Abstract Near threshold fatigue crack growth tests were conducted under
torsion on circumferentially pre--cracked round bars of a
stainless steel. The crack growth rate was decreased with
crack extension because of the sliding contact of the crack
faces. The crack growth rate without the influence of crack
surface contact was determined by extrapolating the
relationship between the crack growth rate and the crack
extension to the zero crack length. The applied stress
intensity factor range is divided into two parts: one is the effective value
responsible for crack growth and the other is the shielding
value dissolved by crack surfaces contact. The
fatigue limits for crack initiation and fracture
were predicted and the predicted values agreed well with the
experimental results.
|
|
Received: 04 November 2004
|
|
|
[1] Pook L P. Int J Fatigue, 1985; 7(1): 21 [2] Yates J R, Miller K J. Fatigue Fract Eng Mater Struct, 1989; 12: 259 [3] Yoshioka S, Watanabe K, Kitagawa H, Inoue A, Kumar sawa M. Trans Jpn Sod Mech Eng, 1984; 50(453): 1267 [4] Tschegg E K. Mater Sci Eng, 1982; 54: 127 [5] Tschegg E K. J Mater Sci, 1983; 18: 1604 [6] Yu H C, Tanaka K, Akiniwa Y. Fatigue Fract Eng Mater Struct, 1998; 21: 1067 [7] Yu H C, Xie S S, Tanaka K, Akiniwa Y. J Mater Eng, 2002; (Suppl.): 317 (于慧臣,谢世殊,田中启介,秋庭义明.材料工程,2002;(增 刊):317) [8] Yu H C, Xie S S, Sun Y G, Tanaka K. J Aeronaut Mater, 2004; 24(5): 53 (于慧臣,谢世殊,孙燕国,田中启介.航空材料学报, 2004; 24(5):53) [9] Yu H C, Sun Y G, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 73 (于慧臣,孙燕国,谢世殊,田中启介.金属学报, 2005;41: 73) [10] Ritchie R O, McClintock F A, Hayeb-Hashemi H, Ritter M A. Metall Trans, 1982; 13A: 101 [11] Tada H, Paris P C, Irwin G R. The Stress Intensity Factor Handbook. 2nd ed., 1985: 27 [12] Tanaka K, Akiniwa Y, Nakamura H. Fatigue Fract Eng Mater Struct, 1996; 19: 571 [13] Tanaka K, Akiniwa Y, Yu H C. ASTM STP 1359, 1999: 295 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|