Abstract Cu-12% Ag (mass fraction) strengthened by double-phase filamentary composite was prepared by heavy drawing. The effect of annealing temperature on the intensity and distribution of crystal texture in both Cu and Ag phases was investigated by annealing the composite at different temperatures. With the increase of annealing temperature up to 400 °C, the <111> component intensity decreases and the <100> component intensity increases in Cu phase while the <111> component intensity in Ag phase changes insignificantly. Annealing at temperatures higher than 400 °C enhances the texture intensities in both Cu and Ag phases. The texture formed by heavy drawing in Ag phase is more stable than that in Cu phase for the composite annealed at lower temperatures. The interface migrating, structure aggregating, fiber glomerating, and grain propagating from recover and recrystallization in annealing process generally change the intensities of the texture components formed by heavy drawing to form annealing texture. Therefore, the annealing texture components have the same orientation indexes as the deformation texture components.
|
|
Received: 18 April 2007
|
|
|
[1]Zhang L,Yan F,Meng L.Mater Rev,2003;17(5):15 (张雷,颜芳,孟亮.材料导报,2003;17(5):15) [2]Benghalem A,Morris D G.Acta Mater,1997;45:397 [3]Maeda H,Inoue K,Kiyoshi T,Asano T,Sakai Y,Takeuchi T.Physica,1996;216B:141 [4]Freudenberger J,Kozlova N,Gaganov A,Schultz L,Witte H,Jones H.Cryogenics,2006;46:724 [5]Grünberger W,Heilmaier M,Schultz L.Physica,2001; 643B:294 [6]Ohsaki S,Yamazaki K,Hono K.Scr Mater,2003;48:1569 [7]Sakai Y,Schneider-Muntau H J.Acta Mater,1997;45: 1017 [8]Han K,Vasquez A A,Xin Y,Kalu P N.Acta Mater,2003; 51:767 [9]He J,Liu J B,Meng L.Acta Metall Sin,2007;43:643 (贺佳,刘嘉斌,孟亮.金属学报,2007;43:643) [10]Hong S I,Hill M A.Acta Mater,1998;46:4111 [11]Hong S I,Hill M A.Mater Sci Eng,1999;A264:151 [12]Kwon H J,Hong S I.J Alloys Compd,2001;32:161 [13]Yan F,Meng L,Zhang L.Acta Metall Sin,2004;40:891 (颜芳,孟亮,张雷.金属学报,2004;40:891) [14]Yang J X.Physical Foundation of Metals Plastic Defor- mation.Beijing:Metallurgical Industry Press,1988:248 (杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988:248) [15]Zhang X Y.Crystal Texture of Metals and Alloys.Beijing: Science Press,1976:79 (张信钰.金属和合金的织构.北京:科学出版社,1976:79)V |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|