Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (4): 337-340     DOI:
Research Articles Current Issue | Archive | Adv Search |
mechanical analysis of tensile instability due to only material parameter
;;;
吉林大学超塑性与塑性研究所
Cite this article: 

;. mechanical analysis of tensile instability due to only material parameter. Acta Metall Sin, 2006, 42(4): 337-340 .

Download:  PDF(542KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Instabilities during superplastic deformation is more complicated than those during plastic deformation. Many valuable papers about mechanical analysis of instability have been published at home and abroad, which contributed much to the development of superplastic research. But their conclusions were different because of the diversity of the researchers’ thoughts and methods. Therefore, it is necessary to normalize these theories. In order to study the impact of material’s mechanical parameter on instability, tensile instability criterion of specimen without geometric defect at constant temperature, that is due to only material parameter, was analyzed based on state equation of deformation in this paper. The results not only coincided with those in some typical papers, but also proved theoretically that, during superplastic deformation, geometrical instability will happen after a period of uniform deformation which follows load instability, rather than in the mean time of load instability.
Key words:  Superplasticity      specimen without geometric defect      constant temperature      tensile instability criterion     
Received:  17 January 2006     
ZTFLH:  TG113.25  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I4/337

[1] Lin L H, Hirth J P, Hart E W. Ada Metall, 1981; 29: 819
[2] Ghosh A K. Acta Metall, 1977; 25: 1413
[3] Jonas J J, Holt R A, Coleman C E. Acta Metall, 1976; 24: 911
[4] Hart E W. Acta Metall, 1967; 15: 351
[5] Jonas J J, Christodoulou N, G'Sell C. Scr Metall, 1978; 12: 565
[6] Burke M A, Nix W D. Acta Metall, 1975; 23: 793
[7] Hutchinson J W, Neale K W. Acta Metall, 1977; 25: 839
[8] Nichols F A. Acta Metall, 1980; 28: 663
[9] Jonas J J, Baudelet B. Acta Metall, 1977; 25: 43
[10] Langdon T G. Met Sci, 1982; 16: 175d
[1] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[2] Guangming XIE, Zongyi MA, Peng XUE, Zongan LUO, Guodong WANG. Effects of Tool Rotation Rates on Superplastic Deformation Behavior of Friction Stir Processed Mg-Zn-Y-Zr Alloy[J]. 金属学报, 2018, 54(12): 1745-1755.
[3] Huiyuan WANG, Hang ZHANG, Xinyu XU, Min ZHA, Cheng WANG, Pinkui MA, Zhiping GUAN. Current Research and Future Prospect on Microstructure Stability of Superplastic Light Alloys[J]. 金属学报, 2018, 54(11): 1618-1624.
[4] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
[5] FU Mingjie, HAN Xiuquan, WU Wei, ZHANG Jianwei. SUPERPLASTICITY RESEARCH OF Ti-23Al-17Nb ALLOY SHEET[J]. 金属学报, 2014, 50(8): 955-961.
[6] MA Pinkui, SONG Yuquan. BINOCULAR STEREO VISION MEASUREMENT RESEARCH FOR SUPERPLASTIC FREE BULGING[J]. 金属学报, 2014, 50(4): 471-478.
[7] GUAN Zhiping, MA Pinkui, SONG Yuquan. ANALYSIS OF FRACTURE DURING SUPERPLASTIC TENSION[J]. 金属学报, 2013, 49(8): 1003-1011.
[8] SHEN Jun, FENG Aihan. RECENT ADVANCES ON MICROSTRUCTURAL CONTROLLING AND HOT FORMING OF Ti2AlNb-BASED ALLOYS[J]. 金属学报, 2013, 49(11): 1286-1294.
[9] HOU Jieshan, ZHOU Lanzhang, GUO Jianting, YUAN Chao. APPLICATION OF ARTIFICIAL NEURAL NETWORK FOR PREDICTION OF SUPERPLASTIC  BEHAVIOUR IN NiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1333-1338.
[10] CAO Furong DING Hua WANG Zhaodong LI Yinglong GUAN Renguo CUI Jianzhong . QUASI–SUPERPLASTICITY AND DEFORMATION MECHANISM OF ULTRALIGHT β SOLID SOLUTION Mg–11Li–3Zn ALLOY[J]. 金属学报, 2012, 48(2): 250-256.
[11] WANG Gang XU Lei WANG Yong ZHENG Zhuo CUI Yuyou YANG Rui. HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF A HIGH-Nb-CONTAINING TiAl BASED ALLOY[J]. 金属学报, 2011, 47(5): 587-593.
[12] CAO Furong GUAN Renguo DING Hua LI Yinglong ZHOU Ge CUI Jianzhong. DISLOCATION CREEP IN SUPER–LIGHT α SOLID SOLUTION BASE Mg–6Li–3Zn ALLOY[J]. 金属学报, 2010, 46(6): 715-722.
[13] ZHANG Han BAI Bingzhe FANG Hongsheng. EFFECT OF PRESTRAIN ON THE SUPERPLASTIC DEFORMATION BEHAVIOR OF LOW-ALLOY HIGH-CARBON STEEL[J]. 金属学报, 2009, 45(9): 1106-1110.
[14] KANG Zhixin PENG Yonghui SANG Jing JIAN Weiwei ZHAO Haidong LI Yuanyuan. SUPERPLASTICITY AND MICROSTRUCTURE EVOLUTION IN Mg-1.5Mn-0.3Ce ALLOY DEFORMED BY T-SHAPE CHANNEL PRESSING[J]. 金属学报, 2009, 45(9): 1117-1124.
[15] SONG Yuquan LIU Ying XU Jin GUAN Xiaofang. STRUCTURAL CERAMICS AND THEIR SUPERPLASTICITY  II. Superplasticity of Structural Ceramics[J]. 金属学报, 2009, 45(1): 6-17.
No Suggested Reading articles found!