CELLULAR SPACING SELECTION OF Al-0.53Zn ALLOY UNDER NEAR-RAPID DIRECTIONAL SOLIDIFICATION CONDITION
FENG Jian; HUANG Weidong; LIN Xin; LI Tao; XUE Yeing; ZHOU Yaohe(State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072)Correspondent:FENG Jian; Tel: (O29)-8494001; Fax: (0E9)-8491544;E-mail. Huang@nwpu.edu.cn Manuscript received 1998-03-10; in revised form 1998-06-01
Cite this article: 

FENG Jian; HUANG Weidong; LIN Xin; LI Tao; XUE Yeing; ZHOU Yaohe(State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072)Correspondent:FENG Jian; Tel: (O29)-8494001; Fax: (0E9)-8491544;E-mail. Huang@nwpu.edu.cn Manuscript received 1998-03-10; in revised form 1998-06-01. CELLULAR SPACING SELECTION OF Al-0.53Zn ALLOY UNDER NEAR-RAPID DIRECTIONAL SOLIDIFICATION CONDITION. Acta Metall Sin, 1998, 34(12): 1267-1272.

Download:  PDF(2252KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to investigate the response of primary cellular/dendritic spacing selection to the variation of growth velocity under near-rapid directional solidification condition, anAl-0.53Zn alloy is directionally solidified with Bridgman apparatus. The results show that atthe given temperature gradient the microstructures is cells and there exists a wide distributionrange of cellular spacing. The maximum, A..., minimum, and average cellular spacing,A, as fullctions of growth rate, v, can be given by λmax=948.51v(-0.4961),λmin=661.16 v(-0.5015),λ=412.41 v(-0.5049), respectively. The experimental results are compared with that predicted bythe current KGT model, and a good agreement is found. Moreover, it is found that the averagecellular spacing is also remarkably history-dependent.
Key words:  Al-Zn alloy      near-rapid directional solidification      cellular spacing selection      history-dependence     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I12/1267

1Warren J A, Langer J S. Phys Rev, 199O; A42: 3518
2 Warren J A, Langer J S. Phys Rev 1993; E47: 2702
3Lu shuzu,Hunt J D.J Cryst Growth,1992;123:17
4 Hunt J D, Lu Shuzu. Metall Mater Trans, 1996; A27: 611
5 Han S H,Trivedi R.Acta Metall Mater,1994242:25
6 Quested P N,McLean M.Mater,Sci Eng,1984;65:171
7 Chopra M A, Tewari S N. Metall Trans,1991; A22: 2467
8 Huang Weidong,Geng Xingguo,ZHou Yaohe,J Cryst Growth,1993;134:105
9 Ding G L, Huang W D, Huang X, Lin X, Zhou Y H. Acta Mater 1996; 44: 3705
10林鑫,黄卫东,潘清跃,丁国陆,薛玉芳,周尧和.金属学报,1997; 33: 1140 (Lin X, Huang W D, Pan Q Y, Ding G L, Xue Y F, Zhou Y H. Acta Metall Sin, 1997; 33: 1140)
11 Kurzw,Gioranola B,Trivedi R,Acta Metall,1986;34:823
12 Boettinger W J,Bendersky L A,Coriell R J.Schaefer R J.Biancaniello F S.J Cryst Growth,1987;80:17
13 Juarez-Islas J A,Jones H ,Kurz W .Mater Sci Eng ,1988;98:201
14 Juarez-Islas J A,Joues H.Acta Metall , 1987; 35:499
15 Gremaud M,Carrard M,Kurz w.Acta Metall Mater,1990;38:2587
16 Kurz W, Fisher D J Acta Metall, 1981; 29: 11
17 Trivedi R.Kurz W.Int Mater Rev,19942 3g:49
18 Hunt J D,Solidification and Casting of Metals London:The Metals Society ,1979:3
19 Sato T, Ito K, Ohira G Trans Jpn Inat Met, 1980; 21: 441
20 Lu S Z, Hunt J D, Gilgien P, Kurz W. Acta Metall Matet 1994; 42: 1653
[1] HOU Danhui, LIANG Songmao, CHEN Rongshi, DONG Chuang. SOLIDIFICATION BEHAVIOR AND GRAIN SIZE OF SAND CASTING Mg-6Al-xZn ALLOYS[J]. 金属学报, 2014, 50(5): 601-609.
[2] ZHAN Meiyan, LI Chunming,ZHANG Weiwen. AN EBSD STUDY ON THE MICROSTRUCTURE AND TEXTURE EVOLUTION OF AZ31 MAGNESIUM ALLOY DURING ACCUMULATIVE ROLL-BONDING[J]. 金属学报, 2012, 48(6): 709-616.
[3] XIE Yu ZHANG Yan CHEN Rongshi HAN Enhou. RELATIONSHIP OF COMPOSITIONS, PHASE CONSTITUENTS AND SOLIDIFICATION PATHS OF CASTING Mg-Al-Zn ALLOYS[J]. 金属学报, 2009, 45(11): 1396-1401.
[4] LIN Xin;HUANG Weidong;PAN Qingyue;DING Guolu;XUE Yufang;ZHOU Yaohe(Stale Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072). RESEARCH ON PRIMARY DENDRITIC SPACING IN UNIDIRECTIONAL SOLIDIFICATION OF Al-4.5Cu SINGLE CRYSTAL[J]. 金属学报, 1997, 33(11): 1140-1146.
[5] LIU Jinshui;SHU Zhen;LI Chuanping Hunan University; Changsha. INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS[J]. 金属学报, 1993, 29(11): 9-13.
No Suggested Reading articles found!