HOT DEFORMATION BEHAVIOR AND CONSTITUTIVE RELATIONSHIP OF NiTi SHAPE MEMORY ALLOY DURING COMPRESSION AT ELEVATED TEMPERATURES
;;;
北京科技大学
Cite this article:
;. HOT DEFORMATION BEHAVIOR AND CONSTITUTIVE RELATIONSHIP OF NiTi SHAPE MEMORY ALLOY DURING COMPRESSION AT ELEVATED TEMPERATURES. Acta Metall Sin, 2007, 43(9): 930-936 .
Abstract The hot deformation behavior of NiTi alloy was studied by compressive deformation tests in the strain rate range 0.001-10s-1 and temperature of 700-900℃, and associated structural changes were investigated by observations of metallography and TEM. By using regression analysis methods based on measured data, the material parameters of the Arrhenius-type hyperbolic-sine equation were resolved, and then fitted against deformation strains. Based on the above analysis, a constitutive equation which related the flow stress to temperature, strain rate and strain was established. The activation energy, Q, and lnA, decrease as the strain increases. However, the stress exponent, n, linearly increases with the increase of the strain. The main reasons that lead to the difference between the true stress-true strain curves of NiTi alloy and those of non-intermetallic materials are reciprocal order-disorder transition and dynamic recovery or dynamic recrystallization.
[1]Kawaguchi Y,Katsube K,Murahashi M,Yamada Y.Wire J Int,1991;24:53 [2]Liu X F,He Y,Bi C W,Xie J X.Chin J Rare Met,2005; 29:762 (刘雪峰,何勇,毕重武,谢建新.稀有金属,2005;29:762) [3]Zhang S H,Wang Z T,Zhang W H.Machinist Met Form- ing,2005;(7):16 (张士宏,王忠堂,张伟红.机械工人:热加工,2005;(7):16) [4]Zhang W H,Zhang S H.Acta Metall Sin,2006;42:1036 (张伟红,张士宏.金属学报,2006;42:1036) [5]Li L,Zhou J,Duszczyk J.J Mater Process Technol,2006; 172:372 [6]Krauss G.Defornation Processing and Structure.Metals Park,OH:American Society for Metals,1984:109 [7]Rao K P,Prasad Y K D V,Hawbolt E B.J Mater Process Technol,1996;56:897 [8]Rao K P,Hawbolt E B.ASME J Eng Mater Technoly, 1992;114:116 [9]Yuan H,Liu W C.Mater Sci Eng,2005;A408:281 [10]Lyszkowski R,Bystrzycki J.Intermetallics,2006;14:1231 [11]Otsuka K,Ren X B.lntermetallics,1999;7:511 [12]Chen G L,Lin J P.Physical Metallography Basis of Or- dered Intermetallic Compound Structure Materials.Bei- jing:Metallurgical Industry Press,1999:140 (陈国良,林均品.有序金属间化合物结构材料物理金属学基础.北京:冶金工业出版社,1999:139) [13]Lou B Y,Liu M S,Mao Z Y.Mater Sci Eng,1995;13(2): 19 (楼白杨,刘茂森,毛志远.材料科学与工程,1995;13(2):19)
SHEN Huimin;HU Meishen;GUI Jianmin;YUAN Fang;WANG Yening;GUO Jinfang;QIAN Dongfan Institute of Solid State Physics; Nanjing University; General Research Institute for Non-Ferrous Metals; Beijing. PRE-TRANSITION AND PSEUDO-ELASTICITY IN NiTi (Fe) ALLOY[J]. 金属学报, 1988, 24(2): 84-88.