Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (4): 473-477     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECT OF Bi ON SHEAR STRENGTH OF Sn3Ag0.5Cu-xBi/Cu SOLDER JOINTS
;;
大连理工大学
Cite this article: 

. EFFECT OF Bi ON SHEAR STRENGTH OF Sn3Ag0.5Cu-xBi/Cu SOLDER JOINTS. Acta Metall Sin, 2008, 44(4): 473-477 .

Download:  PDF(1243KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of Bi on the shear strength for Sn-3Ag-0.5Cu-xBi(x=0,1,3)/Cu solders joints has been studied after being aged at 140℃ and 195℃. The results indicate that fracture type changes from ductile fracture to brittle fracture with the increasing of IMC. Shear strength for Sn3Ag0.5Cu solder joints changes slightly when aged at lower temperature, but increases with the prolonging of the aging time and sharply drop at final by adding of Bi. When aged at higher temperature, shear strength for each kind solder joint decreases with the prolonging of aging time. Although the shear strength is relatively higher by adding Bi, the difference is small. It is seems that Bi can improve the shear strength by strengthening solder and decreasing the growth of IMC.
Key words:  IMC layer      shear strength      ductile fracture      brittle fracture      
Received:  13 August 2007     
ZTFLH:  TG146  
  TG244  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I4/473

[1]Ma X,Dong B X.Electron Process Technol,2002;23(2): 35 (马鑫,董本霞.电子工艺技术,2002;23(2):35)
[2]Zhang H Y.Yunnan Metall,2002;31(5):42 (张红耀.云南冶金,2002;31(5):42)
[3]Zeng K,Tu K N.Mater Sci Eng,2002;R38:55
[4]Lee Y G,Duh J G.Mater Character,1999;42:143
[5]Shawkert A,Du L G,Sun Z G,Sheng M,Luo L.Acta Metall Sin,2001;37:439 (肖克来提,杜黎光,孙志国,盛玫,罗乐.金属学报,2001;37:4391
[6]Kim K S,Huh S H,Suganuma K.J Alloy Compd,2003; 352:226
[7]Kodai D,Horoshi O,Mitsuhiro H.Mater Trans,2004;45: 380
[8]Zhao J,Qi L,Wang X M,Wang L.J Alloy Compd,2004; 375:196
[9]Zhao J,Qi L,Wang L.In:SMIT Centre,ed.,Conference on High Density Microsystem Design and Packaging and Comonent Failure Analysis.Shanghai:the Institute of Electrical and Electronics Engineers,2006:59
[10]Vianco P T,Rejent J A.J Electron Mater,1999;28:1127
[11]Vianco P T,Rejent J A.J Electron Mater,1999;28:1138
[12]Laurila T,Vuorinen V,Kivilahti J K.Mater Sci Eng, 2005;R49:1
[13]Yoon J W,Lee C B,Jung S B.Mater Trans,2002;43: 1821
[14]An M Z,Zhu C Y,Yang Z L,Zhang J S,Tu Z M.Elec- troplat Pollut Control,2001;21(6):1 (安茂忠,朱成勇,杨哲龙,张景双,屠振密.电镀与环保,2001;21(6):1
[15]Lee H T,Chen M H,Jao H M,Liao T L.Mater Sci Eng, 2003;A358:134
[1] XIAO Hong,XU Pengpeng,QI Zichen,WU Zonghe,ZHAO Yunpeng. Preparation of Steel/Aluminum Laminated Composites by Differential Temperature Rolling with Induction Heating[J]. 金属学报, 2020, 56(2): 231-239.
[2] Hua JI,Yunlai DENG,Hongyong XU,Weiqiang GUO,Jianfeng DENG,Shitong FAN. The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z[J]. 金属学报, 2019, 55(3): 376-388.
[3] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
[4] Jialin LIU, Yumin WANG, Guoxing ZHANG, Xu ZHANG, Lina YANG, Qing YANG, Rui YANG. Research on Single SiC Fiber Reinforced TC17 CompositesUnder Transverse Tension[J]. 金属学报, 2018, 54(12): 1809-1817.
[5] Zhi JIANG,Yanhong TIAN,Su DING. SYNTHESIS OF Sn3.5Ag0.5Cu NANOPARTICLE SOLDERS AND SOLDERING MECHANISM[J]. 金属学报, 2016, 52(1): 105-112.
[6] YANG Hao, HUANG Jihua, CHEN Shuhai, ZHAO Xingke, WANG Qi, LI Dehua. INFLUENCE OF THE COMPOSITION OF Zn-Al FILLER METAL ON THE INTERFACIAL STRUCTURE AND PROPERTY OF Cu/Zn-Al/Al BRAZED JOINT[J]. 金属学报, 2015, 51(3): 364-370.
[7] LIU Yi, JIANG Guofeng, XU Kun, LUO Ximing, CHEN Dengquan, LI Wei. EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING[J]. 金属学报, 2015, 51(2): 209-215.
[8] Pingguang XU,Jiang YIN,Shuyan ZHANG. TENSILE DEFORMATION BEHAVIOR OF HYDROGEN CHARGED ULTRAHIGH STRENGTH STEEL STUDIED BY IN SITU NEUTRON DIFFRACTION[J]. 金属学报, 2015, 51(11): 1297-1305.
[9] TAN Xianghu,SHAN Jiguo,REN Jialie. EFFECTS OF Cr PLATING LAYER ON SHEAR STRENGTH AND INTERFACE BONDING CHARACTERISTICS OF MILD STEEL/CFRP JOINT BY LASER HEATING[J]. 金属学报, 2013, 49(6): 751-756.
[10] ;. CRYSTALLOGRAPHIC ANALYSIS OF THE FRACTURE FACETS IN LOW TEMPERATURE BRITTLE FRACTURE OF A HIGH NITROGEN BEARING AUSTENITIC STEEL[J]. 金属学报, 2007, 43(12): 1233-1238 .
[11] . [J]. 金属学报, 2007, 43(10): 1037-1042 .
[12] ;. Numerical Simulation and Damage Fracture Prediction for Thick Sheet Metal Fine-blanking based on Mixed Displacement-Pressure FEM[J]. 金属学报, 2006, 42(10): 1115-1120 .
[13] LIANG Sizu; LIANG Yaoneng; LIU Zhengyi (South China University of Technology; Guangzhou). DIMPLE FORMATION ON FRACTURE SURFACE OF STEEL 55SiMnMo[J]. 金属学报, 1992, 28(10): 41-44.
[14] LIU Yongning;ZHU Jinhua;ZHOU Huijiu;A Kildegaard;J. A. Kristensen Department of Materials Science and Engineering; Xi'an Jiaotong University Department of Mechanical Engineering; Aalborg University; Denmark Department of Materials Science and Engineering;Xi'an Jiaotong University; Xi'an 710049. EFFECT OF LOADING RATE AND TEMPERATURE ON DUCTILE-BRITTLE TRANSITION OF A CARBON STEEL[J]. 金属学报, 1990, 26(3): 44-49.
No Suggested Reading articles found!