Abstract The solidification and cooling of liquid steel in continuous casting process is a complicated non-equilibrium phenomenon. During steel solidification process, the micro-segregation of solute elements between liquid steel and solidified shell will vary with their temperature-dependent diffusion coefficients and equilibrium distribution coefficients. Due to non-uniform cooling pattern in the continuous casting process of steel blooms, the fluctuation of cooling rate in bloom will have a great influence on micro-segregation degree of the elements. The micro-segregation behavior of solute elements in steel solidification process is responsible for the variation of characteristic temperatures such as zero strength temperature (ZST), zero ductility temperature (ZDT) and liquid impenetrable temperature (LIT), which make up the brittle temperature range in steel solidification. During continuous casting process of steel, internal cracks created by thermal and mechanical deformation tend to occur in this range. To prevent the occurrence of these cracks in continuous casting bloom, it is essential to better understand about the internal crack susceptibility concerning micro-segregation behavior in the non-uniform cooling process. In this work, a micro-segregation analytical model for YQ450NQR1 steel continuous casting bloom is established to study the inter-dendritic segregation behavior of main solute elements C, Si, Mn, P and S at various cooling rates, the results show that P and S are more likely to segregate compared with C, Si and Mn and the increase of cooling rate weakens the micro-segregation degree of C, Si, Mn, P and S. Based on the micro-segregation model established above, ZST, ZDT and LIT for YQ450NQR1 steel are calculated and the influences of cooling rate on ZST, ZDT and LIT are analyzed. It reveals that ZST, ZDT and LIT of YQ450NQR1 steel bloom decrease accordingly with the increase of cooling rate. On this basis, the index of internal crack susceptibility (IICS) is defined to quantitatively characterize the internal crack susceptibility of the bloom. The results show that the internal crack susceptibility becomes larger while the IICS value approaches to 1. Furthermore, an internal crack susceptibility model is obtained concerning IICS and cooling rate (CR) and the validation is performed to certify the model′s suitability in quantitatively predicting internal crack susceptibility of YQ450NQR1 steel continuous casting bloom in the non-uniform cooling process.
|
|
|
Fund: Supported by National Natural Science Foundation of China (No.51074023) and Independent R&D Foundation for State Key Laboratory of Advanced Metallurgy (No.41602023) |
About author: null
作者简介: 窦 坤, 男, 1988年生, 博士生 |
[1] |
Cai K K. Quality Control of Continuous Casting Billet. Beijing: Metallurgical Industry Press, 2010: 90
|
|
(蔡开科. 连铸坯质量控制. 北京: 冶金工业出版社, 2010: 90)
|
[2] |
Brimacombe J K, Sorimachi K. Metall Mater Trans, 1977; 8B: 489
|
[3] |
Mintz B, Yue S, Jonas J J. Int Mater Rev, 1991; 36: 187
|
[4] |
Liu Q, Zhang L Q, Wang L Z, Ding X Z, Cao L G, Qi Y G, Liu Y W. J Univ Sci Technol Beijing, 2006; 28: 133
|
|
(刘 青, 张立强, 王良周, 丁秀中, 曹立国, 齐永革, 刘彦伟. 北京科技大学学报, 2006; 28: 133)
|
[5] |
Himemiya T, Umeda T. ISIJ Int, 1998; 38: 730
|
[6] |
Han Z Q, Cai K K. Acta Metall Sin, 2000; 36: 869
|
|
(韩志强, 蔡开科. 金属学报, 2000; 36: 869)
|
[7] |
Luo H W, Karjalainen L P, Porter D A, Liimatainen H M, Zhang Y. ISIJ Int, 2002; 42: 273
|
[8] |
El-Bealy M, Leskinen N, Fredrikson H. Ironmaking Steelmaking, 1995; 22: 246
|
[9] |
Hardin R A, Liu K, Beckermann C, Kapoor A. Metall Mater Trans, 2003; 34B: 297
|
[10] |
Wang X Y, Liu Q, Wang B. Ironmaking Steelmaking, 2011; 38: 552
|
[11] |
Clyne T W, Kurz W. Metall Mater Trans, 1981; 12A: 965
|
[12] |
Yaguchi H. Metall Mater Trans, 1986; 17A: 2080
|
[13] |
Won Y M, Thomas B G. Metall Mater Trans, 2001; 32A: 1755
|
[14] |
Clyne T W, Wolf M, Kurz W. Metall Mater Trans, 1982; 13B: 259
|
[15] |
Dhindaw B K, Antonsson T, Fredriksson H, Tinoco J. Metall Mater Trans, 2004; 35A: 2869
|
[16] |
Cornelissen M C M. Ironmaking Steelmaking, 1986; 13: 204
|
[17] |
Liu Z Z, Wei J, Cai K K. ISIJ Int, 2002; 42: 958
|
[18] |
Matsumiya T, Kajioka H, Mizoguchi S, Ueshima Y, Esaka H. Trans Iron Steel Inst Jpn, 1984; 24: 873
|
[19] |
Liu Q, Wang L Z, Zhang L Q, Cao L G, Ding X Z, Liang M, Qi Y G. Int J Miner Metall Mater, 2008; 15: 17
|
[20] |
Cai Z Z, Zhu M Y. Acta Metall Sin, 2009; 45: 949
|
|
(蔡兆镇, 朱苗勇. 金属学报, 2009; 45: 949)
|
[21] |
Wang W L, Zhu M Y, Cai Z Z, Luo S, Ji C. Steel Res Int, 2012; 83: 1152
|
[22] |
Cai Z Z, Zhu M Y. Foundry Technol, 2009; 11: 1396
|
|
(蔡兆镇, 朱苗勇. 铸造技术, 2009; 11: 1396)
|
[23] |
Luo S, Zhu M Y, Ji C, Cai Z Z. Iron Steel, 2010; 45(6): 31
|
|
(罗 森, 朱苗勇, 祭 程, 蔡兆镇. 钢铁, 2010; 45(6): 31)
|
[24] |
Jing C L, Wang X H, Jiang M. Steel Res Int, 2011; 82: 1173
|
[25] |
Zhang Z X, Min Y, Jiang M F. J Northeastern Univ (Nat Sci Ed), 2010; 31: 966
|
|
(张志祥, 闵 义, 姜茂发. 东北大学学报(自然科学版), 2010; 31: 966)
|
[26] |
Yoon J K. ISIJ Int, 2008; 48: 879
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|