Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy
;;;
Cite this article: 

;. Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy. Acta Metall Sin, 2007, 43(5): 477-481 .

Download:  PDF(467KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  High boron iron-base alloy is a new kind of wear-resistant material, which takes borides as wear-resistant phases. In structure, matrixes and borides were included in as-cast condition and the matrixes were changed with different alloying elements and quantity. Borides were distributed in the shape of continuous net in the structure of high boron iron-base alloy. When the melt was solidified in metal mould and sand mould respectively, the grain size of austenitic primary crystal decreases with the cooling rate increase. In addition, the morphology of borides was changed greatly. After heat treatment, borides of samples made of sand mould were changed little, otherwise, borides of samples made of metal mould were changed to granulation shape and the impact toughness was increased by 60%..
Key words:  high boron iron-base alloy      borides      solidification condition      
Received:  01 September 2006     
ZTFLH:  TG113.22  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I5/477

[1] Guo C Q, Gao S Z. Foundry, 2004; 53: 761 (郭长庆,高守忠.铸造,2004;53:761)
[2] Gol'dshtein Y E, Mizin V G. Met Sci Heat Treat, 1989; 30: 479
[3] Egorov E D, Sapozhnikov Yu L, Shakhnazarov Yu V. Met Sci Heat Treat, 1989; 31: 387
[4] Lorinczi J, Kralik G, Kovaces M, Horvath A. Mater Sci Forum, 2003; 414-415: 267
[5] Baarman M H. Scand J Metall, 1998; 27: 157
[6] Okita T, Wolfer W G, Garner F A, Sekimura N. J Nucl Mater, 2004; 329-333: 1013
[7] Middleham T H, Rait J R, Colbeck E W. J Iron Steel Inst, 1957; 187(1): 1
[8] Llewellyn D T. Ironmaking Steelmaking, 1993; 20: 338
[9] Taylor K A, Hansen S S. Metall Trans, 1990; 21A: 1706
[10] Wang X M, He X L. ISIJ Int, 2002; 42(Suppl.): 38
[11] The First Steel Works of Benxi Steel Corp. Boron Steel. Beijing: Metallurgical Industry Press, 1977: 2 (本溪钢铁公司第一炼钢厂.硼钢.北京:冶金工业出版社,1977: 2)
[12] Ren Y H. Spec Steel, 1992; 13(5): 57 (任元和.特殊钢,1992;13(5):57)
[13] Abenojar J, Velasco F, Martinez M A. J Mater Process Technol, 2003; 143-144: 28
[14] Palumbo M, Cacciamani G, Bosco E, Baricco M. Inter- metallics, 2003; 11: 1294
[15] Yang C L, Yang G C, Liu F, Chen Y Z, Liu N, Chen D, Zhou Y H. Physica, 2006; 373B: 136L
[1] HU Qiang ZENG Xierong QIAN Haixia XIE Shenghui SHENG Hongchao. CORRELATION BETWEEN THE GLASS-FORMING ABILITY AND CHARACTERISTIC FREE VOLUMES OF THE IRON BASE BULK METALLIC GLASSES[J]. 金属学报, 2012, 48(11): 1329-1334.
[2] WU Jie CUI Hongzhi CHI Jing YAO Shuyu HAN Fusheng. INTERNAL FRICTION PEAK IN B2 Fe--Al ALLOYS DURING ORDERING PROCESS[J]. 金属学报, 2009, 45(4): 396-399.
[3] XIAO Fu ZHAO Xinqing XU Huibin JIANG Haichang RONG Lijian. DAMPING CAPACITY AND MECHANICAL PROPERTY OF
NiTiNb SHAPE MEMORY ALLOYS
[J]. 金属学报, 2009, 45(1): 18-24.
[4] ZHANG Congyang ZHU Jie ZHANG Maocai. NEGATIVE THERMAL EXPANSION PHENOMENA\par OF Mn3(Cu1-xGexN[J]. 金属学报, 2009, 45(1): 97-101.
[5] Bai-Gang JIN. NUMERICAL SIMULATION OF ELECTROMAGNETISM PARAMETERS AND STRUCTURE PARAMETERS IN TWO-STAGE SLIT-LESS MOLD[J]. 金属学报, 2007, 43(4): 427-432 .
[6] FU Hanguang. A Study of Abrasion Resistant Cast Fe-B-C Alloy[J]. 金属学报, 2006, 42(5): 545-548 .
[7] . [J]. 金属学报, 2006, 42(4): 411-414 .
[8] Honglin Jiang. MAGNETOSTRICTION AND MICROSTRUCTURE OF THE MELT-SPUN Fe83Ga17 ALLOY[J]. 金属学报, 2006, 42(2): 177-180 .
[9] WANG Lianwen; XIAN Aiping; SHAO Hanru. Density Measurement of Liquid Indium Using r--Ray Attenuation Method[J]. 金属学报, 2004, 40(6): 643-.
[10] WANG Yugui; QIAO Lijie; GAO Kewei; SU Yanjing; CHU Wuyang; WANG Zhonglin. Measurement of the Fracture Toughness and Critical Stress for Cracking in SnO2 Nanobelts Using Nanoindentation[J]. 金属学报, 2004, 40(6): 594-.
[11] WANG Hongbin; WANG Xiaoyu; ZHANG Jihua; XU Zuyao T. Y. Hsu. Internal Friction of Nano--Grained Fe--25\%Ni Alloy Bulk[J]. 金属学报, 2004, 40(5): 523-526 .
[12] . [J]. 金属学报, 2003, 39(11): 1225-1227 .
[13] . [J]. 金属学报, 2003, 39(11): 1139-1144 .
[14] . [J]. 金属学报, 2003, 39(11): 1170-1172 .
[15] . [J]. 金属学报, 2003, 39(11): 1163-1166 .
No Suggested Reading articles found!