Mechanical Behaviors of Nanotwinned Metals and Nanotwinned Covalent Materials |
WEN Bin(), TIAN Yongjun() |
Center for High Pressure Science, State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004, China |
|
Cite this article:
WEN Bin, TIAN Yongjun. Mechanical Behaviors of Nanotwinned Metals and Nanotwinned Covalent Materials. Acta Metall Sin, 2021, 57(11): 1380-1395.
|
Abstract Metallic and covalent materials are important structural materials. Traditional strategies for strengthening materials compromise their ductility and toughness. Recent experimental results show that twinning can simultaneously improve the strength (hardness) and toughness of copper and diamond; as the inverse relationship between the strength and toughness of materials is broken, this has become a hot research topic. By studying the strengthening mechanism of nanotwinned copper and diamond, methods to simultaneously improve strength and toughness may be found. Herein, this paper presents a comprehensive overview of the recent developments in the experimental and theoretical studies of nanotwinned metals and covalent materials. The microstructures, fabrication methods, and mechanical properties of nanotwinned metals and covalent materials are summarized. Further, the strengthening mechanism of nanotwinned metals and the hardening mechanism of covalent materials are introduced. Finally, the research trend on the mechanical behavior of nanotwinned materials is discussed in detail.
|
Received: 16 July 2021
|
|
Fund: National Funds for Distinguished Young Scholars(51925105);National Natural Science Foundation of China(52090020) |
About author: TIAN Yongjun, professor, Tel: (0335)8387688, E-mail: fhcl@ysu.edu.cn WEN Bin, professor, Tel: (0335)8057047, E-mail: wenbin@ysu.edu.cn
|
1 |
Lu K. The future of metals [J]. Science, 2010, 328: 319
|
2 |
Ritchie R O. The conflicts between strength and toughness [J]. Nat. Mater., 2011, 10: 817
|
3 |
Sun L G, He X Q, Lu J. Nanotwinned and hierarchical nanotwinned metals: A review of experimental, computational and theoretical efforts [J]. npj Comput. Mater., 2018, 4: 6
|
4 |
Chen A Y, Li D F, Zhang J B, et al. Make nanostructured metal exceptionally tough by introducing non-localized fracture behaviors [J]. Scr. Mater., 2008, 59: 579
|
5 |
Fang T H, Li W L, Tao N R, et al. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper [J]. Science, 2011, 331: 1587
|
6 |
Lu K. Making strong nanomaterials ductile with gradients [J]. Science, 2014, 345: 1455
|
7 |
Wu X L, Jiang P, Chen L, et al. Extraordinary strain hardening by gradient structure [J]. Proc. Natl. Acad. Sci. USA, 2014, 111: 7197
|
8 |
Wang T M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal [J]. Nature, 2002, 419: 912
|
9 |
Zhu L L, Lu J. Modelling the plastic deformation of nanostructured metals with bimodal grain size distribution [J]. Int. J. Plast., 2012, 30-31: 166
|
10 |
Zhu L L, Shi S Q, Lu K, et al. A statistical model for predicting the mechanical properties of nanostructured metals with bimodal grain size distribution [J]. Acta Mater., 2012, 60: 5762
|
11 |
Zhu L L, Guo X, Ruan H H, et al. Prediction of mechanical properties in bimodal nanotwinned metals with a composite structure [J]. Compos. Sci. Technol., 2016, 123: 222
|
12 |
Hall E O. Yield Point Phenomena in Metals and Alloys [M]. New York: Plenum Press, 1970: 37
|
13 |
Horita Z, Ohashi K, Fujita T, et al. Achieving high strength and high ductility in precipitation-hardened alloys [J]. Adv. Mater., 2005, 17: 1599
|
14 |
