| Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel |
HAN Ruyang1, YANG Gengwei1( ), SUN Xinjun2, ZHAO Gang1, LIANG Xiaokai2, ZHU Xiaoxiang1 |
1.State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China 2.Department of Structrual Steels, Central Iron and Steel Research Institute, Beijing 100053, China |
|
Cite this article:
HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel. Acta Metall Sin, 2022, 58(12): 1589-1599.
|
|
|
Abstract Medium manganese martensitic wear-resistant steel is a new type of wear-resistant steel with high hardenability and hardness; moreover, the controlling austenite grain size is of great significance for improving its comprehensive properties. In this study, the austenite growth behavior of vanadium microalloying medium manganese martensitic wear-resistant steel was systematically investigated using the Gleeble-3500 thermal simulation testing machine, OM, and HRTEM. The morphology, size, and particle size distribution of the second phase particles at different heating temperatures and holding times were analyzed. The influence of second phase particles on the growth behavior in austenite was also revealed. The results showed that the ultra-fine austenite grains with grain size of 3.98 μm were obtained when the sample was held at 820oC for 10 s. After holding for 3600 s, the average grain size of austenite only increased by 1.47 μm, and the austenite grains showed a strong ability to resist coarsening at 820oC. This could be attributed to the fine V(C, N) particles which could pin the austenite grain boundary and inhibit the growth of austenite grains. Furthermore, when reheating temperatures and holding times increase, the dissolution and coarsening of V(C, N) particles lead to the decrease of pining ability and then to the rapid growth of austenite. A new Sellars model with a time index was used to establish austenite growth model using a new method with a predetermined error function. The accuracy of the prediction for austenite grain sizes with new Sellars model was greatly improved compared with the traditional Beck model.
|
|
Received: 14 December 2021
|
|
|
| Fund: National Key Research and Development Program of China(2017YFB0305100);Key Research and Development Program of Hubei Province(2020BAB057) |
About author: YANG Gengwei, associate professor, Tel: (027)68862085, E-mail: yanggengwei@wust.edu.cn
|
| 1 |
Gramlich A, Schmiedl T, Schönborn S, et al. Development of air-hardening martensitic forging steels [J]. Mater. Sci. Eng., 2020, A784: 139321
|
| 2 |
Yan X C, Hu J, Yu H, et al. Unraveling the significant role of retained austenite on the dry sliding wear behavior of medium manganese steel [J]. Wear, 2021, 476: 203745
|
| 3 |
Sun R M, Xu W H, Wang C Y, et al. Wear resistant of new type medium manganese high strength Martensite steel [J]. Iron Steel, 2012, 47: 64
|
|
孙荣民, 徐文欢, 王存宇 等. 新型中锰马氏体高强度钢的耐磨性能 [J]. 钢铁, 2012, 47: 64
|
| 4 |
Luo K S, Bai B Z. Microstructure, mechanical properties and high stress abrasive wear behavior of air-cooled MnCrB cast steels [J]. Mater. Des., 2010, 31: 2510
doi: 10.1016/j.matdes.2009.11.040
|
| 5 |
Gramlich A, Middleton A, Schmidt R, et al. On the influence of vanadium on air-hardening medium manganese steels for sustainable forging products [J]. Steel Res. Int., 2021, 92: 2000592
|
| 6 |
Pei Z Z, Song R B, Ba Q N, et al. Dimensionality wear analysis: Three-body impact abrasive wear behavior of a martensitic steel in comparison with Mn13Cr2 [J]. Wear, 2018, 414-415: 341
doi: 10.1016/j.wear.2018.09.002
|
| 7 |
Deng X T, Wang Z D, Tian Y, et al. An investigation of mechanical property and three-body impact abrasive wear behavior of a 0.27%C dual phase steel [J]. Mater. Des., 2013, 49: 220
doi: 10.1016/j.matdes.2013.01.024
|
| 8 |
Mondal J, Das K, Das S. An investigation of mechanical property and sliding wear behaviour of 400HV grade martensitic steels [J]. Wear., 2020, 458-459: 203436
|
| 9 |
Beck P A, Holzworth M L, Hu H. Instantaneous rates of grain growth [J]. Phys. Rev., 1948, 73: 526
doi: 10.1103/PhysRev.73.526
