| EFFECT OF SURFACE TREATMENT BY PHOSPHORIC ACID ON OXIDATION RESISTANCE OF TiAl INTERMETALLICS |
| TANG Zhaolin; WANG Fuhui; WU Weitao(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Coerespondent: TANG Zhaolin; Tel: (024)23915911; Fax: (024)23894149;E-mail: zltang@icpm.syb.ac.cn |
|
Cite this article:
TANG Zhaolin; WANG Fuhui; WU Weitao(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Coerespondent: TANG Zhaolin; Tel: (024)23915911; Fax: (024)23894149;E-mail: zltang@icpm.syb.ac.cn. EFFECT OF SURFACE TREATMENT BY PHOSPHORIC ACID ON OXIDATION RESISTANCE OF TiAl INTERMETALLICS. Acta Metall Sin, 1998, 34(10): 1084-1088.
|
|
|
Abstract The effect of phosphoric acid surface treatment on oxidation resistance of TiAlintermetallics was investigated. The results showed that this surface treatment reduced theoxidation rate of TiAl by one order of magnitude, and it is very effective in improving the cyclicokidation resistance. It is determined that the improvement of the oxidation resistance was dueto the formation of a nearly continuous inner A12O3 layer.Keywods:TiAl intermetallics, isothermal/cyclic oxidation, surface treatment
|
|
Received: 18 October 1998
|
1 Tetsui T. In: Nathal M V, Datolia K Liu C L, Martin P L, Miracle D B, Wagner R, Yamaguchi M eds, Stractural Intermetallics 1997, Warrendale, PA: Miner Met Mater Soc, 1997: 489 2 Brady M P, Brindley W J, Smialek J L, Locci I. JOM, 1996; 48: 46 3 Tang Zhaolin, Wang Fuhui, Wu Weitao. In: Nathal M V, Darolia R, Liu C L, Martin P L, Miracle D B,Wagner R, Yamaguchi M eds., Structural Intermetallics 1997, Warrendale,PA: Miner Met Mater Soc, 1997:341 4 Taniguchi S.MRS Bull,1994 ; 10: 31 5 贺跃辉,黄伯云,曲选辉,刘业翔.材料研究学报,1996;10:603(He Y H, Huang B Y, Qu X H, Liu Y X.Chin J Mater Res,1996; 10: 603) 6 Zhang Y, Li X, Chen C. In: Nathal M V, Darolia R, Liu C L, Martin P L, Mircle D B, Wagner R,Yamaguchi M eds., Structural Intermetallics 1997, Warendale, PA: Mine Met Mater Soc, 1997: 411 7 熊谷正树,涉江和久,金 睦淳.日本金属学会志,1993;57:721(Kuwi M, Shibue K, Kim M. J Jpn Inst Met, 1993; 57: 721) 8 辛丽.中国科学院金属腐蚀与防护研究所博士学位论文,1997(Xin L. PhD Thesis, Institute of Corrosion and Protection of Metals, The Chinese Academy of Sclemy of Sciences, 1997) 9 Kawnura H, Nishiuo K, Saito T. In: Nathal M V, Darolia R D, Liu C L, Martin P L, Miracle D B,Wagner R, Yamaguchi M eds., Structural Intermetallics 1997, Warrendale, PA: Miner Met Mater Soc,1997: 377t |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|