| Ultra-high cycle fatigue behavior of Ti-6Al-4V alloy |
| ZUO Jinghui; WANG Zhongguang; HAN Enhou |
| Environmental Corrosion Center; Institute of Metal Research; Chinese Academy of Sciences |
|
Cite this article:
ZUO Jinghui; WANG Zhongguang; HAN Enhou. Ultra-high cycle fatigue behavior of Ti-6Al-4V alloy. Acta Metall Sin, 2007, 43(7): 705-709 .
|
|
|
|
|
Received: 16 November 2006
|
|
|
[1]Li X W,Xia S Y,Sha A X.Acta Metall Sin,2002;38(增刊):S277 (李兴无,夏绍玉,沙爱学.金属学报,2002,38(Suppl.):S277) [2]Tobler R L.ASTM STP 601,1976:346 [3]Williams 3 C,Starke E A.Acta Mater,2003;51:5775 [4]Bathias C.Fatigue Fract Eng Mater Struct,1999;22:559 [5]Bathias C,Drouillac L,le Francois P.Int J Fatigue,2001; 23:143 [6]Yang Z G,Li S X,Zhang J M,Zhang J F,Li G Y,Li Z B,Hui W J,Weng Y Q.Acta Mater,2004;52:5235 [7]Cao W D,Zhou Y G.Acta Metall Sin,2002;1273 (曹卫东,周义刚.金属学报,2002,38:1273 [8]Eylon D,Pierce C M.Metall Tran,1976;7A:111 [9]Papakyriacou M,Mayer H,Pyper C,Plenk H,Stanzl- Tschegg S E.Mater Sci Eng,2001;A308:143 [10]Shu D L.Mechanical Performance of Metals.Beijing: China Mathine Press,1995:19 (束德林.金属力学性能.北京:机械工业出版社,1995:19) [11]Ritchie R O,Boyce B L,Campbell J P,Roder O,Thomp- son A W,Milligan W W.Int J Fatigue,1999;21:653 [12]Morrissey R J,Mcdowell D L,Nicholas T.Int J Fatigue, 1999;21:679 [13]Wang Q Y,Beard J Y,Dubarre A,Baudry G,Rathery S, and Bathias C.Fatigue Fracture Eng Mater Struct,1999, 22:667 [14]Morrissey R J.Nicholas T.Int J Fatigue,2006;28:1577 [15]Morrissey R J,Nicholas T.Int J Fatigue,2005,27:1608 [16]Tens A,Hoffelner W,Duerig T W,Allison J E.Scr Metall, 1983;17:601 [17]Osamu Umezawa,Kotobu Nagai.ISIJ Int,1997;37:1170 [18]Ravichandran K S.Acta Metall Mater,1991;39:401 [19]Nalla R K,Boyce B L,Campbell J P,Peters J O,Ritchie R O.Metall Mater Trans,2002;33A:899 [20]Eylon D.J Mater Sci,1979;14:345B |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|