Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (11): 1195-1206     DOI:
Research Articles Current Issue | Archive | Adv Search |
Fluid Flow and Inclusion's Collision--Growth in the Slab Continuous Casting Mold
LEI Hong; HE Jicheng
Key Laboratory of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University
Cite this article: 

LEI Hong; HE Jicheng. Fluid Flow and Inclusion's Collision--Growth in the Slab Continuous Casting Mold. Acta Metall Sin, 2007, 43(11): 1195-1206 .

Download:  PDF(1067KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mathematical model was developed to study fluid flow and inclusion collision and growth in the slab continuous caster. Due to the interaction of the moving solidifying shell and the upward flow, a small corner-vortex appears near the narrow face of the mold. Such a corner-vortex leads to the peak value of inclusion’s concentration, number density and characteristic radius near the narrow face. Numerical results also showed that convective transfer of molten steel is the key factor to influence the inclusion distribution. In the upper recirculation zone, the inclusion has the annular distribution. Wall effect and inclusion’s collision and aggregation are two important factors. Under the mold, the inclusion has the “W” shape distribution in the middle plane and the “8” shape distribution in the horizontal plane. And the inclusion has the “V” shape at the narrow face and symmetry plane under the nozzle.
Key words:  Inclusion      Collision      Aggregation      Continuous casting      
Received:  28 March 2007     
ZTFLH:  TF777  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I11/1195

[1]Zhang L,Taniguchi S,Cai K.Metall Mater Trans,2000; 31B:253
[2]Nakanishi K,Szekely J.Trans ISIJ,1975;15:522
[3]Miki Y,Shimada Y,Thomas B G,Denissov A.lronmaking Steelmaking,1997;24(8):31
[4]Zhang L.Steel Res Int,2005;76:784
[5]Lei H,Zhu M Y,He J C.J Iron Steel Res Int,2003;10(2): 21
[6]Lei H,Zhu M Y,He J C.Chin J Process Eng,2001;1(2): 138 (雷洪,朱苗勇,赫冀成.过程工程学报,2001;1:138)
[7]Tacke K H,Ludwig J G.Steel Res,1987;58:262
[8]Joo S,Han J W,Guthrie R I L.Metall Trans,1993;24B: 767
[9]Javurek M,Gittler P,Rossler R,Kaufmann B,Preblinger H.Steel Res Int,2005;76:64
[10]Shirabe K,Szekely J.Trans Iron Steel Inst Jpn,1983;23: 465
[11]Sinha A K,Sahai Y.ISIJ Int,1993;33:556
[12]Zhang B W,Deng K,Lei Z Z.Ren Z M.Acta Metall Sin, 2004;40:623 (张邦文,邓康,雷作胜,任忠鸣,金属学报;2004,40:623)
[13]Lei H,He J C.J Non-Cryst Solids,2006;352:3772
[14]Zhao L G,Liu K.J Ree Iron Steel,2002;14(6):19 (赵连刚,刘坤.钢铁研究学报,2002;14(6):19)
[15]Lei H,Wang L,Wu Z,Fan J.ISIJ Int,2002;42:717
[16]Zhu M,Zhen S,Huang Z,Gu W.Steel Res Int,2005;76: 718
[17]Miki Y,Thomas B G.Metall Mater Trans,1999;30B:639
[18]Tozawa H,Kata Y,Sorimachi K,Nakanishi T.ISIJ Int, 1999;39:426
[19]Saffman P G,Turner J S.J Fluid Meeh,1956;1:16
[20]Thomas B G,Mika L J,Najjar F M.Metall Trans,1990; 21B:387
[21]Thomas B G,Huang X,Sussman R C.Metall Mater Trans,1994;25B:527
[22]Bouris D,Bergeles G.Metall Mater Trans,1998;29B:614
[23]Lei H,Jin Y,Zhu M,He J.J Mater Sci Technol,2002; 18:403
[24]Lu L F,Lu S P,Zhou S Q,Ren Q,Li D,Kang R M,Wu W D.J Chongqing Univ,2006;29(2):72 (刘林飞,刘守平,周上祺,任勤,李丁,康人木,吴文东,重庆大学学报,2006;29(2):72)
[25]Lan Y G.Zou Z S,Jiang M F,Yao Y K.Spec Steel,2003; 24(4):48 (兰岳光,邹宗树,姜茂发,姚永宽.特殊钢,2003;24(4):48)
[26]Liu Y R,Song J X,Cheng N L.Steelmaking,2003;19(2): 36 (刘友荣,宋景欣,程乃良.炼钢,2003;19(2):36)
[1] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[2] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[3] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[4] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[5] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[6] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[7] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[8] ZHU Miaoyong, DENG Zhiyin. Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process[J]. 金属学报, 2022, 58(1): 28-44.
[9] GUO Zhongao, PENG Zhiqiang, LIU Qian, HOU Zibing. Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. 金属学报, 2021, 57(12): 1595-1606.
[10] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[11] CAI Laiqiang, WANG Xudong, YAO Man, LIU Yu. Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet[J]. 金属学报, 2020, 56(8): 1165-1174.
[12] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[13] SUN Feilong, GENG Ke, YU Feng, LUO Haiwen. Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel[J]. 金属学报, 2020, 56(5): 693-703.
[14] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[15] ZHANG Xinfang, YAN Longge. Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal[J]. 金属学报, 2020, 56(3): 257-277.
No Suggested Reading articles found!