DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS |
WANG Weiguo; ZHOU Bangxin; ZHENG Zhongmin(Laboratory for Nuclear Fuel and Materials; Nuclear Power Institute of China; Chengdu 610041)Correspondent: WANG Weiguo; Tel: (028)5582199-88531 |
|
Cite this article:
WANG Weiguo; ZHOU Bangxin; ZHENG Zhongmin(Laboratory for Nuclear Fuel and Materials; Nuclear Power Institute of China; Chengdu 610041)Correspondent: WANG Weiguo; Tel: (028)5582199-88531. DAMPING CAPACITY OF Fe-Cr-Al-Si ALLOYS. Acta Metall Sin, 1998, 34(10): 1039-1042.
|
Abstract The effect of silicon on the damping capacity of Fe-Cr-Al alloy has beeninvestigated with the inverted torsion pendulum teclmiques. The results indicate that, smallamount silicon (app. 1% mass fraction) addition to Fe-Cr-Al or substitution of silicon foraluminum in Fe-Cr-Al alloy can make the damping capacity of the alloys higher than that ofFe-Cr-Al alloy when annealed below 1273 K; substituting silicon for small amount aluminum inFe-Cr-Al, the damping capacity of the alloy is much higher than that of Fe-Cr-Al alloy whenannealed above 1373 K followed by air cooling. The curves of logajrithmic decrement versus strainamplitude reveal the damping of the alloys resulting mainly from magonetomechanical hystereses.
|
Received: 18 October 1998
|
1Masumoto H, Hinai M, Sawsya S. Trans Jpn Inst Met, 1984; 25: 891 2Karimi A, Giaugue P H, Martin J L. Mater Sci Forum, 1995; 179-181: 679 3Hinai M, Sawaya S, Masumoto H. Trans Jpn Inst Met, 1994; 35: 74 4Yamada T, Takamura T, Hashisume S, Odakei T, Omori T, Hation K. NKK Technical Review, No.65, 1992: 21 5佐藤昭治,砂田晃,渡边敏.热处理, 1992; 32: 340 (Sotoh S, Sunada A, Watanabe S, Heat Treat, 1992; 32: 340) 6Cochart A W.J Appl Mech,1961; 15: 196 7Smith G W, Birchak J R. J Appl Phgs, 1968; 39: 2311 8Astie B, Dugaugue J.J Phys(Paris), 1981; 42: 627 9Lee K H, Vdovenko V A, Cho K K.J Korean Inst Met Mater 1994; 32: 1499 10冯端,王业宁,丘第荣.金属物理.第一版,北京:科学出版社,1964 (Feng D,Wang Y N,Qiu D R.Metal Physics.Beijing:Science Press,1964) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|