Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (12): 1273-1278    DOI:
Current Issue | Archive | Adv Search |
ON CHARACTERIZATION OF MICROSTRESS MEASURED BY X-RM DIFFRACTION
ZHANG Dingquan(Shaoxing College of Arts and Sciences; Shaoxing 312000)HE Jiawen(State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 710049)Correspondent:ZHANG Dingquan; associate professor;Tel: (O575)8067050-2812; Fax. (0575)8067917;E-mail: ZX9915@163.NetManuscript received 1998-02-09; in revised form 1998-07-10
Cite this article: 

ZHANG Dingquan(Shaoxing College of Arts and Sciences; Shaoxing 312000)HE Jiawen(State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 710049)Correspondent:ZHANG Dingquan; associate professor;Tel: (O575)8067050-2812; Fax. (0575)8067917;E-mail: ZX9915@163.NetManuscript received 1998-02-09; in revised form 1998-07-10. ON CHARACTERIZATION OF MICROSTRESS MEASURED BY X-RM DIFFRACTION. Acta Metall Sin, 1998, 34(12): 1273-1278.

Download:  PDF(558KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Microstress measured by X-ray diffraction method is usually characterized bypeak profile. When the classification of internal stress is based on the model suggested by Macherauch, the second kind of internal stress in the crystalline should be associated with the statisticdeviation of strains in various grains with respect to macro-strain.The value of macro-strainleads to the evaluation of the first kind of internal stress. However, in some cases micro-strainalso results in the peak shift of X-ray diffraction profile. Therefore, besides of peak broadening,one should keep an eye on the effect of dricro-strain on peak shift when microstress is evaluated.The peak shift part stands for the average value and the peak broadening stands for its deviation.
Key words:  internal stress      microstress      pseudo-macrostress      X-ray method     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I12/1273

1 1935;4(6):688(Daviginkof N N Industrial Laboratory, 1935i 4(6): 688)
2 Greenough G B.J Iron Steel Iust, 1951; 169: 235
3辛岛诚一,岛谷幸治,一柳肇材料,1963;12:848(Karashim S, Shimatani K, Hitotssuyanagi H. Material, 1963; 12: 848
4 Bollenrath P, Hank V, Ohly W. Areh Eisewhuettenwes, 1970; 41: 445
5 Garrod RI, Hawkes G A. Br J Appl Phys, 1963; 14: 422
6Macherauch E,Wohlfahrt H.Wolfstieg V.Haerterei-Tech Mitt,1973;28:201(Macherauch E, WOhlfahrt H, Wolfstieg V. Trans Hardening Technol,1973; 28: 201)
7Eigenmann B,Macherauch E,Mat-wiss werkstofftech,1995;26:148(Eigenmann B,Macherauch E.Mater Sci Technol,19952 26:148)
8Cullity B D. Ady X-Ray Anal, 1976; 20: 259
9康飞宇,唐遒泳,刘秀瀛.机械强度,19912 13(1:22(Kang F Y, Tang N Y, Liu X Y.J Mech Strength ,1991; 13(1): 22)
10Scholtes B.Eigenspannungen in Mechanisch Randschichtverformten Werkstoffzustaenden,Oberurel:DGMInformationsg6sellschaft Verlag, 1991: 120(Scholtes B,Residual Stresser in Mehanic surface-deformed Materials.Oberursel:GSM Information Society Press, 1991: 120)
11张建中,冯忠信,张定铨,胡志忠,陈新增,胡奈赛西安交通大学学报,1982;16(1):23(zhang J z,Feng z x,zhang D Q,Hu z z,chen x z,Hu N s.J xi’an Jiaotong Univ 1982; 16(1):23)3
[1] Teng GUO, Hongtao LI, Bailing JIANG, Yibin XING, Xinyu ZHANG. Evolution of Substrate "Heat Affected Zone" in Ion Plating and Its Effect on Coatings[J]. 金属学报, 2018, 54(3): 463-469.
[2] ZHANG Haixia, LI Zhongkui, ZHOU Lian, XU Bingshe, WANG Yongzhen. EFFECTS OF STRUCTURE AND INTERNAL STRESSES IN OXIDE FILMS ON CORROSION MECHANISM OF NEW ZIRCONIUM ALLOY[J]. 金属学报, 2014, 50(12): 1529-1537.
[3] CHAI Huifen;RUAN Zheng;FAN Qunchen Xi'an Jiaotong University associate professor; Department of Materials; Xi'an Jiaotong University; Xi'an 710049. EFFECT OF SLIP MODE ON CYCLIC BEHAVIOUR OF PRESTRAINED MATERIALS[J]. 金属学报, 1993, 29(4): 7-12.
No Suggested Reading articles found!