Zhao Y H, Zhu Y T, Lavernia E J. Strategies for improving tensile ductility of bulk nanostructured materials [J]. Adv. Eng. Mater., 2010, 12: 769
|
15 |
Jiao Z B, Luan J H, Zhang Z W, et al. Synergistic effects of Cu and Ni on nanoscale precipitation and mechanical properties of high-strength steels [J]. Acta Mater., 2013, 61: 5996
|
16 |
Lu K, Lu L, Suresh S. Strengthening materials by engineering coherent internal boundaries at the nanoscale [J]. Science, 2009, 324: 349
|
17 |
Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422
|
18 |
Lu L, Chen X, Huang X X, et al. Revealing the maximum strength in nanotwinned copper [J]. Science, 2009, 323: 607
|
19 |
Wei Y J, Li Y Q, Zhu L C, et al. Evading the strength-ductility trade-off dilemma in steel through gradient hierarchical nanotwins [J]. Nat. Commun., 2014, 5: 3580
|
20 |
Zhang Z J, Sheng H W, Wang Z J, et al. Dislocation mechanisms and 3D twin architectures generate exceptional strength-ductility-toughness combination in CrCoNi medium-entropy alloy [J]. Nat. Commun., 2017, 8: 14390
|
21 |
Kou H N, Lu J, Li Y. High-strength and high-ductility nanostructured and amorphous metallic materials [J]. Adv. Mater., 2014, 26: 5518
|
22 |
Wu G, Chan K C, Zhu L L, et al. Dual-phase nanostructuring as a route to high-strength magnesium alloys [J]. Nature, 2017, 545: 80
|
23 |
Mahajan S, Williams D F. Deformation twinning in metals and alloys [J]. Int. Metall. Rev., 1973, 18: 43
|
24 |
Yoo M H, Lee J K. Deformation twinning in h.c.p. metals and alloys [J]. Philos. Mag., 1991, 63A: 987
|
25 |
Christian J W, Mahajan S. Deformation twinning [J]. Prog. Mater. Sci., 1995, 39: 1
|
26 |
Zhu Y T, Liao X Z, Wu X L. Deformation twinning in bulk nanocrystalline metals: Experimental observations [J]. JOM, 2008, 60(9): 60
|
27 |
Zhu Y T, Liao X Z, Wu X L. Deformation twinning in nanocrystalline materials [J]. Prog. Mater. Sci., 2012, 57: 1
|
28 |
Huang Q, Yu D L, Xu B, et al. Nanotwinned diamond with unprecedented hardness and stability [J]. Nature, 2014, 510: 250
|
29 |
Xu B, Tian Y J. Diamond gets harder, tougher, and more deformable [J]. Matter Radiat. Extrem., 2020, 5: 068103
|
30 |
Yue Y H, Gao Y F, Hu W T, et al. Hierarchically structured diamond composite with exceptional toughness [J]. Nature, 2020, 582: 370
|
31 |
Anderoglu O, Misra A, Wang H, et al. Thermal stability of sputtered Cu films with nanoscale growth twins [J]. J. Appl. Phys., 2008, 103: 094322
|
32 |
Bufford D, Wang H Y, Zhang X H. Thermal stability of twins and strengthening mechanisms in differently oriented epitaxial nanotwinned Ag films [J]. J. Mater. Res., 2013, 28: 1729
|
33 |
Bufford D, Wang H, Zhang X. High strength, epitaxial nanotwinned Ag films [J]. Acta Mater., 2011, 59: 93
|
34 |
Tian Y J, Xu B, Yu D L, et al. Ultrahard nanotwinned cubic boron nitride [J]. Nature, 2013, 493: 385
|
35 |
Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747
|
36 |
Petch N J. The cleavage strength of polycrystals [J]. J. Iron Steel Inst., 1953, 174: 25
|
37 |
Lu K. Stabilizing nanostructures in metals using grain and twin boundary architectures [J]. Nat. Rev. Mater., 2016, 1: 16019
|
38 |
Hu J, Shi Y N, Sauvage X, et al. Grain boundary stability governs hardening and softening in extremely fine nanograined metals [J]. Science, 2017, 355: 1292
|
39 |
Li X Y, Wei Y J, Lu L, et al. Dislocation nucleation governed softening and maximum strength in nano-twinned metals [J]. Nature, 2010, 464: 877
|
40 |
Wang J, Li N, Anderoglu O, et al. Detwinning mechanisms for growth twins in face-centered cubic metals [J]. Acta Mater., 2010, 58: 2262
|
41 |
