Abstract Because of the important application of the austenitic stainless steel in the nuclear industry, formation enrgies of a single vacancy(V), a self-interstitial atom(SIA), an interstitial helium atom(HeI) and helium-vacancy(He-V) clusters in γ-Fe, which has the same faced-centered cubic (fcc) structure as the austenitic stainless steel, are calculated by molecule statics. The modified embedded atom method potential, Wilson-Johnson potential and Beck potential are employed to describe the interactions of Fe-Fe, Fe-He and He-He respectively. The calculation results show that the formation energy of slit <100> SIA in γ-Fe is lower than that of slit <110> in α-Fe, and the tetrahedral interstitial position in γ-Fe is the most stable site for HeI. When the number of helium atoms in cluster of HenV0, HenV1, HenV2, HenV3 is 2, 5, 9, 11 respectively, the clusters will self-trap by forming Frenkel pair. The He/V of self-trapped cluster is not a constant, it will gradually decrease with the number of vacancies increasing.
[1] Morishita K, Sugano R,Wirth B D.J Nucl Mater,2003; 323:243 [2] Morishita K,Sugano R,Wirth B D,de la Rubia T D.Nucl Instrum Methods Phys Res,2003;202B:76 [3] Morishita K,Sugano R,Wirth B D.Fusion Sci Technol, 2003;44:441 [4]Ackland G J,Bacon D J,Calder A F,Harry T.Philos Mag, 1997;75A:713 [5] Johnson R A,Wilson W D.In:Gehlen P C,Beeler J R Jr,Jaflee R I,eds.,Interatomic Potentials and Simulation of Lattice Defects,New York:Plenum,1972:375 [6] Beck D E.Mol Phys,1968;14:311 [7] Baskes M I.Phys Rev,1992;46B:2727 [8] Baskes M I.Mater Sci Eng,1999;A261:165 [9] Baskes M I.Mater Chem Phys,1997;55:152 [10] Ventelon L,Wirth B D.Fusion Materials Semian- nual Progress Report for the Period Ending,DOE-ER- 0313/37, US Department of Energy,2005:140 [11]Seletskaia T,Osetsky Y,Stoller R E,Stocks G M.Phys Rev Lett,2005;94:046403 [12] Wilson W D,Baskes M I,Bisson C L.Phys Rev,1976; 13B:2470 [13] Adams J B,Wolfer W G.J Nucl Mater,1989;166:235 [14] Wilson W D,Bisson C L,Baskes M I.Phys Rev,1981; 24B:5616