|
| 10 |
Sellars C M, Whiteman J A. Recrystallization and grain growth in hot rolling [J]. Met. Sci., 1979, 13: 187
|
| 11 |
Uhm S, Moon J, Lee C, et al. Prediction Model for the austenite grain size in the coarse grained heat affected zone of Fe-C-Mn steels: Considering the effect of initial grain size on isothermal growth behavior [J]. ISIJ. Int., 2004, 44: 1230
doi: 10.2355/isijinternational.44.1230
|
| 12 |
Staśko R, Adrian H, Adrian A. Effect of nitrogen and vanadium on austenite grain growth kinetics of a low alloy steel [J]. Mater. Charact., 2006, 56: 340
doi: 10.1016/j.matchar.2005.09.012
|
| 13 |
Yang G W, Sun X J, Li Z D, et al. Effects of vanadium on the microstructure and mechanical properties of a high strength low alloy martensite steel [J]. Mater. Des., 2013, 50: 102
doi: 10.1016/j.matdes.2013.03.019
|
| 14 |
Yang G W, Sun X J, Yong Q L, et al. Austenite grain refinement and isothermal growth behavior in a low carbon vanadium microalloyed steel [J]. J. Iron Steel Res. Int., 2014, 21: 757
doi: 10.1016/S1006-706X(14)60138-2
|
| 15 |
Sha Q Y, Sun Z Q. Grain growth behavior of coarse-grained austenite in a Nb-V-Ti microalloyed steel [J]. Mater. Sci. Eng., 2009, A523: 77
|
| 16 |
Moon J, Lee C, Uhm S, et al. Coarsening kinetics of TiN particle in a low alloyed steel in weld HAZ: Considering critical particle size [J]. Acta Mater., 2006, 54: 1053
doi: 10.1016/j.actamat.2005.10.037
|
| 17 |
Moon J, Kim S, Lee J, et al. Coarsening behavior of the (Ti, Nb)(C, N) complex particle in a microalloyed steel weld heat-affected zone considering the critical particle size [J]. Metall. Mater. Trans., 2007, 38A: 2788
|
| 18 |
Dong J, Liu C X, Liu Y C, et al. Effects of two different types of MX carbonitrides on austenite growth behavior of Nb-V-Ti microalloyed ultra-high strength steel [J]. Fusion. Eng. Des., 2017, 125: 415
doi: 10.1016/j.fusengdes.2017.05.084
|
| 19 |
Maalekian M, Radis R, Militzer M, et al. In situ measurement and modelling of austenite grain growth in a Ti/Nb microalloyed steel [J]. Acta Mater., 2012, 60: 1015
doi: 10.1016/j.actamat.2011.11.016
|
| 20 |
Zhang Y, Li X H, Liu Y C, et al. Study of the kinetics of austenite grain growth by dynamic Ti-rich and Nb-rich carbonitride dissolution in HSLA steel: In-situ observation and modeling [J]. Mater. Charact., 2020, 169: 110612
|
| 21 |
Yan B Y, Liu Y C, Wang Z J, et al. The effect of precipitate evolution on austenite grain growth in RAFM Steel [J]. Materials, 2017, 10: 1017
doi: 10.3390/ma10091017
|
| 22 |
Militzer M, Hawbolt E B, Ray Meadowcroft T, et al. Austenite grain growth kinetics in Al-killed plain carbon steels [J]. Metall. Mater. Trans., 1996, 27A: 3399
|
| 23 |
Pellissier G E. Stereology and Quantitative Metallography [M]. Philadelphia: American Society for Testing and Materials, 1972: 129
|
| 24 |
Ma H X, Li Y G. Measurement of size distribution and volume fraction of precipitates in silicon steel [J]. Mater. Sci. Eng., 2002, 20: 328
doi: 10.1016/0921-5107(93)90249-M
|
|
马红旭, 李友国. 硅钢中析出物的尺寸分布以及体积分数的测定 [J]. 材料科学与工程, 2002, 20: 328
|
| 25 |
Dang S E, Su Z N, Liu Z L, et al. Austenite grain growth behavior during heating process of as-cast 30Cr2Ni4MoV steel [J]. Chin. J. Mater. Res., 2014, 28: 675
doi: 10.11901/1005.3093.2014.024
|
|
党淑娥, 宿展宁, 刘志龙 等. 30Cr2Ni4MoV钢铸态加热过程中奥氏体晶粒的长大行为 [J]. 材料研究学报, 2014, 28: 675
doi: 10.11901/1005.3093.2014.024
|
| 26 |
Xu Y, Liu J S, Zhao Y, et al. Austenite grain growth kinetics and mechanism of grain growth in 12Cr ultra-super-critical rotor steel [J]. Philos. Mag., 2021, 101: 77
doi: 10.1080/14786435.2020.1821113
|
| 27 |
Ji G, Gao X H, Liu Z G, et al. In situ observation and modeling of austenite grain growth in a Nb-Ti-bearing high carbon steel [J]. J. Iron Steel Res. Int., 2019, 26: 292
doi: 10.1007/s42243-018-0083-6
|
| 28 |
Liu Z B, Tu X, Wang X H, et al. Carbide dissolution and austenite grain growth behavior of a new ultrahigh-strength stainless steel [J]. J. Iron Steel Res. Int., 2020, 27: 732
doi: 10.1007/s42243-020-00429-6
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|