Schiøtz J, Di Tolla F D, Jacobsen K W. Softening of nanocrystalline metals at very small grain sizes [J]. Nature, 1998, 391: 561
|
42 |
Yip S. The strongest size [J]. Nature, 1998, 391: 532
|
43 |
Van Swygenhoven H. Grain boundaries and dislocations [J]. Science, 2002, 296: 66
|
44 |
Schiøtz J, Vegge T, Di Tolla F D, et al. Atomic-scale simulations of the mechanical deformation of nanocrystalline metals [J]. Phys. Rev., 1999, 60B: 11971
|
45 |
Schiøtz J, Jacobsen K W. A maximum in the strength of nanocrystalline copper [J]. Science, 2003, 301: 1357
|
46 |
Dubrovinskaia N, Solozhenko V L, Miyajima N, et al. Superhard nanocomposite of dense polymorphs of boron nitride: Noncarbon material has reached diamond hardness [J]. Appl. Phys. Lett., 2007, 90: 101912
|
47 |
Sumiya H, Irifune T. Hardness and deformation microstructures of nano-polycrystalline diamonds synthesized from various carbons under high pressure and high temperature [J]. J. Mater. Res., 2007, 22: 2345
|
48 |
Wen B, Xu B, Wang Y B, et al. Continuous strengthening in nanotwinned diamond [J]. npj Comput. Mater., 2019, 5: 117
|
49 |
Xiao J W, Yang H Z, Liu H X, et al. Strengthening-softening transition in yield strength of nanotwinned Cu [J]. Scr. Mater., 2019, 162: 372
|
50 |
Hu W T, Wen B, Huang Q, et al. Role of plastic deformation in tailoring ultrafine microstructure in nanotwinned diamond for enhanced hardness [J]. Sci. China Mater., 2017, 60: 178
|
51 |
Xiao J W, Yang H Z, Wu X Z, et al. Dislocation behaviors in nanotwinned diamond [J]. Sci. Adv., 2018, 4: eaat8195
|
52 |
Bilby B A, Crocker A G. The theory of the crystallography of deformation twinning [J]. Proc. Roy. Soc., 1965, 288A: 240
|
53 |
Jaswon M A, Dove D B. The prediction of twinning modes in metal crystals [J]. Acta Cryst., 1956, 10: 14
|
54 |
Jaswon M A, Dove D B. The crystallography of deformation twinning [J]. Acta Cryst., 1960, 13: 232
|
55 |
Kiho H. The crystallographic aspect of the mechanical twinning in Ti and α-U [J]. J. Phys. Soc. Jpn., 1958, 13: 269
|
56 |
Yu Y N. Fundamentals of Materials Science [M]. 2nd Ed., Beijing: Higher Education Press, 2012: 570
|
|
余永宁. 材料科学基础 [M]. 第2版, 北京:高等教育出版社, 2012: 570
|
57 |
Hall E. Twinning and Diffusionless Transformations in Metals [M]. London: Butterworths Scientific Publications, 1954: 53
|
58 |
Christian J W. The Theory of Transformations in Metals and Alloys: An Advanced Textbook in Physical Metallurgy [M]. 3rd Ed., Oxford: Pergamon, 2002: 859
|
59 |
Christian J W, Laughlin D E. Overview no.67 The deformation twinning of superlattice structures derived from disordered B.C.C. or F.C.C. solid solutions [J]. Acta Metall., 1988, 36: 1617
|
60 |
Bevis M, Crocker A G. Twinning shears in lattices [J]. Proc. Roy. Soc., 1968, 304A: 123
|
61 |
Bevis M, Crocker A G. Twinning modes in lattices [J]. Proc. Roy. Soc., 1969, 313A: 509
|
62 |
Jaswon M A, Dove D B. Twinning properties of lattice planes [J]. Acta Cryst., 1956, 9: 621
|
63 |
Churchman A T, Geach G A, Winton J. Deformation twinning in materials of the A4 (diamond) crystal structure [J]. Proc. Roy. Soc., 1956, 238A: 194
|
64 |
Chen T P, Chen F R, Chuang Y C, et al. Study of twins in GaAs, GaP and InAs crystals [J]. J. Cryst. Growth, 1992, 118: 109
|
65 |
Tang C Y, Li F H, Wang R, et al. Atomic configurations of dislocation core and twin boundaries in 3C-SiC studied by high-resolution electron microscopy [J]. Phys. Rev., 2007, 75B: 184103
|
66 |
Huang C, Yang B, Peng X H, et al. Plastic deformation and hardening mechanisms of a nano-twinned cubic boron nitride ceramic [J]. ACS Appl. Mater. Interfaces, 2020, 12: 50161
|
67 |
