| RAPID DIRECTIONAL SOLIDIFICATION AND ITS SIMULATION OF Al-Pb ALLOYS |
| ZHANG Qin-Xia;;; |
| 中国科学院金属研究所 |
|
Cite this article:
ZHANG Qin-Xia. RAPID DIRECTIONAL SOLIDIFICATION AND ITS SIMULATION OF Al-Pb ALLOYS. Acta Metall Sin, 2007, 43(9): 925-929 .
|
|
|
Abstract Rapid directional solidification experiments were carried out with Al-Pb alloy. The microstructure evolution during the solidification was calculated according to the practical experimental conditions. The results indicate that, under a constant solidification velocity, the size and its distribution width of the minority phase droplets increases with the Pb content of the alloy. For an alloy of given composition, the size and its distribution width of the minority phase droplets decreases with the solidification velocity. The numerical results, which have an acceptable coincidence with the experimental ones, show the microstructure evolution process clear.
|
|
Received: 06 March 2007
|
|
|
[1]Walter H U.Materials Science in Space.New York: Springer Verlag,1986:343 [2]Pratt G C.Int Met Rev,1973;18:62 [3]Inoue A,Yano N.J Mater Sci,1987;22:123 [4]Zhao J Z,Ratke L.Scr Mater,1998;39:181 [5]Ahlborn H,Diefenbach S,Neumann H,Prinz B,Ratke L, Romero A.Mater Sci Eng,1993;A173:133 [6]Xian A P,Zhang X M,Li Z Y,Liu Q Q,Chen J Z,Li Y Y.Acta Metall Sin,1996,32:113 (冼爱平,张修睦,李忠玉,刘清泉,陈继志,李依依.金属学报,1996;32:113) [7]Zhao J Z,Hu Z Q.Acta Metall Sin,2004;40:27 (赵九洲,胡壮麒.金属学报,2004;40:27) [8]Su Y Q,Cui H B,Guo J J,Liu Y,Jia J.Foundry,2002; 51:618 (苏彦庆,崔红保,郭景杰,刘源。贾均.铸造,2002;51:618) [9]Liu X R,Lu X Y,Wei B B.Sci Chin,2004;34E:1234 (刘向荣,鲁晓宇,魏炳波.中国科学,2004;34E:1234) [10]Zhu D Y,Yang X H,Han X J,Wei B B.Chin J Nonferrous Met,2003;13:328 (朱定一,杨晓华,韩秀君,魏炳波.中国有色金属学报,2003;13:328) [11]He J,Zhao J Z,Wang X F,Li Z Y.Acta Metall Sin,2006; 42:67 (何杰,赵九洲,王晓峰,李中原.金属学报,2006;42:67) [12]Yang S,Liu W J,Jia J.Mater Sci Technol,2002;10(1): 19 (杨森,刘文今,贾均.材料科学与工艺,2002;10(1):19) [13]Prinz B,Romero A,Ratke L.J Mater Sci,1995;30:4715 [14]Prinz B,Romero A.In:Ratke L,ed.,Immiscible Liq- uid Metals and Organics,Oberursel,Germany:DGM- Informationsgesellschaft,1993:281 [15]Weibel E R.Stereological Methods.Vol.2,New York:Aca- demic Press,1980:175 [16]Jia J,Zhao J Z,Guo J J,Liu Y.Immiscible Alloys and Their Preparation Techniques.Harbin:Harbin Institute of Technology Press,2002:199 (贾均,赵九洲,郭景杰,刘源.难混溶合金及其制备技术.哈尔滨:哈尔滨工业大学出版社,2002:199) [17]Zhao J Z,Drees S,Ratke L.Mater Sci En9,2000:A282: 262P |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|