CA SIMULATION OF MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY
State Key Laboratory of Solidification Processing;Northwestern Polytechnical University
Cite this article: 

. CA SIMULATION OF MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY. Acta Metall Sin, 2008, 44(3): 365-370 .

Download:  PDF(927KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  24 July 2007     
ZTFLH:  TG115  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/365

[1]Boettinger W J,Coriell S R,Greer A L,Karma A,Kurz W,Rappaz M,Trivedi R.Acta Mater,2000;48:43
[2]Rappaz M,Rettenmayr M.Curt Opin Solid State Mater Sci,1998;3:275
[3]Zhu M F,Hong C P.ISIJ Int,2001;41:436
[4]Xu Q Y,Liu B C.Rare Met Mater Eng,2003;32:401 (许庆彦,柳百成.稀有金属材料与工程,2003;32:401)
[5]Hou S E,Zheng Y R,Chen R Z.Aeronaut Mater,1997; 17(1):10 (侯淑娥,郑运荣,陈荣章.航空材料学报,1997;17(1):10)
[6]Zhang G D,Yu H C,He Y H,Su B.Mater Eng,2007;5: 28 (张国栋,于慧臣,何玉怀,苏彬.材料工程,2007;(5):28)
[7]Nastac L.Acta Mater,1999;47:4253
[8]Nastac L,Stefanescu D M.Mater Sci Eng,1997;A54:391
[9]Liu D R.PhD Dissertation,Harbin Institute of Technol- ogy,2006 (刘东戎.哈尔滨工业大学博士学位论文,2006)
[10]Carter P,Cox D C,Gandin C A,Reed R C.Mater Sci Eng,2000;A280:233
[11]Li D Z,Su S F,Xu X H,Wang J Q,Chen J Z,Liu Y M. Foundry,1997;(8):1 (李殿中,苏仕方,徐雪华,王君卿,陈家芝,刘一鸣.铸造,1997;(8):1)
[12]Wang W,Lee P D,McLean M.Acta Mater,2003;51: 2971
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!