Export:  BibTeX | EndNote (RIS)      
Abstract  The ultrafine WC-10Co cemented carbides were prepared by spark plasma sintering (SPS) using sub-micron WC/nano Co and sub-micron WC/micron Co with nanocrystalline structures as the raw powders in this paper. The SPS process, microstructure and properties of the sintered samples were investigated. The ultrafine cemented carbides with mean grain size of less than 200nm were prepared using the two kinds of raw powders. The sintered sample using sub-micron WC/micron Co powders as raw materials has a relative density of 98%, hardness of HRA94.5 and fracture toughness of 13.50MPa•m1/2, which indicate an very good combination of mechanical properties. While the sample sintered using the sub-micron WC/nano Co powders as raw materials has lower properties. The densification mechanisms of sintering the two kinds of WC/Co mixed powders were analyzed based on the special SPS mechanism.
Key words:  spark plasma sintering      WC-Co cemented carbides      high energy ball-milling      densification mechanism      
Received:  12 April 2006     
ZTFLH:  TG146  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/0

[1] LIU Ze, NING Hanwei, LIN Zhangqian, WANG Dongjun. Influence of Spark Plasma Sintering Parameters on the Microstructure and Room-Temperature Mechanical Properties of NiAl-28Cr-5.5Mo-0.5Zr Alloy[J]. 金属学报, 2021, 57(12): 1579-1587.
[2] LIN Zhangqian, ZHENG Wei, LI Hao, WANG Dongjun. Microstructures and Mechanical Properties of TA15 Titanium Alloy and Graphene Reinforced TA15 Composites Prepared by Spark Plasma Sintering[J]. 金属学报, 2021, 57(1): 111-120.
[3] Limei KANG,Chao YANG,Yuanyuan LI. Fabrication of Novel Bimodal Titanium Alloy with High-Strength and Large-Ductility by Semi-Solid Sintering[J]. 金属学报, 2017, 53(4): 440-446.
[4] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[5] Kunming PAN,Laiqi ZHANG,Shizhong WEI,Jiwen LI,Hao LI,Junpin LIN. STUDY ON THE PREPARATION PROCESS OF T2 ALLOY IN THE Mo-Si-B SYSTEM[J]. 金属学报, 2015, 51(11): 1377-1383.
[6] LE Guomin, Godfrey Andrew, LIU Wei. MICROSTRUCTURES AND MECHANICAL PROPERTIES OF SINTERED FINE-GRAINED Al[J]. 金属学报, 2013, 49(8): 939-945.
[7] GU Jian, GU Sasa, XUE Lihong, WU Shusen, YAN Youwei. MICROSTRUCTURE EVOLUTION OF Al-Fe ALLOYS PREPARED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2013, 29(4): 435-442.
[8] TAN Jun ZHOU Zhangjian LIU Yaqin QU Dandan ZHONG Ming GE Changchun. EFFECT OF CARBON NANOTUBES ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF W[J]. 金属学报, 2011, 47(12): 1555-1560.
[9] ZHAO Shixian SONG Xiaoyan WANG Mingsheng WEI Chongbin ZHANG Jiuxing LIU Xue. MATCHING OF PARTICLE SIZES OF WC/Co POWDERS AND SPARK PLASMA SINTERING DENSIFICATION[J]. 金属学报, 2009, 45(4): 497-502.
[10] LU Ni; uan; SONG Xiaoyan; ZHANG Jiuxing; LI Erdong. Preparation of Nd Bulk with Ultrafine Nanocrystalline Structure and its Physical Property[J]. 金属学报, 2007, 43(7): 739-743 .
[11] LIU Xuemei; SONG Xiaoyan; ZHANG Jiuxing. Temperature Distribution Simulation and Neck Evolution of Powder Particles During Spark Plasma Sintering[J]. 金属学报, 2006, 42(7): 757-762 .
[12] ZHAO Zhankui; YAO Kefu; JIN Songzhe; LI Jingfeng. BULK Al90Mn9Ce1 ALLOY WITH ULTRA-HIGH STRENGTH PREPARED BY SPARK PLASMA SINTERING[J]. 金属学报, 2005, 41(12): 1298-1302 .
No Suggested Reading articles found!