Research on the solidification characteristic scale and undercooling during directional solidification of single-phase alloy
;;;;
西北工业大学凝固技术国家重点实验室
Cite this article: 

. Research on the solidification characteristic scale and undercooling during directional solidification of single-phase alloy. Acta Metall Sin, 2006, 42(10): 1025-1030 .

Download:  PDF(269KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A transparent model alloy, succininitrile-1.48 wt%Salol, was directionally solidified on a temperature gradient stage at the constant velocity. The primary spacing, tip radius and tip temperatures have been measured as a function of growth rate. The critical velocity for planar interface instability Vc was obtained. It is shown that, with the increase of growth velocity, the primary spacing decreases first, go through a local minimum value, and then increases to a local maximum value, finally decrease again. The cell-dendrite transition happens when the primary spacing increases from the local minimum to maximum value. Experimental results were compared to BH-L and self-consistent model. It’s found that the tip temperature predicted by BH-L model shows a large difference with the experimental results, and there shows a good agreement between all experimental results and self-consistent model.
Key words:  directional solidification      primary spacing      tip radius      tip temperature      
Received:  24 February 2006     
ZTFLH:  TG24  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I10/1025

[1]Kurz W,Fisher D J.Fundamentals of Solidification.3rd edition,Aedermansdorf,Switzerland:Trans Tech Publications,1992
[2]Huang W D,Shang B L,Zhou Y H.Chin J Aeronaut,1992;13A:376(黄卫东,商宝禄,周尧和.航空学报,1992;13A:376)
[3]Huang W D,Shang B L,Zhou Y H.Acta Phys Sin,1991;40:323(黄卫东,商宝禄,周尧和.物理学报,1991;40:323)
[4]Burden M H,Hunt J D.J Cryst Growth,1974;22:99
[5]Burden M H,Hunt J D.J Cryst Growth,1974;22:109
[6]Somboonsuk K,Mason J T,Trivedi R.Metall Trans,1984;15A:967
[7]Huang W D.PhD Dissertation,Northwestern Polytechnical University,Xi'an,1989(黄卫东.西北工业大学博士学位论文,西安,1989)
[8]Somboonsuk K,Mason J T,Trivedi R.Metall Trans,1984;15A:977
[9]Huang W D,Geng X G,Zhou Y H.J Cryst Growth,1993;134:105
[10]Lin X,Huang W D,Pan Q Y,Ding G L,Xue Y F,Zhou Y H.Acta Metall Sin,1997;33:1140(林鑫,黄卫东,潘清跃,丁国陆,薛玉芳,周尧和.金属学报,1997;33:1140)
[11]Lin X,Huang W D,Fen J,Li T,Zhou Y H.Acta Mater,1999;47:3271
[12]Ding G L,Huang W D,Huang X,Lin X,Zhou Y H.Acta Mater,1996;44:3705
[13]Ding G L,Lin X,Huang W D,Zhou Y H.Acta Metall Sin,1995;31:20(丁国陆,林鑫,黄卫东,周尧和.金属学报,1995;31:20)
[14]Esaka H,Kurz W.J Cryst Growth,1985;72:578
[15]Lin X,Li Y M,Liu Z X,Li T,Huang W D.Sci Technol Adv Mater,2001;2:293
[16]Lin X.PhD Dissertation,Northwestern Polytechnical University,Xi'an,2000(林鑫.西北工业大学博士学位论文,西安,2000)
[17]Huang W D,Ding G L,Zhou Y H.Chin J Mater Res,1995;9:193(黄卫东,丁国陆,周尧和.材料研究学报,1995;9:193)
[18]Lin X,Li T,Wang L L,Su Y P,Huang W D.Acta Phys Sin,2004;53:3971(林鑫,李涛,王琳琳,苏云鹏,黄卫东.物理学报,2004;53:3971)
[19]Huang W D,Lin X,Li T,Wang L L,Inatomi Y.Acta Phys Sin,2004;53:3978(黄卫东,林鑫,李涛,王琳琳,Inatomi Y.物理学报,2004;53:3978)
[20]Mullins W W,Sekerka R F.J Appl Phys,1963;34:323
[21]Mullins W W,Sekerka R F.J Appl Phys,1964;35:444
[22]Ding G L.PhD Dissertation,Northwestern Polytechnical University,Xi'an,1996(丁国陆.西北工业大学博士学位论文,西安,1996)
[23]Eshelman M A,Seetharaman V,Trivedi R.Acta Metall,1988;36:1165
[24]Burden M H,Hunt J D.J Cryst Growth,1974;22:109
[25]Laxmanan V.Acta Metall,1985;33:1037
[26]Laxmanan V.J Cryst Growth,1986;75:5733
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[4] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[5] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[6] ZHANG Xiaoli, FENG Li, YANG Yanhong, ZHOU Yizhou, LIU Guiqun. Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2020, 56(7): 969-978.
[7] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[8] XU Qingyan,YANG Cong,YAN Xuewei,LIU Baicheng. Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification[J]. 金属学报, 2019, 55(9): 1175-1184.
[9] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[10] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[11] JIN Hao, JIA Qing, LIU Ronghua, XIAN Quangang, CUI Yuyou, XU Dongsheng, YANG Rui. Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. 金属学报, 2019, 55(12): 1519-1526.
[12] Yuan HOU, Zhongming REN, Jiang WANG, Zhenqiang ZHANG, Xia LI. Effect of Longitudinal Static Magnetic Field on the Columnar to Equiaxed Transition in Directionally Solidified GCr15 Bearing Steel[J]. 金属学报, 2018, 54(5): 801-808.
[13] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[14] Jincheng WANG, Chunwen GUO, Junjie LI, Zhijun WANG. Recent Progresses in Competitive Grain Growth During Directional Solidification[J]. 金属学报, 2018, 54(5): 657-668.
[15] Guang CHEN, Gong ZHENG, Zhixiang QI, Jinpeng ZHANG, Pei LI, Jialin CHENG, Zhongwu ZHANG. Research Progress on Controlled Solidificationand Its Applications[J]. 金属学报, 2018, 54(5): 669-681.
No Suggested Reading articles found!