THEORY ANALYSIS ON THE NEW GENERATION OF CLEAN STEEL PRODUCTION PROCESS |
XU Kuangdi1), XIAO Lijun2), GAN Yong2), LIU Liu2), WANG Xinhua3) |
1) Chinese Academy of Engineering, Beijing 100088
2) State Key Laboratory of Advanced Steel Processes and Products, Central Iron and Steel Research Institute, Beijing 100081
3) Jing Tang Iron and Steel Corporation, Tangshan 063200 |
|
Cite this article:
XU Kuangdi XIAO Lijun GAN Yong LIU Liu WANG Xinhua. THEORY ANALYSIS ON THE NEW GENERATION OF CLEAN STEEL PRODUCTION PROCESS. Acta Metall Sin, 2012, 48(1): 1-10.
|
Abstract Based on the thermodynamic analysis on the selective oxidation of the main elements in the new generation of clean steel production process, and the production practices of hot metal treatment in the new process of clean steel production accumulated by the Jing Tang Iron and Steel Corporation, the control of the main elements such as S, P, C, etal., were investigated, and the main characteristics of the new generation of clean steel production process were analyzed. We indicate that several production problems must be solved. The research results show that, by using KR desulphurization technology, the S content of hot metal can be steadily controlled to less than 0.0020%. The final S control of the new production process of clean steel depends mainly on the resulfurization content in the dephosphorization furnace. Increasing the slag basicity and reducing the content of S from scrap and slag forming materials can reduce the resulfurization of hot metal. The formation of proper slag basicity at relatively lower hot metal pretreatment temperature (1300-1350 ℃) and at relatively higher oxygen potential is the key to solving the problem of removing P at high C content. The P content in dephosphorization furnace, when producing common low P steel (P<0.006%), may be controlled at less than 0.03%, whereas the P content should be below 0.008% when producing ultra low P steel (P<0.002%). Less-slag smelting, lower Fe losing and high carbon tapping of decarburization furnace are the important technological characteristics of the new generation of clean steel production process.
|
Received: 04 August 2011
|
[1] Oeters F, Stromenger P, Pluschkell W. Arch Eisenhuttenwes, 1977; (44): 727[2] Niedringhaus J C, Fruehan R J. Metall Trans, 1988; 19B: 261[3] Iron and Steel Institute of Japan. Iron and Steel Manual. Tokyo: MARUZEN Company Limited, 1981: 154(日本铁钢协会 编. 铁钢便览. 东京: 丸善株式会社, 1981: 154)[4] Turkdogan E T. Fundamentals of Steelmaking. London: Cambridge University Press, 1996: 180[5] Thomas R. Free Energy of Formation of Binary Compounds. London: MIT Press, 1971: 32[6] Chipman J. Metall Trans, 1970; 1: 2163[7] Fumitaka T, Midiei N, Takashi O, Nobuo S. Tetsu Hagan´e, 1990; 76: 1664(月桥文孝, 中村右英, 折本隆, 佐野信雄. 铁と钢, 1990, 76: 1664)[8] Matsuo T, Yamazaki I, Masuda S, Yoshida K. Steelmaking Conference Proceedings, Detroit: ISS–AIME, 1990: 115[9] Shozo K, Matsuhide A, Toshiharu T. R&D Kobe Steel Engineering Reports, 1986; 36(1): 23[10] Toshiyuki U, Kiyohito F. The Tenth Japan–China Symposium on Science and Technology of Iron and Steel, Chiba, Japan, 2004(11): 122 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|