Shiga K, Maeda K, Morito H, et al. Effect of twin boundary formation on the growth rate of the GaSb{111} plane [J]. Acta Mater., 2020, 185: 453
|
68 |
Beyerlein I J, Zhang X H, Misra A. Growth twins and deformation twins in metals [J]. Annu. Rev. Mater. Res., 2014, 44: 329
|
69 |
Lu L, Lu K. Metallic materials with nano-scale twins [J]. Acta Metall. Sin., 2010, 46: 1422
|
|
卢 磊, 卢 柯. 纳米孪晶金属材料 [J]. 金属学报, 2010, 46: 1422
|
70 |
Lu L, You Z S. Plastic deformation mechanisms in nanotwinned metals [J]. Acta Metall. Sin., 2014, 50: 129
|
|
卢 磊, 尤泽升. 纳米孪晶金属塑性变形机制 [J]. 金属学报, 2014, 50: 129
|
71 |
Cheng Z. Mechanical properties and deformation mechanisms of gradient nanotwinned Cu [D]. Hefei: University of Science and Technology of China, 2019
|
|
程 钊. 梯度纳米孪晶Cu的力学性能和变形机制研究 [D]. 合肥: 中国科学技术大学, 2019
|
72 |
Zhang Y Z. Mechanical properties and plastic deformation mechanism of nano-twinned 316L austenitic stainless steel [D]. Hefei: University of Science and Technology of China, 2019
|
|
张友昭. 纳米孪晶316L奥氏体不锈钢的力学性能和塑性变形机制研究 [D]. 合肥: 中国科学技术大学, 2019
|
73 |
Zhang Z Y. Microstructures and properties of nanotwinned CuCrZr alloy strengthened by precipitates [D]. Hefei: University of Science and Technology of China, 2020
|
|
张志远. 时效强化纳米孪晶铜铬锆合金微观结构和性能研究 [D]. 合肥: 中国科学技术大学, 2020
|
74 |
Meng G Z, Shao Y W, Zhang T, et al. Synthesis and corrosion property of pure Ni with a high density of nanoscale twins [J]. Electrochim. Acta, 2008, 53: 5923
|
75 |
Wu B Y C, Schuh C A, Ferreira P J. Nanostructured Ni-Co alloys with tailorable grain size and twin density [J]. Metall. Mater. Trans., 2005, 36A: 1927
|
76 |
Nakamoto Y, Yuasa M, Chen Y Q, et al. Mechanical properties of a nanocrystalline Co-Cu alloy with a high-density fine nanoscale la-mellar structure [J]. Scr. Mater., 2008, 58: 731
|
77 |
Chen X H, Lu L, Lu K. Electrical resistivity of ultrafine-grained copper with nanoscale growth twins [J]. J. Appl. Phys., 2007, 102: 083708
|
78 |
You Z S, Lu L, Lu K. Tensile behavior of columnar grained Cu with preferentially oriented nanoscale twins [J]. Acta Mater., 2011, 59: 6927
|
79 |
Kelly P J, Arnell R D. Magnetron sputtering: A review of recent developments and applications [J]. Vacuum, 2000, 56: 159
|
80 |
Zhang X H, Wang H, Chen X H, et al. High-strength sputter-deposited Cu foils with preferred orientation of nanoscale growth twins [J]. Appl. Phys. Lett., 2006, 88: 173116
|
81 |
Dahlgren S D. Columnar grains and twins in high-purity sputter-deposited copper [J]. J. Vac. Sci. Technol., 1974, 11: 832
|
82 |
Dahlgren S D, Nicholson W L, Merz M D, et al. Microstructural analysis and tensile properties of thick copper and nickel sputter deposits [J]. Thin Solid Films, 1977, 40: 345
|
83 |
Zhang X, Misra A, Wang H, et al. Enhanced hardening in Cu/330 stainless steel multilayers by nanoscale twinning [J]. Acta Mater., 2004, 52: 995
|
84 |
Zhang X, Misra A. Superior thermal stability of coherent twin boundaries in nanotwinned metals [J]. Scr. Mater., 2012, 66: 860
|
85 |
Tao N R, Lu K. Dynamic plastic deformation (DPD): A novel technique for synthesizing bulk nanostructured metals [J]. J. Mater. Sci. Technol., 2007, 23: 771
|
86 |
Li Y S, Tao N R, Lu K. Microstructural evolution and nanostructure formation in copper during dynamic plastic deformation at cryogenic temperatures [J]. Acta Mater., 2008, 56: 230
|
87 |
Li Y S, Zhang Y, Tao N R, et al. Effect of the Zener-Hollomon parameter on the microstructures and mechanical properties of Cu subjected to plastic deformation [J]. Acta Mater., 2009, 57: 761
|
88 |
