    					| THE OBSERVATION AND ANALYSIS OF ε-Cu PHASE IN THE CU CONTAINING ANTIBACTERIAL AUSTENITESTAINLESS STEEL | 
  					 
  					  										
						| hengwu li;; | 
					 
															
						| 上海天宝不锈钢有限公司 | 
					 
										
						 | 
					 
				 
				
				Cite this article: 
				
					
			      hengwu li. THE OBSERVATION AND ANALYSIS OF ε-Cu PHASE IN THE CU CONTAINING ANTIBACTERIAL AUSTENITESTAINLESS STEEL. Acta Metall Sin, 2008, 44(1): 39-42        .	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract  The paper presented Some results about ε-Cu phases formed during antibacterial treatment in the antibacterial stainless steel by LM,X-Ray, SEM,EPM and TEM, and then discussed form process ε-Cu phases.
																										     | 
														 
												  		
														
															| 
															    																	Received:  10 April 2007
																	    
															    															    															  
															 | 
															
														 
														 														
															| 
																
															 | 
														 
																																									    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  
															  [1]Nakamura S,Ookubo N,Miyakusu K,Hasegawa M.Nis- shin Steel Technical Rep,1997;76:48 (中村定幸,大久保直人,宫楠克久,长谷川守弘.日新制钢技报,1997;76:48)  [2]Ookubo N,Nakamura S,Yamamoto M,Miyakusu K, Hasegawa M.Nisshin Steel Technical Rep,1998;77:61 (大久保直人,中村定幸,山本正人,宫楠克久,长谷川守弘日新制钢技报,1998;77:61)  [3]Yamamoto M.Spec Steels,1999;48(6):24 (山本正人.特殊钢,1999;48(6):24)  [4]Yokota T,Tochihara M,Ohta M.Kawasaki Steel Technol Rep,2001;33:88 (横田毅,枥原美佐子,太田稚之.川崎制铁技报,2001;33:88)  [5]Yang K,Chen S H,Dong J S,LüM Q.Met Funct Mater, 2005;12(6):6 (杨柯,陈四红,董加胜,吕曼祺.金属功能材料,2005;12(6):6)  [6]Chen S H,LüM Q,Zhang J D,Dong J S,Yang K.Acta Metall Sin,2004;40:314 (陈四红,吕曼祺,张敬党,董加胜,杨柯.金属学报,2004;40:314  [7]LüM Q,Chen S H,Dong J S,Yang K.Met Funct Mater, 2005;12(6):10 (吕曼祺,陈四红,董加胜,杨柯.金属功能材料,2005;12(6):10)  [8]Zhang T B,Zhang T Y.Chin Pat,ZL 02 1 48742.1,2007 (张体宝,张体勇.中国发明号利,ZL02148742.1,2007)  [9]Zhou J,Chang X,Guo K X.Acta Metall Sin,1978;14: 246 (周敬,常昕,郭可信.金属学报,1978;14:246)  [10]Zhou Y X,Huang Q Z,Chen Q T,Deng D Q,Pu S K. Acta Metall Sin,1978;14:292 (周永忻,黄清珠,陈乾惕,邓定庆,蒲绍康.金属学报,1978;14:292)  [11]Thompson S W,Krauss G.Metall Mater Trans,1996; 27A:1573	 | 
														   
																											 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |