Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (7): 831-836     DOI:
Research Articles Current Issue | Archive | Adv Search |
THERMAL EFFECT SIMULATION OF 45# STEEL SURFACE IRRADIATED BY HIGH INTENSITY PULSED ION BEAMS
;;;
中科院金属所 八室 材料加工模拟组沈阳航空工业学院材料系
Cite this article: 

;. THERMAL EFFECT SIMULATION OF 45# STEEL SURFACE IRRADIATED BY HIGH INTENSITY PULSED ION BEAMS. Acta Metall Sin, 2008, 44(7): 831-836 .

Download:  PDF(754KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on Fourier transient state heating conduction equation, this paper confirms the heating conduction equation of HIPIB. The thermal effect of the target 45# Steel surface irradiated by HIPIB with different power density is simulated. In view of the behavior of ion injection into the metal, thermal load of ion current density were simulated with body heat flux mode and surface heat flux mode. The result with two mode were compared. Another amelioration in the simulation is element removed and reactivated method, which can simulate the evaporation of surface metal under injection by high energy ions. The result show that element removed and reactivated method to simulate disabled element was more alike the forming of crater. The element vaporized on the surface were removed so that the elements around it have been no effect their solidification and cooling. Element removed and reactivated method have little effect in the heating process but improved simulated precision in cooling precess sharply
Key words:       
Received:  06 November 2007     
ZTFLH:  TG156.99  
  TG142.3  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I7/831

[1]Remnev G E,Isakov I F,Tarbokov V A.Surf Coat Tech- nol,1999;114:206
[2]Davis H A,Stinnett R W,Yatsui K.MRS Bull,1996; 21(8):121
[3]Shulov V A,Nochovnaya N A,Remnev G E,Pellerin F, Monge-Cadet P.Surf Coat Technol,1998;99:74
[4]Miao S M.Masteral Dissertation,Dalian University of Technology,2004 (苗收谋.大连理工大学硕士学位论文,2004)
[5]Wu D,Gong Y,Liu J Y,Wang X G,Liu Y,Ma T C.Acta Phys Sin,2006;55:398 (吴迪,宫野,刘金远,王晓钢,刘悦,马腾才.物理学报,2006;55:398)
[6]Miao S M,Lei M K.Acta Metall Sin,2004;40:1221 (苗收谋,雷明凯.金属学报,2004;40:1221)
[7]Zhang T H,Wu Y G.Ion Beam Surface Engineering and Its Application.Beijing:China Machine Press,2005:266 (张通和,吴瑜光.离子束表面工程技术与应用.北京:机械工业出版社,2005:266)
[8]Li C S,Huang D B.Manual for Mechanical Engineering Material.Beijing:Publishing House of Electronics Indus- try,2006:150 (李春胜,黄德彬.机械工程材料手册.北京:电子工业出版社,2006:150)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!