| MAGNETOMECHANICAL COUPLING FACTOR (k33) OF Tb0.36Dy0.64(Fe0.85Co0.15)2 <110> ORIENTED CRYSTALS |
| BAI Xia-Bing 白夏冰;MA Tian-Yu; |
| 北京航空航天大学 |
|
Cite this article:
BAI Xia-Bing; MA Tian-Yu. MAGNETOMECHANICAL COUPLING FACTOR (k33) OF Tb0.36Dy0.64(Fe0.85Co0.15)2 <110> ORIENTED CRYSTALS. Acta Metall Sin, 2008, 44(10): 1231-1234 .
|
|
|
Abstract <110> oriented crystals Tb0.36Dy0.64(Fe0.85Co0.15)2 have been prepared by zone melting directional solidification method. The magnetomechanical coupling factor (k33) was determined by resonance/anti-resonance method in low bias fields. It was found that k33 is sensitive to both the bias field and the compressive pre-stress. Without compressive pre-stress, optimum k33 can be obtained with the value of 0.513 at a bias field of 50.9 kA/m. When applying a compressive pre-stress of 10 MPa, relatively lower k33 was obtained. It was attributed that extra energy of 71° domain wall is induced by the compressive pre-stress, which hinders the movement of magnetic moments or domain walls, decreasing the transition efficiency between the magnetic and mechanical energies.
|
|
Received: 22 February 2008
|
|
|
[1]Clark A E.Ferromagnetic Materials.Vol.1,Amsterdam: North-Holland,1980:531 [2]Jiles D C.Acta Mater,2003;51:5907 [3]Zhang T L,Jiang C B,Zhang H,Xu H B.Smart Mater Sturct,2004;13:473 [4]Greenough R D,Shulze M P,Jenner A G I,Wilkinson A J.IEEE Trans Magn,1991;27:5346 [5]Abell J S,Butler D,Greenough R D,Joyce V,Pitman K C.J Magn Magn Mater,1986;62:6 [6]Kendall D,Piercy A R.IEEE Trans Magn,1990;26:1837 [7]Jiang C B,Zhao Y,Xu H B.Acta Metall Sin,2004;40: 373 (蒋成保.赵岩,徐惠彬.金属学报,2004;40:373) [8]Ma T Y,Jiang C B,Xu H B.Appl Phys Lett,2005;86: 162505 [9]Zhao Y,Jiang C B,Zhang H,Xu H B.J Alloy Compd, 2003;354:263 [10]Bai X B,Jiang C B,Gong S K.Acta Metall Sin,2007;43: 413 (白夏冰,蒋成保,宫声凯.金属学报,2007;43:413) [11]Ma T Y,Yan M,Zhang J J,Luo W,Jiang C B,Xu H B. Appl Phys Lett,2007;90:102502 [12]Clark A E,Teter J P,McMasters 0 D.J Appl Phys,1988; 63:3910 [13]Branwood A,Janio A L,Piercy A R.J Appl Phys,1987; 61:3796 [14]Claeyssen F,Colombani D,Tessereau A,Ducros B.IEEE Trans Magn,1991;27:53432 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|