EXFOLIATION CORROSION BEHAVIOR OF T6 TREATED 2090 Al-Li ALLOY IN EXCO SOLUTION AND EIS DURING EXFOLIATION CORROSION EVOLUTION
SU Jingxin; ZHANG Zhao; CAO Fahe; ZHANG Jianqing; CAO Chunan
Department of Chemistry; Zhejiang University; Hangzhou 310027
Cite this article: 

SU Jingxin; ZHANG Zhao; CAO Fahe; ZHANG Jianqing; CAO Chunan. EXFOLIATION CORROSION BEHAVIOR OF T6 TREATED 2090 Al-Li ALLOY IN EXCO SOLUTION AND EIS DURING EXFOLIATION CORROSION EVOLUTION. Acta Metall Sin, 2005, 41(9): 974-978 .

Download:  PDF(265KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Electrochemical impedance spectroscopy (EIS) and in situ microscopic image of T6 peak-aged AA2090 Al-Li alloys in EXCO solution were studied. The localized corrosion form of the alloy during immersion evolved from pitting through intergranular corrosion, exfoliation corrosion (EC) to post EC. EC initiated at big corrosion pits which were formed with inclusion phase as center in pitting stage. The EC blisters propagate from these big pits till the upper layer is totally lifted. EIS of the initiation stage of pitting corrosion consists of a high frequency capacitive arc and a middle-low frequency inductive arc, and the inductive arc tends to disappear when pitting corrosion starts to propagate. In the intergranular corrosion stage, the second time constant corresponding to the corroded area can hardly be distinguished in the capacitive part of the EIS. In the stages of EC propagation and post EC, their EIS consist of two capacitive arcs.
Key words:  Al-Li alloy      electrochemical impedance spectroscopy (EIS)      EXCO solutio      
Received:  18 January 2005     
ZTFLH:  TG174.3  
  O646  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I9/974

[1] Liu J A, Zhu X W. Light Alloy Fabr Technol, 1996; 24(5): 2 (刘静安,朱献文.轻合金加工技术, 1996;24(5):2)
[2] He J P, Chen W L, Xu W, Fan W X. J Nanjing Univ Aeronaut Astronaut, 1999; 31: 575 (何建平,陈文理,许玮,樊蔚勋.南京航空航天大学学报, 1999;31:575)
[3] He B, Sun Y C, Fan W X. J Nanjing Univ Aeronaut Astronaut, 1998; 30: 306 (贺斌,孙有朝,樊蔚勋.南京航空航天大学学报,1998;30: 306)
[4] ASTM G34-79.Exfoliation Corrosion Susceptibility in 2xxx and 7xxx Series Aluminum Alloys (EXCO test), 1999
[5] Kelly D J, Robinson M J. Corros Sci,1993;49: 787
[6] Habashi M, Bonte E,Galland J, Bodu J J. Corros Sci, 1993; 35: 169
[7] Conde A, de Damborenear J. Electrochim Acta, 1998; 43: 849
[8] Coude A, de Damborenear J. Corros Sci, 2000; 42: 1393
[9] Buchheit R G Jr, Moran J P, Stoner G E. Corrosion, 1990; 46: 610
[10] Garrard W N. Corrosion, 1994, 50: 215
[11] Buchheit R G, Moran J P, Stoner G E. Corrosion,1994; 50: 120
[12] Kumai G, Kusinski J, Thomas G, Devine T M. Corrosion, 1989; 45: 294
[13] Cao C N, Wang J, Lin H C. J Chin Soc Corros Protect, 1989; 9: 261 (曹楚南,王 佳,林海潮.中国腐蚀与防护学报,1989;9: 261)
[14] Cao C N, Zhang J Q. An Introduction to Electrochemical Impedance Spectroscopy.Beijing:Science Press, 2002: 177 (曹楚南,张鉴清.电化学阻抗谱导论.北京:科学出版社,2002: 177)
[1] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[2] LI Shiju, LI Yang, CHEN Jianqiang, LI Zhonghao, XU Guangming, LI Yong, WANG Zhaodong, WANG Guodong. Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field[J]. 金属学报, 2020, 56(6): 831-839.
[3] Chao CAI,Yang LI,Jinfeng LI,Zhao ZHANG,Jianqing ZHANG. Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. 金属学报, 2019, 55(8): 958-966.
[4] Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG. Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy[J]. 金属学报, 2019, 55(6): 709-719.
[5] Jinfeng LI,Danyang LIU,Ziqiao ZHENG,Yonglai CHEN,Xuhu ZHANG. EFFECT OF Er MICRO-ALLOYING ON MECHANICAL PROPERTIES AND MICROSTRUCTURES OF 2055 Al-Li ALLOY[J]. 金属学报, 2016, 52(7): 821-830.
[6] Xianfeng ZHANG,Guoai LI,Zheng LU,Juan YU,Min HAO. EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. 金属学报, 2016, 52(12): 1497-1502.
[7] LIU Fenjun, FU Li, ZHANG Wenyuan, MENG Qiang, DONG Chunlin, LUAN Guohong. INTERFACE STRUCTURE AND MECHANICAL PRO-PERTIES OF FRICTION STIR WELDING JOINT OF 2099-T83/2060-T8 DISSIMILAR Al-Li ALLOYS[J]. 金属学报, 2015, 51(3): 281-288.
[8] FU Xinxin, DONG Junhua, HAN En-hou, KE Wei. ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY MONITORING ON MILD STEEL Q235 IN SIMULATED INDUSTRIAL ATMOSPHERIC CORROSION ENVIORNMENT[J]. 金属学报, 2014, 50(1): 57-63.
[9] ZHOU Xiaowei,SHEN Yifu. CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. 金属学报, 2013, 49(9): 1121-1130.
[10] WANG Dong DONG Chunlin XIAO Bolv GAO Cong HE Miao LUAN Guohong MA Zongyi. EFFECT OF WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED AlCuLi ALLOY JOINTS[J]. 金属学报, 2012, 48(9): 1109-1115.
[11] ZHAO Bo DU Cuiwei LIU Zhiyong LI Xiaogang YANG Jike LI Yueqiang. CORROSION BEHAVIOR OF X80 STEEL IN YINGTAN SOIL SIMULATED SOLUTION UNDER DISBONDED COATING[J]. 金属学报, 2012, 48(12): 1530-1536.
[12] WANG Changgang DONG Junhua KE Wei CHEN Nan. EFFCTS OF pH AND Cl− CONCENTRATION ON THE CORROSION BEHAVIOR OF COPPER IN BORIC ACID BUFFER SOLUTION[J]. 金属学报, 2011, 47(3): 354-360.
[13] YANG Bo LI Moucheng YAO Meiyi ZHOU Bangxin SHEN Jianian. IN SITU IMPEDANCE CHARACTERISTICS OF ZIRCONIUM ALLOY CORROSION IN HIGH TEMPERATURE AND PRESSURE WATER ENVIRONMENT[J]. 金属学报, 2010, 46(8): 946-950.
[14] ;. SURFACE MODIFICATION OF 316L STAINLESS STEEL BY HIGH CURRENT PULSED ELECTRON BEAM Part II Corrosion behaviors in the simulated body fluid[J]. 金属学报, 2007, 42(1): 71-76 .
[15] WU Ximao;Al Suhua;ZHANG Yun;WANG Zhonmang;HAN Xinglin (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Shenyang Polytechnic University. Shenyang 110023). THE LOW CYCLE FATIGUE BEHAVIOUR FOR 8090 Al-Li ALLOYS[J]. 金属学报, 1997, 33(7): 702-708.
No Suggested Reading articles found!