Abstract The grain growth behavior in reactive spray formed TiCP/7075 Al alloy was studied and compared with that of spray formed 7075 Al alloy at semi-solid state. The specimens were heat-treated isothermally at 600℃ for times in the range of 10-60min,then quenched in water. The microstructure of reheated specimens was characterized using OP、SEM and TEM. The grain size was measured using a mean linear intercept method. Results shows that the in-situ TiC particles can effectively retard grain growth, grain growth exponent (n) for Arrhenius equation was increased from 2 to 3, which indicates that the in-situ TiC particles have the significant pinning effect on grain coarsening in the semi-solid state. The analysis also showed that the activation energy for grain growth for the samples with TiC addition was over twice of that for the samples without TiC additions, which made it more difficult for grain.
|
|
Received: 13 May 2005
|
|
|
[1] Kang Z T, Zhang H, Chen Z H. Chin J Nonferrous Met,1998; 8: 595(康智涛,张豪,陈振华.中国有色金属学报,1998;8:595) [2] Yu F X, Cui J H, Ranganathan S, Dwarakadasa E S. Mater Sci Eng, 2001; A304-306: 261 [3] Jung H K, Kang C G. J Mater Proc Technol, 2000; 104: 244 [4] Annavarapu S, Doherty R D. Acta Metall Mater, 1995; 43: 3207 [5] Lawrynowicz D E, Wolfenstine J, Lavernia E J. Mater Sci Eng, 1997; A230: 1 [6] Wang J L, Su Y H, Tsao C Y A. Scr Mater, 1997: 37: 2003 [7] MansonWhitton E D, Stone I C, Jones J R, Grant P S, Cantor B. Acta Mater, 2002; 50: 2517 [8] Yang B, Wang F, Huang Z J, Duan X J, Zhang J S. Mater Rev, 2001; 15(3): 4(杨滨,王锋,黄赞军,段先进,张济山.材料导报,2001;15(3):4) [9] Wu G, Yao L J, Li Z X, Peng R Q, Zhao Z D. Aluminum and Aluminum Alloys Handbook. Beijin: Science Press, 1997: 255(武恭,姚良均,李震霞,彭如清,赵祖德.铝及铝合金材料手册.北京:科学出版社,1997:255) [10] Lu G M, Dong J, Cui J Z. Chin J Nonferrous Met, 2001; 11: 211(路贵民,董杰,崔建忠.中国有色金属学报,2001;11:211) [11] Lawrynowicz D E, Wolfenstine J, Lavernia E J. Mater Sci Eng, 1997; A230: 1 [12] Kawanishi S, Isonishi K, Okazaki K. Mater Trans, 1993; 34(1): 49C |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|