The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds
许良红 Xu Liang-Hong;tian zhiling Tian
钢铁研究总院结构
Download:  PDF(491KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure in the partially melted zone of an arc-welded 20mm thickness 2519-T87 high strength aluminum alloy is investigated, an oriented precipitate-free zone is found behind the grain boundary, and this zone is not uniformly surrounding the grain, but usually oriented toward the fusion line. The formation mechanism of this zone is also studied. Results indicate that the mechanism of grain boundary liquid film migration is favored the formation of the precipitate free zone, the driving forces include coherency strain energy, the differential strain energy between the two grains induced by the elastic stresses generated during welding and differential surface energy due to grain boundary curvature. And with the increase of heat input, the thickness of the precipitate free zone increase. The precipitate free zone is harmful to the mechanical property of partially melted zone, and the fractography of PMZ showing the intergranular fracture.
Key words:  high strength aluminum alloy      partially melted zone      driving force      grain boundary migration      
Received:  20 March 2007     
ZTFLH:  TG146.2  
  TG457.1  
Corresponding Authors:  许良红 Xu Liang-Hong     E-mail:  xlh_smile@sohu.com

Cite this article: 

许良红 Xu Liang-Hong; tian zhiling Tian. The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds. Acta Metall Sin, 2008, 44(1): 91-97 .

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I1/91

[1]Kramer L S,Blair T P,Blough S D,Pickens J R.Mater Eng Perform,2002;11:645
[2]Carter H B,David H E,Ashok S.Eng Fract Mech,1999; 62(1):1
[3]Fisher J,James J.Adv Mater Process,2002;160(9):43
[4]Devincent S M,Devletian J H,Gedeon S A.Weld J,1988; 67(7):33
[5]Huang C,Kon S.Weld J,2001;80(1):9
[6]Srinivasa R,Madhusudhana R,Prasad R.Mater Sci Eng, 2005;A403:69
[7]Ojo O A,Richards N L,Chaturvedi M C.Scr Mater,2004; 51:141
[8]Bj(?)rneklett B I,Grong (?),Myhr O R,Kluken A O.Sci Technol Weld Joining,1999;4:161
[9]Meyer B C,Doyen H,Emanowski D,Hirsch T,Mayr P. Metall Mater Trans,2000;31A:1454
[10]Wilson A.PhD Thesis,Pennsylvania State University, 2001
[11]Huang C,Kou S.Weld J,2001;80(2):46
[12]Huang C,Kou S.Weld J,2000;79(5):113
[13]Cahn J W.Acta Metall,1961;9:795
[14]Kuo M,Fournelie R A.Acta Metall Mater,1991;39:2835
[15]Barker S W,Purdy G R.Acta Mater,1998;46:511
[16]Nakkalil R,Richards N L,Chaturvedi M C.Acta Metall Mater,1993;41:3381
[17]Ryosnke K,Ikuo O,Kiyohito I.Mater Trans,2003;44: 1768
[18]Tian R Z,Wang Z T.Aluminum and Its Workin9 Hand Book.Changsha:Central and South University Press, 2000:97 (田荣璋,王祝堂.铝合金及其加工手册.长沙:中南大学出版社,2000:97)
[1] ZHANG Xinming, DENG Yunlai, ZHANG Yong. DEVELOPMENT OF HIGH STRENGTH ALUMINUM ALLOYS AND PROCESSING TECHNIQUES FOR THE MATERIALS[J]. 金属学报, 2015, 51(3): 257-271.
[2] ZHOU Deqiang, LIU Xiongjun, WU Yuan, WANG Hui, LV Zhaoping. RECRYSTALLIZATION BEHAVIOR AND ITS INFLU- ENCES ON MECHANICAL PROPERTIES OF AN ALUMINA-FORMING AUSTENITIC STAINLESS STEELS[J]. 金属学报, 2014, 50(10): 1217-1223.
[3] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. CALCULATION OF TRANSFORMATION DRIVING FORCE FOR THE PRECIPITATION OF NANO-SCALED CEMENTITES IN THE HYPOEUTECTOID STEELS THROUGH ULTRA FAST COOLING[J]. 金属学报, 2013, 49(1): 26-34.
[4] CAO Yu DI Hongshuang ZHANG Jiecen ZHANG Jingqi MA Tianjun. RESEARCH ON DYNAMIC RECRYSTALLIZATION BEHAVIOR OF INCOLOY 800H[J]. 金属学报, 2012, 48(10): 1175-1185.
[5] CONG Baoqiang QI Bojin ZHOU Xingguo LUO Jun. INFLUENCES OF ULTRASONIC PULSE SQUARE-WAVE CURRENT PARAMETERS ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 2219 ALUMINUM ALLOY WELD JOINTS[J]. 金属学报, 2009, 45(9): 1057-1062.
[6] Na Wang; Zhenmin Du. Driving Force for the Nucleation from Supercooled Liquid and Thermodynamic Analysis of Glass Forming Ability for Binary Alloys[J]. 金属学报, 2008, 44(9): 1111-1115 .
[7] XIONG Ying. A TWO-PARAMETER DRIVING FORCE FOR FATIGUE CRACK GROWTH[J]. 金属学报, 2008, 44(11): 1348-1353 .
[8] TIAN Sugui ; ZHOU Huihua ; ZHANG Jinghua; YANG Hongcai ; XU Yongbo;HU Zhuangqi ( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)( Department of Materials Science and Engineering; Northeastern University ; Shenyang 110006)( Department of Materials Science and Engineering; Shenyang Polytechnic University; Shenyang 110023)Correspondent: TIAN Sugui; associate professor Tel: (024)5927399. A DIRECTIONAL COARSENING MECHANISM OF THE γ'-PHASE DURING CREEP OF A SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(6): 591-596.
[9] (TIAN Sugui ; ZHOU Huihua; ZHANG Jinghua;YANG Hongcai;XU YOngboHU Zhuangqi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal ReSearch; The Chinese Academyof Sciences; Shenyang 110015)(Department of Materials Sciences and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials Engineering; Shenyang Polytechnic University 110023)Correspondent:TIAN Sugui; associate professor; Tel: (o24)-25927399; Fax: (024)e3891s2oManuscript received 1997-12-23; in revised form 1998-03-16. DIRECTIONAL COARSENING OF THE γ'-PHASE DURING COMPRESSION CREEP OF A SINGLE CRVSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(12): 1261-1266.
[10] YANG Liu;LIU Shikai;YANG Ping Southwest Jiaotong University; Chengdu. CALCULATION OF BAINIT TRANSFORMATION KINETICS IN Fe-C-Si-Mn ALLOYS[J]. 金属学报, 1993, 29(1): 1-5.
[11] LIN Guangming;HUANG Yuanshi;ZHANG Jinxiu Zhongshan University; Guangzhou LIN Guangming; Associate Professor; Department of Physics; Zhongshan University;Guongzhou 510275. TRANSFORMATION OF TWO WAY SHAPE MEMORY MATERIAL CONSTRAINED BY STRESS[J]. 金属学报, 1989, 25(6): 16-21.
[12] XIE Changsheng;SUN Peizhen;CHEN Yuqiu;ZHAO Jiansheng Huazhong University of Science and Technology. QUASI-EQUILIBRIUM MICROSTRUCTURES AND EFFECT OF ALLOY ELEMENTS IN Fe-Mn-Ni-Cr STEELS[J]. 金属学报, 1989, 25(4): 54-59.
No Suggested Reading articles found!