DEVELOPMENT OF A NEW HIGH STRENGTH AND GOOD HOT CORROSION RESISTANCE FOR LOW SEGREGATION SUPERALLOY DZ68
Cite this article: 

. DEVELOPMENT OF A NEW HIGH STRENGTH AND GOOD HOT CORROSION RESISTANCE FOR LOW SEGREGATION SUPERALLOY DZ68. Acta Metall Sin, 2007, 43(4): 422-426 .

Download:  PDF(457KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A more homogeneous microstructure and more alloying of alloys can be obtained by controlling segregation during solidification, so properties of alloys can be improved. For directional solidification (DZ) of turbine blades,a new nickel-base superalloy DZ68, which makes use of low-segregation, is developed. This superalloy can meet the need of engine operation under offshore condition. Besides the hot corrosion resistance, DZ68 possesses an outstanding property of the high-strength aero engine blade material. This paper mainly studies properties of mechanic and hot corrosion resistance. It is shown that DZ68 possesses an excellent performance of hot corrosion resistance similar to DZ38G(In738)and shows mechanical properties equivalent to DZ125.
Key words:  Low-segregation      High temperature strength      Hot corrosion      
Received:  21 July 2006     
ZTFLH:  TG111.4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/422

[1]Miki Y,Takeuchi S.ISIJ Int,2003;43:1548
[2]Wang Z,Mukai K,Ma Z Y,Nishi M,Tsukamoto H,Shi F.ISIJ Int,1999;39:795
[3]Huang X,Thomas B G.Can Metall Q,1998;37:197
[4]Kubo N,Ishii T,Kubota J,Aramaki N.ISIJ Int,2002; 42:1251
[5]Takatani K.ISIJ Int,2003;43:915
[6]Nagai J,Suzuki K I,Kojima S,Kollberg S.Iron Steel Eng, 1984;61(5):41
[7]Yamamura H,Toh T,Harada H,Takeuchi E,Iahii T.ISIJ Int,2001;41:1229
[8]Suzuki M,Nakada M.ISIJ Int,2001;41:670
[9]Haxada H,Takeuchi E,Zeze M,Ishii T.Testu Hagané,2000;86:278 (原田宽,竹内栄,濑昌文,石井孝宣.铁钢,2000; 86:278)
[10]Harada H,Toh T,Ishii T,Kaneko K,Takeuchi E.ISIJ Int,2001;41:1236
[11]Takatani K,Tanizawa Y,Mizukami H,Nishimura K.ISIJ Int,2001;41:1252
[12]Bessho N,Yoda R,Yamasaki H,Fujii T,Nozaki T,Taka- tor S.ISIJ Int.1991;31:40
[1] WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia. Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy[J]. 金属学报, 2021, 57(6): 780-790.
[2] Yimin LIAO, Min FENG, Minghui CHEN, Zhe GENG, Yang LIU, Fuhui WANG, Shenglong ZHU. Comparative Study of Hot Corrosion Behavior of theEnamel Based Composite Coatings and the ArcIon Plating NiCrAlY on TiAl Alloy[J]. 金属学报, 2019, 55(2): 229-237.
[3] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[4] Chengyang JIANG, Yingfei YANG, Zhengyi ZHANG, Zebin BAO, Shenglong ZHU, Fuhui WANG. Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. 金属学报, 2018, 54(4): 581-590.
[5] Xin PENG, Sumeng JIANG, Xudong SUN, Jun GONG, Chao SUN. CYCLIC OXIDATION AND HOT CORROSION BEHAVIORS OF A GRADIENT NiCoCrAlYSi COATING[J]. 金属学报, 2016, 52(5): 625-631.
[6] Haigen ZHAO,Shusuo LI,Yanling PEI,Shengkai GONG,Huibin XU. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni3Al-BASED SINGLE CRYSTSAL ALLOY IC21[J]. 金属学报, 2015, 51(10): 1279-1287.
[7] JING Yanhong, LIU Enze, ZHENG Zhi, TONG Jian, Ning Likui, HE Ping. HOT CORROSION RESISTANCE OF FILLER ALLOY BCo46[J]. 金属学报, 2014, 50(1): 79-87.
[8] LI Haizhao, ZHANG Ji. HIGH TEMPERATURE STRENGTH AND AMBIENT DUCTILITY DEPENDENCES ON Al CONTENTS OF HIGH Nb CONTAINING TiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1423-1427.
[9] LU Xuyang, YU Daqian, JIANG Sumeng, LIU Shanchuan, GONG Jun, SUN Chao. HOT CORROSION BEHAVIOR OF A (NiCoCrAlYSiB+AlSiY) COMPOSITE COATING[J]. 金属学报, 2012, 48(4): 461-468.
[10] LV Jiaxin; ZHENG Lei; ZHANG Maicang; DONG Jianxin. CORROSION BEHAVIOR OF NICKEL BASE ALLOY FGH95 IN MOLTEN NaCl–Na2SO4[J]. 金属学报, 2009, 45(2): 204-210.
[11] NING Likui ZHENG Zhi TAN Yi LIU Enze TONG Jian YU Yongsi WANG Hua. STUDY ON HOT CORROSION RESISTANCE OF A NEW DIRECTIONAL SOLIDIFICATION Ni–BASED SUPERALLOY[J]. 金属学报, 2009, 45(2): 161-166.
[12] YAN Wei SUN Fengjiu WANG Qingjiang LIU Jianrong CHEN Zhiyong LI Shaoqiang. HOT CORROSION BEHAVIOR OF ARC-ION PLATING Ti-Al-Cr(Si, Y) COATINGS ON Ti60 ALLOY[J]. 金属学报, 2009, 45(10): 1171-1178.
[13] LIU Enze SUN Shunchen TU Ganfeng ZHENG Zhi NING Likui ZHANG Lingfeng . STUDY OF A NEW-TYPE HIGH STRENGTH Ni--BASED SUPERALLOY DZ68 WITH GOOD HOT CORROSION RESISTANCE[J]. 金属学报, 2009, 45(10): 1217-1224.
[14] LI Mengjin; SUN Xiaofeng; GUAN Hengrong; JIANG Xiaoxia; HU Zhuangqi. HIGH TEMPERATURE HOT-CORROSION BEHAVIOR OF (Ni, Pd)Al COATING[J]. 金属学报, 2004, 40(7): 773-778 .
[15] JIN Guangxi; QIAO Lijie; GAO Kewei; KIMURA Takashi; HASHIMOTO Kenki$. Effect of Mn and V on Hot Corrosion of TiAl Alloy[J]. 金属学报, 2004, 40(2): 179-184 .
No Suggested Reading articles found!