THE THRESHOLD STRESS FOR HYDSOGEN-INDUCED CRACKING OF C90 TUBULAR STEELS |
CHU Wuyang; LU Rongbang;QIAO Lijie; WANG Yanbin (Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083)CHENG Yihuan; CHEN Hongxing(Baoshan Iron and Steel Corporation; Shanghai 201900);GUAN Yongsheng; YAN Yinglong; SUN Wei(Tianjin Steel Pipe Corporation; Tianjin 300310)Correspondent:CHU Wuyang; professor Tel: (010)62332906; Fax: (010)62327283;E-mail: ljqiao@public.bta.net.cn |
|
Cite this article:
CHU Wuyang; LU Rongbang;QIAO Lijie; WANG Yanbin (Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083)CHENG Yihuan; CHEN Hongxing(Baoshan Iron and Steel Corporation; Shanghai 201900);GUAN Yongsheng; YAN Yinglong; SUN Wei(Tianjin Steel Pipe Corporation; Tianjin 300310)Correspondent:CHU Wuyang; professor Tel: (010)62332906; Fax: (010)62327283;E-mail: ljqiao@public.bta.net.cn. THE THRESHOLD STRESS FOR HYDSOGEN-INDUCED CRACKING OF C90 TUBULAR STEELS. Acta Metall Sin, 1998, 34(10): 1077-1083.
|
Abstract During dynamically charging four kinds of C90 tubular steels with hydrogen,the concentration of divisible hydrogen c0 is directly proportional to cathodic current i, and thenormalized threshold stress σc.(H)/σt decreases linearly with hi c0, i.e., σc(H)/σt=A-B ln c0.The concentrations of diffusible hydrogen in the steels during immersing in the H2S saturationsolution, c0*, have been measured. The values of σc(H)/σt during dynamically charging withic corresponding to c0* for the four steels are consistent with the threshold stress σc(H2S)/ctduring SCC in H2S solution. The result shows that the threshold stress during charging with asuitable current density ic can substitute for the threshold stress during SCC in H2S solution.
|
Received: 18 October 1998
|
1褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,1988(Chu W Y.Hudrogen Damage and Delayed Fracture.Beijing:The Metallurgicla Industry Press,,1988) 2黄长河,梅东生,俞梦文,王燕斌,褚武扬.中国腐蚀与防护学报,1997;17:129(Huang C H, Mei D S, Yu M W, Wang Y B, Chu W Y. J Chin Soc Corros Prot, 1997; 17: 129) 3于广华,程以环,陈红星,牛学军,乔利杰,褚武扬.金属学报,1996;32:617(Yu G H, Cheng Y H, Chen H X, Niu X J, Qiao L J, Chu W Y. Acta Metall Sin, 1996; 32: 617) 4Gao K W, Wang Y B, Chu W Y. Sci Chin, 1995; 38A: 1501 5Gu B, Gao K W, Huang Y Z, Chu W Y .Sci Chin, 1997; 40E: 235 6Su Y J, Wang Y B, Chu W Y. Sci Chin, 1997; 40E: 661 7Li M D, Zhang T C, Lu H, Chu W Y. Sci Chin, 1997; 40E: 530 8于广华,程以环,陈廉,乔利杰,褚武扬.金属学报,1995;31:A454(Yu G H, Cheng Y H, Chen L, Qiao L J, Chu W Y. Acta Metall Sin, 1995; 31: A454) 9Bao X; Chu W Y, Hsiao C M. Scr Metall, 1987; 21: 613( |