EFFECT OF POTENTIAL PERTURBATION POLARIZATION ON THE STRESS CORROSION CRACKING OF 1Cr18Ni9Ti STAINLESS STEEL |
NIU Lin; CAO Chunan; LIN Haichao (State Key Laboratary for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: NIU Lin; Tel: (024)23915893; Fax: (094)23894149; E-mail: lin.h.c@icpm.syb.ac.cn |
|
Cite this article:
NIU Lin; CAO Chunan; LIN Haichao (State Key Laboratary for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: NIU Lin; Tel: (024)23915893; Fax: (094)23894149; E-mail: lin.h.c@icpm.syb.ac.cn. EFFECT OF POTENTIAL PERTURBATION POLARIZATION ON THE STRESS CORROSION CRACKING OF 1Cr18Ni9Ti STAINLESS STEEL. Acta Metall Sin, 1998, 34(9): 959-965.
|
Abstract The SCC susceptibility of 1Cr18Ni9Ti austenitic stainless steel in 0.75mol·L-1HCl +0.25mol·L-1NaCl solution has been studied by slow strain rate tests(SSRT) and SEM. During the slow rate tensile process, the specimen was polarized with different potential perturbation modes such as potentiostatic, cyclic potential scan and cyclic potential step methods. The results indicated that potential scan rate and step frequency played an essential role in the initiation and propagation of crack. Potential step at high frequency led to much higher cracking susceptibility than potential scan within the same potential ranges.
|
Received: 18 September 1998
|
1 Hoar T P, Hines J G Corrosion, 1963; 19: 331t 2 Hehemann R F. Metall Trans A, 1985; 16A: 1909 3 Haruyama S, Asawa S. Corros Sci, 1973;13:395 4 Tanno K, Yashiro H, Kawamura Y, Umegai K, Kumagai N. Corrosion, 1993; 49: 319 5 Maier I, Galvele J R. Corrosion, 1980; 36: 309 6 Congleton J, Yang W Corros Sci, 1995; 37: 429 7 Manfredi C, Maier I A, Galvele J R. CorrosSci, 1987; 27: 887 8 Parkins R N. Corros Sci, 1980; 20: 147 9 Magniu T, Chieragatti R, Oltra R. Acta Metall Mater, 1990; 38: 1313 10 KanfmanM J, Fink J K. Acta Metall, 1988; 36: 2213 11 张天成,褚武扬,史训清,朱万旭,刘宝深.金属学报,1997;33:309(Zhang T C, Chu W Y, Shi X C, Zhu W X, Liu B C, Acta Metall Sin , 1997; 33: 309) 12 林昌健,冯祖德,林福龄,王发扬,谭建光,王元辉电化学,1995;1:439(Lin C J, Feng Z D, Lin F L, Wang F Y, Tan J G, Wang Y H. Electrochemistry, 1995;1: 439) 13 田昭武著.电化学研究方法北京:科学出版社,1984:201(Tian Z W. Research Method inElectrochemistry. Beijing: Science Press, 1984: 201) |