MICROSCOPIC PHASE-FIELD SIMULATION OF COARSENING BEHAVIOR OF PRECIPITATE OF Ni75AlxV25-x ALLOY
Cite this article: 

. MICROSCOPIC PHASE-FIELD SIMULATION OF COARSENING BEHAVIOR OF PRECIPITATE OF Ni75AlxV25-x ALLOY. Acta Metall Sin, 2006, 42(3): 239-244 .

Download:  PDF(355KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the microelasticity theory of coherent strain and the microscopic phase-field dynamic model, the morphology evolution and the coarsening behavior of Ni75AlxV25-x alloy during precipitation was simulated. The precipitates particles have the obvious orientation for the two phases when the coarsening happened. The [100] directions of phases are the preference orientation during the growth, and aligned along the <001> directions. The growth and coarsening of the first precipitates have two evident stage,but growth and coarsening of the last precipitates are proceeding simultaneously. The growth and coarsening of precipitates are take place by means of the coalescence between neighboring particles. In despite of the precipitation order and the volume fraction are different for different concentration, the morphology of two phases is almost same at last, which has the quadrate shape, and the orientation relationship of (001) //{100} is exist between two phases.
Key words:  Ni75AlxV25-x      precipitation      coherent strain      coarsening      microscopic phase-field      
Received:  21 June 2005     
ZTFLH:  TG111.5  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I3/239

[1] Tomihisa K, Kaneno Y, Takasugi T. Intermetallics, 2004; 12: 317
[2] Hagihara K, Nakano T, Umakoshi Y. Scr Mater, 2003; 48: 577
[3] Ni Y, He L H, Yin L. Mater Chem Phys, 2002; 78: 442
[4] Wen Y H, Wang Y, Chen L Q. Philos Mag, 2000 , 80A: 1967
[5] Vaithyanathan V, Chen L Q. Acta Mater, 2002; 50: 4061
[6] Khachaturyan A G. Theory of Structural Transformation in Solids. New York: Wiley, 1983: 139
[7] Jiang Z H, Wang Y X, Chen Z. Acta Metall Sin, 2004; 40: 616 (江志华,王永欣,陈铮.金属学报, 2004;40:616)
[8] Li X L, Chen Z, Liu X G, Liu B. Acta Metall Sin, 2002; 38: 458 (李晓玲,陈铮,刘晓光,刘兵.金属学报,2002;38: 458)
[9] Li Y S, Chen Z, Lu Y L, Wang Y X. J Mater Sci Technol, 2005; 21: 395
[10] Pareige C, Blavette D. Scr Mater, 2001; 44: 243
[11] Marteau L, Pareige C, Biavette D. J Microsc, 2001; 204: 247
[12] Chen L Q. Scr Metall Mater, 1993; 29: 683
[13] Khachaturyan A G. Theory of Structural Transformation in Solids. New York: Wiley, 1983: 57
[14] Onuki A. J Phys Soc Jpn, 1989; 58: 3065
[15] Wang Y, Khachaturyan A G. Acta Metall Mater, 1995; 43: 1837
[16] Prikhodko S V, Carnes J D, Isaak D G, Ardell A J. Scr Mater, 1998; 38: 67
[17] Wen Y H, Simmons J P, Shen C. Acta Mater, 2003; 51: 1123
[18] Su C H, Voorhees P W. Acta Mater, 1996; 44: 1987
[19] Sequera A D, Calderon H A, Kostotz G. Scr Metall Mater, 1994; 30: 7
[20] Takeyama M, Kikuchi M. Intermetallic, 1998; 6: 573
[21] Orlikowski D, Sagui C, Somoza A, Roland C. Phys Rev, 1999; 59B: 8646
[22] Langer J S, Schwartz A J. Phys Rev, 1980; 21A: 948
[23] Wang Y, Banerjee D, Su C C, Khachaturyan A G. Acta Mater, 1998; 46: 2983
[1] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[2] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[3] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[4] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[5] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[6] YUAN Bo, GUO Mingxing, HAN Shaojie, ZHANG Jishan, ZHUANG Linzhong. Effect of 3%Zn Addition on the Non-Isothermal Precipitation Behaviors of Al-Mg-Si-Cu Alloys[J]. 金属学报, 2022, 58(3): 345-354.
[7] TANG Shuai, LAN Huifang, DUAN Lei, JIN Jianfeng, LI Jianping, LIU Zhenyu, WANG Guodong. Co-Precipitation Behavior in Ferrite Region During Isothermal Process in Ti-Mo-Cu Microalloyed Steel[J]. 金属学报, 2022, 58(3): 355-364.
[8] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[9] SUN Shijie, TIAN Yanzhong, ZHANG Zhefeng. Strengthening and Toughening Mechanisms of Precipitation- Hardened Fe53Mn15Ni15Cr10Al4Ti2C1 High-Entropy Alloy[J]. 金属学报, 2022, 58(1): 54-66.
[10] XUE Kemin, SHENG Jie, YAN Siliang, TIAN Wenchun, LI Ping. Influence of Precipitation of China Low Activation Martensitic Steel on Its Mechanical Properties After Groove Pressing[J]. 金属学报, 2021, 57(7): 903-912.
[11] XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan. Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. 金属学报, 2021, 57(6): 822-830.
[12] CHEN Guo, WANG Xinbo, ZHANG Renxiao, MA Chengyue, YANG Haifeng, ZHOU Li, ZHAO Yunqiang. Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel[J]. 金属学报, 2021, 57(6): 725-735.
[13] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[14] HAN Baoshuai, WEI Lijun, XU Yanjin, MA Xiaoguang, LIU Yafei, HOU Hongliang. Effect of Pre-Deformation on Microstructure and Mechanical Properties of Ultra-High Strength Al-Zn-Mg-Cu Alloy After Ageing Treatment[J]. 金属学报, 2020, 56(7): 1007-1014.
[15] SUN Xinjun,LIU Luojin,LIANG Xiaokai,XU Shuai,YONG Qilong. TiC Precipitation Behavior and Its Effect on Abrasion Resistance of High Titanium Wear-Resistant Steel[J]. 金属学报, 2020, 56(4): 661-672.
No Suggested Reading articles found!