Acta Metall Sin  2009, Vol. 45 Issue (2): 189-194    DOI:
论文 Current Issue | Archive | Adv Search |
FEA OF EVALUATING MATERIAL YIELD STRENGTH AND STRAIN HARDENING EXPONENT USING A SPHERICAL INDENTATION
CUI Hang; CHEN Huaining; CHEN Jing; HUANG Chunling; WU Changzhong
Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

CUI Hang CHEN Huaining CHEN Jing HUANG Chunling WU Changzhong. FEA OF EVALUATING MATERIAL YIELD STRENGTH AND STRAIN HARDENING EXPONENT USING A SPHERICAL INDENTATION. Acta Metall Sin, 2009, 45(2): 189-194.

Download:  PDF(789KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Dimensional analysis was constructed to derive the dimensionless functions of a spherical indenter with 1 mm in diameter. The function can be used to extract the yield strength and strain hardening exponent of metal materials by means of finite element analysis. The fitting functions used to analyze materials yield strength and strain hardening exponent within the yield strains ranging from 0.00769 to 0.04 were obtained by numerical simulation. It has been validated that the prediction accuracy is enhanced and the average errors of the yield strength and strain hardening exponent are 1.6% and 12.6%, respectively.

Key words:  FEA (finite element analysis)      spherical indentation, yield strength      strain hardening exponent      dimensionless function     
Received:  16 June 2008     
ZTFLH: 

TG146

 
Fund: 

Supported by Science Cooperative Foundation of Chinese and Russian Governments (No.20070634)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I2/189

[1] Suresh S, Alcala J, Giannakopoulos E. US Pat, US 6 247 355 B1, 2001
[2] Kwon D I, Choi Y, Lee Y H. US Pat, US 6 718 820 B2, 2004
[3] Hernot X, Bartier O, Bekouche Y, Bekouche Y, Abdi R E I, Mauvoisin G. Int J Solids Struct, 2006; 43: 4136
[4] Matthews J R, Acta Metall, 1980; 28: 311
[5] Herbert E G, Pharr G M, Oliver W C, Lucas B N, Hay J L. Thin Solid Films, 2001; 398–399: 331
[6] Cao Y P, Lu J. Acta Mater, 2004; 52: 4023
[7] Cheng Y T, Cheng C M. J Appl Phys, 1998; 84: 1284
[8] Chollacoop N W, PhD Thesis, Massachusetts Institute of Technology, Cambridge, 2004
[9] Dao M, Chollacoop N, Van Vliet K J, Venkatesh T A, Suresh S. Acta Mater, 2001; 49: 3899
[10] Lee H L, Lee J H, Pharr G M. J Mech Phys Solids, 2005; 53: 2046

[1] QIN Fei, XIANG Min, WU Wei. THE STRESS-STRAIN RELATIONSHIP OF TSV-Cu DETERMINED BY NANOINDENTATION[J]. 金属学报, 2014, 50(6): 722-726.
[2] CHEN Jun, TANG Shuai, LIU Zhenyu, WANG Guodong. EFFECTS OF COOLING PROCESS ON MICROSTRUCTURE, MECHANICAL PROPERTIES AND PRECIPITATION BEHAVIORS OF NIOBIUM-TITANIUM MICRO-ALLOYED STEEL[J]. 金属学报, 2012, 48(4): 441-449.
[3] SONG Renbo ZHANG Yongkun WEN Xinli JIA Yisu. HOT DEFORMATION BEHAVIOR OF A HIGH STRENGTH CONTAINER STEEL COMPOUNDED WITH Nb-B[J]. 金属学报, 2011, 47(1): 34-40.
[4] TIAN Ni ZHAO Gang ZUO Liang LIU Chunming. STUDY ON THE STRAIN HARDENING BEHAVIOR OF Al-Mg-Si-Cu ALLOY SHEET FOR AUTOMOTIVE BODY[J]. 金属学报, 2010, 46(5): 613-617.
[5] MO Defeng HE Guoqiu HU Zhengfei LIU Xiaoshan ZHANG Weihua. EFFECT OF MICROSTRUCTURES ON STRAIN HARDENING EXPONENT PREDICTION OF CAST ALUMINUM ALLOY[J]. 金属学报, 2010, 46(2): 184-188.
[6] WANG Shuhan LIU Zhenyu WANG Guodong. INFLUENCE OF GRAIN SIZE ON TWIP EFFECT IN A TWIP STEEL[J]. 金属学报, 2009, 45(9): 1083-1090.
[7] LIU Jiangtao;WANG Zhongguang;SHANG Jianku. DEFORMATION BEHAVIORS OF [110] AND [112] ORIENTED β-Sn SINGLE CRYSTALS[J]. 金属学报, 2008, 44(12): 1409-1414.
No Suggested Reading articles found!