Correcting of Hot Compression Test and Constitutive Equation of NiTi SMA
Cite this article: 

. Correcting of Hot Compression Test and Constitutive Equation of NiTi SMA. Acta Metall Sin, 2006, 42(10): 1036-1040 .

Download:  PDF(193KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In this paper, the hot compression test results of NiTi alloy have been analyzed. Errors caused by friction and thermal effect were corrected. The test temperature ranged from 725℃ to 975℃, and the strain rate ranged from 0.1 s-1 to 10 s-1. Constitutive equation at high temperature of NiTi alloy was established by curvilinear regression method. The simulation results agreed with the experiment. Research results provided the accurate material model for the numerical simulation of NiTi SMA plastic formation process.
Key words:  NiTi alloy      compression test      correcting      constitutive equation      
Received:  21 March 2006     
ZTFLH:  TG139  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I10/1036

[1]Huang X W,Dong G N,Zhou Z R,Xie Y B.Chin J Nonferrous Met,2004;14(7):1168(黄学文,董光能,周仲荣,谢友柏.中国有色金属学报,2004;14(7):1168)
[2]Dolce M,Cardone D.Int J Mech Sci,2001;43:2657
[3]Dolce M.Cardone D.Int J Mech Sci,2001;43:2631
[4]Yah W,Chen G X.J Plast Eng,2004;11(4):19(严巍,陈国学.塑性工程学报,2004;11(4):19)
[5]Tseng A A,Horsk(?) J,Raudensk(?) M,Kotrbácek P.Mater Design,2001;22:83
[6]Xu S Q,Chen Z Y,Zhang S Y.Forg Starp Technol,2004;29(5):46(许树勤,陈志英,张善元.锻压技术,2004;29(5):46)
[7]Wang S L,Ruan X Y,Yu X L,Chen S C,Hu Z S.Chin Mech Eng,1996;7(6):101(王少林,阮雪榆,俞新陆,陈森灿,胡宗式.中国机械工程,1996;7(6):101)
[8]Luo Z J,Yang Q,Ji W H.Chin J Nonferrous Met,2000;10:804(罗子健,杨旗,姬婉华.中国有色金属学报,2000;10:804)
[9]Wang D N.Principles of Metal Forming.Beijing:China Machine Press,1982:140(汪大年.金属塑性成形原理.北京:机械工业出版社,1982:140)
[10]Ebrahimi R,Najafizadeh A.J Mater Process Technol,2004;152(20):136
[11]Laasraoui A,Jonas J J.Metall Trans,1991;22A:1545
[1] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[2] LIU Qingqi, LU Ye, ZHANG Yifei, FAN Xiaofeng, LI Rui, LIU Xingshuo, TONG Xue, YU Pengfei, LI Gong. Thermal Deformation Behavior of Al19.3Co15Cr15Ni50.7 High Entropy Alloy[J]. 金属学报, 2021, 57(10): 1299-1308.
[3] ZHAO Manman, QIN Sen, FENG Jie, DAI Yongjuan, GUO Dong. Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel[J]. 金属学报, 2020, 56(7): 960-968.
[4] Zhipeng WAN, Tao WANG, Yu SUN, Lianxi HU, Zhao LI, Peihuan LI, Yong ZHANG. Dynamic Softening Mechanisms of GH4720Li AlloyDuring Hot Deformation[J]. 金属学报, 2019, 55(2): 213-222.
[5] MA Kai, ZHANG Xingxing, WANG Dong, WANG Quanzhao, LIU Zhenyu, XIAO Bolv, MA Zongyi. Optimization and Simulation of Deformation Parameters of SiC/2009Al Composites[J]. 金属学报, 2019, 55(10): 1329-1337.
[6] Bolü XIAO, Zhiye HUANG, Kai MA, Xingxing ZHANG, Zongyi MA. Research on Hot Deformation Behaviors of Discontinuously Reinforced Aluminum Composites[J]. 金属学报, 2019, 55(1): 59-72.
[7] Yusen SU, Yinhui YANG, Jianchun CAO, Yuliang BAI. Research on Hot Working Behavior of Low-NickelDuplex Stainless Steel 2101[J]. 金属学报, 2018, 54(4): 485-493.
[8] Zhaozhao WEI, Xiao MA, Xinping ZHANG. Topological Modelling of the B2-B19' Martensite Transformation Crystallography in NiTi Alloy[J]. 金属学报, 2018, 54(10): 1461-1470.
[9] Xiaoyun YUAN, Liqing CHEN. HOT DEFORMATION AT ELEVATED TEMPERATURE AND RECRYSTALLIZATION BEHAVIOR OF A HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. 金属学报, 2015, 51(6): 651-658.
[10] LI Junru, GONG Chen, CHEN Lie, ZUO Hui, LIU Yazheng. HOT DEFORMATION BEHAVIOR OF BLADES STEEL 10Cr12Ni3Mo2VN FOR ULTRA- SUPERCRITICAL UNITS[J]. 金属学报, 2014, 50(9): 1063-1070.
[11] FU Mingjie, HAN Xiuquan, WU Wei, ZHANG Jianwei. SUPERPLASTICITY RESEARCH OF Ti-23Al-17Nb ALLOY SHEET[J]. 金属学报, 2014, 50(8): 955-961.
[12] YU Hui KIM Youngmin YU Huashun YOU Bongsun MIN Guanghui. HOT DEFMATION BEHAVIOR AND HOT WORKABILITY OF Mg-Zn-Zr-Ce ALLOY[J]. 金属学报, 2012, 48(9): 1123-1131.
[13] ZHANG Huibo JIN Wei YANG Rui. 3D FINITE ELEMENT SIMULATION OF PULL–OUT FORCE OF TiNiFe SHAPE MEMORY PIPE COUPLING WITH INNER CONVEX[J]. 金属学报, 2012, 48(12): 1520-1524.
[14] CAO Yu DI Hongshuang ZHANG Jiecen ZHANG Jingqi MA Tianjun. RESEARCH ON DYNAMIC RECRYSTALLIZATION BEHAVIOR OF INCOLOY 800H[J]. 金属学报, 2012, 48(10): 1175-1185.
[15] SUN Chaoyang LIU Jinrong LI Rui ZHANG Qingdong. CONSTITUTIVE MODELING FOR ELEVATED TEMPERATURE FLOW BEHAVIOR OF INCOLOY 800H SUPERALLOY[J]. 金属学报, 2011, 47(2): 191-196.
No Suggested Reading articles found!