SIMULATION OF SINTERING PROCESS IN BIPHASIC POROUS MATERIAL[J]. 金属学报, 2012, 48(10): 1207-1214.
[5] CHEN Yexin CHANG Qinggang. EFFECT OF TRAPS ON DIFFUSIVITY OF HYDROGEN IN 20g CLEAN STEEL[J]. 金属学报, 2011, 47(5): 548-552.
[6] . The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel[J]. 金属学报, 2007, 43(8): 785-790 .
[7] LIU Shi; ZHENG Hua; GUI Quanhong; MA Aihua; YU Hongbo; WANG Longbao. MEASUREMENTS OF HYDROGEN DIFFUSION COEFFICIENT FOR TUBE SAMPLES AT MEDIUM AND HIGH TEMPERATURES[J]. 金属学报, 2004, 40(4): 393-398 .
[8] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[9] WANG Wendong; ZHANG Sanhong; HE Xinlai(University of Science and Technology Beijing; 100083)(Manuscript received 93-09-21. in revised form 94-01-26). DIFFUSION OF BORON IN Fe-BASE AND Ni-BASE ALLOYS[J]. 金属学报, 1995, 31(2): 56-63.
[10] WU Zhichun Institute of Chemical Metallurgy; Academia Sinica; Beijing. DETERMINATION OF DIFFUSION COEFFICIENT OF CuCl_2 IN AQUEOUS SOLUTIONS[J]. 金属学报, 1991, 27(4): 93-99.
[11] ZHU Xiaohe;YU Yongning University of Science and Technology Beijing. DIFFUSION COEFFICIENTS IN α(δ)-PHASE OF Fe-Mn-Si TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1991, 27(3): 106-110.
[12] YANG Zhen'guo;DU Weixi;DU Senlin;LIU Sulan Jilin University of Technology; Changchun Changchun Institute of Applied Chemistry; Academia Sinica. DIFFUSION OF La IN LIQUID Al-Si ALLOY[J]. 金属学报, 1989, 25(2): 104-108.
No Suggested Reading articles found!