| The Evolution of Intermediate Transformation Microstructures in Mn-Mo-Nb-B Low Carbon Microalloyed Steel |
| SHANG Chengjia; WANG Xuemin; ZHOU Zhaojin; LIANG Xin; MIAO Chengliang;HE Xinlai |
| School of Materials Science and Engineering; University of Science and Technology Beijing |
|
Cite this article:
SHANG Chengjia; WANG Xuemin; ZHOU Zhaojin; LIANG Xin; MIAO Chengliang; HE Xinlai. The Evolution of Intermediate Transformation Microstructures in Mn-Mo-Nb-B Low Carbon Microalloyed Steel. Acta Metall Sin, 2008, 44(3): 287-291 .
[1]ISIJ.Atlas for Bainitic Microstructures (Vol.1),Tokyo: ISIJ,1992 [2]Krauss G,Thomposon T W.ISIJ Int,1995;35:937 [3]Ohtani H,Okaguchi S,Fujishro Y,Ohmori Y.Metall Trans,1990;21A:877 [4]Shang C J,Hu L J,Yang S W,Wang X M,Zhao Y T,He X L.Acta Metall Sin,2005;41:471 (尚成嘉,胡良均,杨善武,王学敏,赵运堂,贺信莱.金属学报,2005;41:471) [5]Zhao Y T,Shang C J,He X L,Guo H.Acta Metall Sin, 2006;42:54 (赵运堂,尚成嘉,贺信莱,郭晖.金属学报,2006;42:54) [6]Zhao Y T,Shang C J,Yang S W,Wang X M,He X L. Mater Sci Eng,2006;A433:169 [7]Mangonon P L.Merall Trans,1976;9A:1389 [8]Bhadeshia H K D H,Svensson L E,Gretoft B.Acta Met- all,1985;33:1271 [9]Bhadeshia H K D H,Svensson L E.J Mater Sci,1989;24: 3180 [10]Ali A,Bhadeshia H K D H.Mater Sci Technol,1991;7: 895 [11]Thompson S W,Colvin D J,Krass G.Metall Trans,1990; 21A:1493 [12]Habraken L J.Proc 4th Inter Conf on Electron Mi- croscopy.Berlin:Springer-Verlag,1958:621 [13]Suh D W,Kang J H,Oh K H,Lee H C.Scr Mater,2003; 48:91 [14]Chio Y,Choo W Y,Kwon D.Scr Mater,2001;45:1401 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|