Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (5): 509-514    DOI:
Current Issue | Archive | Adv Search |
FLOWING SIMULATION OF MOLTEN STEEL IN SLAB TUNDISH BY HOT WATER MODEL
WANG Jianjun;DAI Chaoshan;ZHOU Li(East China Institute of Metallurgy;Ma'anshan 243002); ZHANG Yuzhu (Handan Iron and Steel Co.; Handan 056000);LI Zhenghang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081); XIAO Zeqiang (Northeastern University; Shenyang 110006)
Cite this article: 

WANG Jianjun;DAI Chaoshan;ZHOU Li(East China Institute of Metallurgy;Ma'anshan 243002); ZHANG Yuzhu (Handan Iron and Steel Co.; Handan 056000);LI Zhenghang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081); XIAO Zeqiang (Northeastern University; Shenyang 110006). FLOWING SIMULATION OF MOLTEN STEEL IN SLAB TUNDISH BY HOT WATER MODEL. Acta Metall Sin, 1997, 33(5): 509-514.

Download:  PDF(442KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The paper studies the flow pattern of molten steel in slab tundish by a hot water model. The results provide that the flow pattern with changed density is opposite from that with constant density because of heat loosing in tundish, which provides the natural convection in slab tundish shouldn't be neglected.
Key words:  continuous casting      tundish      water model     
Received:  18 May 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I5/509

1 Lowry H L,Sahai Y.ISS Trans,1993;14:17
2 Joo S Guthrie R L L.Metall Trans,1993;24B:767
3 Damle C,Sahai Y.ISIJ Int,1996;36:681
4高家锐.动量、热量、质量传输原理,重庆:重庆大学出版社,1987:216
[1] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[3] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[4] GUO Zhongao, PENG Zhiqiang, LIU Qian, HOU Zibing. Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. 金属学报, 2021, 57(12): 1595-1606.
[5] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[6] CAI Laiqiang, WANG Xudong, YAO Man, LIU Yu. Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet[J]. 金属学报, 2020, 56(8): 1165-1174.
[7] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[8] TANG Haiyan, LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan. Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control[J]. 金属学报, 2020, 56(12): 1629-1642.
[9] LI Yaqiang, LIU Jianhua, DENG Zhenqiang, QIU Shengtao, ZHANG Pei, ZHENG Guiyun. Peritectic Solidification Characteristics and Mechanism of 15CrMoG Steel[J]. 金属学报, 2020, 56(10): 1335-1342.
[10] Chunlei WU,Dewei LI,Xiaowei ZHU,Qiang WANG. Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet[J]. 金属学报, 2019, 55(7): 875-884.
[11] GUO Junli, WEN Guanghua, FU Jiaojiao, TANG Ping, HOU Zibing, GU Shaopeng. Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels[J]. 金属学报, 2019, 55(10): 1311-1318.
[12] Zibing HOU, Rui XU, Yi CHANG, Jianghai CAO, Guanghua WEN, Ping TANG. Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet[J]. 金属学报, 2018, 54(6): 851-858.
[13] Xinhua LIU, Huadong FU, Xingqun HE, Xintong FU, Yanqing JIANG, Jianxin XIE. Numerical Simulation Analysis of Continuous Casting Cladding Forming for Cu-Al Composites[J]. 金属学报, 2018, 54(3): 470-484.
[14] Miaoyong ZHU, Wentao LOU, Weiling WANG. Research Progress of Numerical Simulation in Steelmaking and Continuous Casting Processes[J]. 金属学报, 2018, 54(2): 131-150.
[15] Qiang WANG, Ming HE, Xiaowei ZHU, Xianliang LI, Chunlei WU, Shulin DONG, Tie LIU. Study and Development on Numerical Simulation for Application of Electromagnetic Field Technologyin Metallurgical Processes[J]. 金属学报, 2018, 54(2): 228-246.
No Suggested Reading articles found!