| Glass--Forming Ability and Soft Magnetic Properties of Fe--Co--Nd--Nb—B Amorphous Alloys |
| XU Min; SUN Yu; QUAN Mingxiu;WANG Yandong; ZUO Liang |
| henyang National Laboratory for Materials Science; Institute of Metal Research;Chinese Academy of Sciences |
|
Cite this article:
XU Min; SUN Yu; QUAN Mingxiu; WANG Y; ong; ZUO Liang. Glass--Forming Ability and Soft Magnetic Properties of Fe--Co--Nd--Nb—B Amorphous Alloys. Acta Metall Sin, 2007, 43(7): 699-704 .
|
|
|
|
|
Received: 10 January 2007
|
|
|
[1]Duwez P,Lin S C H.J Appl Phys,1967;38:4096 [2]Masumoto T,Kimura H M,Inoue A,Waseda Y.Mater Sci Eng,1976;24:141 [3]Kikuchi M,Fujimori H,Obi T,Masumoto T.Jpn J Appl Phys,1975;14:1077 [4]Inoue A,Masumoto T,Arakawa S,Iwadachi T.In:Canter Bed,Rapidly Quenched MetalsⅢ,London:The Metals Society,1978:265 [5]Inoue A,Kobayashi K,Kanehira J,Masumoto T.Sci Rep Res Inst Tohoku Univ,1981;29A:331 [6]Raskin D,Smith C H.In:Luborsky F E ed,Amorphous Metallic Alloys,London:Butterwoths,1983:381 [7]Smith C H.In:Liebermann H H ed,Rapidly Solidified Alloys,New York:Marcel Dekker,1993:617 [8]Davies H A.In:Luborsky F E ed,Amorphous Metallic Alloys,London:Butterwoths,1983:14 [9]Johnson W L.MRS Bull,1999;24(10):42 [10]Shen T D,Schwarz R B.Appl Phys Lett,1999;75:49 [11]Inoue A.Acta Mater,2000;48:279 [12]Wang W H,Dong C,Shek C H.Mater Sci Bng,2004; R44:45 [13]Inoue A,Gook J S.Mater Trans JIM,1995;36:1282 [14]Inoue A,Zhang T,Takeuchi A,Murakami A,Makino A. IEEE Trans Magn,1996;32:4866 [15]Inoue A,Zhang T,Itoi T,Takeuchi A.Mater Trans JIM, 1997;38:359 [16]Inoue A,Zhang T,Takeuchi A.Appl Phys Lett,1997;71: 464 [17]Shen T D,Schwarz R B.Acta Mater,2001;49:837 [18]Zhang W,Inoue A.Mater Trans,2001;42:1142 [19]Zhang W,Inoue A.Mater Trans,2001;42:1835 [20]Lu Z P,Liu C T.Acta Mater,2002;50:3501 [21]Lu Z P,Liu C T.Phys Rev Lett,2003;91:115505 [22]Turnbull D.Contemp Phys,1969;10:473 [23]Inoue A,Shibata T,Zhang T.Mater Trans JIM,1995;36: 1420 [24]Imafuku M,Yaoita K,Sato S,Zhang W,Inoue A,Waseda Y.Mater Sci Eng,2001;A304-306:660 [25]Granshaw T E,Longworth G.In:Long G J ed,M(?)ssbauer Spectroscopy Applied to Inorganic Chemistry.Vol 1, NewYork:Plenum,1984:173 [26]Ok H N,Morrish A H.J Phys,1981;11 F:1495 [27]Soresue M,Knobbe E T.Phgs Rev,1994;49 B:3253 [28]Kong H Z,Li Y,Ding J.J Magn Magn Mater,2000;217: 65 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|