Xiao G H, Tao N R, Lu K. Effects of strain, strain rate and temperature on deformation twinning in a Cu-Zn alloy [J]. Scr. Mater., 2008, 59: 975
|
89 |
Zhang Y, Tao N R, Lu K. Effect of stacking-fault energy on defor-mation twin thickness in Cu-Al alloys [J]. Scr. Mater., 2009, 60: 211
|
90 |
Yan F K, Liu G Z, Tao N R, et al. Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles [J]. Acta Mater., 2012, 60: 1059
|
91 |
Zhang B B, Yan F K, Zhao M J, et al. Combined strengthening from nanotwins and nanoprecipitates in an iron-based superalloy [J]. Acta Mater., 2018, 151: 310
|
92 |
Yi H Y, Yan F K, Tao N R, et al. Comparison of strength-ductility combinations between nanotwinned austenite and martensite-austenite stainless steels [J]. Mater. Sci. Eng., 2015, A647: 152
|
93 |
Tao Q, Wei X, Lian M, et al. Nanotwinned diamond synthesized from multicore carbon onion [J]. Carbon, 2017, 120: 405
|
94 |
Feng X, Xiao J W, Wen B, et al. Temperature-dependent hardness of zinc-blende structured covalent materials [J]. Sci. China Mater., 2021, 64: 2280
|
95 |
Zhao Z S, Xu B, Tian Y J. Recent advances in superhard materials [J]. Annu. Rev. Mater. Res., 2016, 46: 383
|
96 |
Xiao J W. Investigation on mechanical properties of nanotwinned diamond and nanotwinned copper [D]. Qinhuangdao: Yanshan University, 2018
|
|
肖建伟. 纳米孪晶金刚石和纳米孪晶铜的力学性质研究 [D]. 秦皇岛: 燕山大学, 2018
|
97 |
Hartley C S, Blachon D L A. Reactions of slip dislocations at coherent twin boundaries in face-centered-cubic metals [J]. J. Appl. Phys., 1978, 49: 4788
|
98 |
Zhu T, Gao H J. Plastic deformation mechanism in nanotwinned metals: An insight from molecular dynamics and mechanistic modeling [J]. Scr. Mater., 2012, 66: 843
|
99 |
Zhu T, Li J, Samanta A, et al. Interfacial plasticity governs strain rate sensitivity and ductility in nanostructured metals [J]. Proc. Natl. Acad. Sci. USA, 2007, 104: 3031
|
100 |
Misra A, Hirth J P, Hoagland R G. Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites [J]. Acta Mater., 2005, 53: 4817
|
101 |
Gu P, Dao M, Suresh S. Analysis of size-dependent slip transfer and inter-twin flow stress in a nanotwinned fcc metal [J]. Acta Mater., 2014, 67: 409
|
102 |
Zhu Y T, Wu X L, Liao X Z, et al. Dislocation-twin interactions in nanocrystalline fcc metals [J]. Acta Mater., 2011, 59: 812
|
103 |
Dao M, Lu L, Shen Y F, et al. Strength, strain-rate sensitivity and ductility of copper with nanoscale twins [J]. Acta Mater., 2006, 54: 5421
|
104 |
Ovid’ko I A, Sheinerman A G. Plastic deformation through de-twinning mediated by incoherent twin boundaries in nanotwinned metallic alloys [J]. Rev. Adv. Mater. Sci., 2016, 47: 1
|
105 |
Barnett M R, Keshavarz Z, Ma X. A semianalytical sachs model for the flow stress of a magnesium alloy [J]. Metall. Mater. Trans., 2006, 37A: 2283
|
106 |
Blumenau A T, Heggie M I, Fall C J, et al. Dislocations in diamond: Core structures and energies [J]. Phys. Rev., 2002, 65B: 205205
|
107 |
Blumenau A T, Jones R, Frauenheim T, et al. Dislocations in diamond: Dissociation into partials and their glide motion [J]. Phys. Rev., 2003, 68B: 014115
|
108 |
Masuya S, Hanada K, Oshima T, et al. Formation of stacking fault and dislocation behavior during the high-temperature annealing of single-crystal HPHT diamond [J]. Diam. Relat. Mater., 2017, 75: 155
|
109 |
Cahoon J R, Broughton W H, Kutzak A R. The determination of yield strength from hardness measurements [J]. Metall. Trans., 1971, 2: 1979
|
110 |
Bringa E M, Caro A, Wang Y M, et al. Ultrahigh strength in nanocrystalline materials under shock loading [J]. Science, 2005, 309: 1838
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|